Robust Nanogenerators Based on Tribo-Positive Graft Copolymers of Tribo-Negative Poly(vinylidene fluoride) Robust Nanogenerators Based on Tribo-Positive Graft Copolymers of Tribo-Negative Poly(vinylidene fluoride) AITranslate
Abstract AITranslate
Poly(vinylidene fluoride) (PVDF) and its copolymers are useful for a diverse range of applications in energy production and storage, sensors, actuators, separator, and filter membranes. Herein, we report on the single-step transformation of electroactive tribo-negative pristine PVDF into tribo-positive PVDF copolymer (G-PVDF) by grafting poly(diethylene glycol methyl ether methacrylate) on the backbone by a coupled atom-transfer radical polymerization protocol. The resultant G-PVDF with rough spherulitic morphology is utilized to fabricate a triboelectric nanogenerator (G-TENG) using the combination of tribo-negative polydimethylsiloxane as active materials. Highly robust G-TENG generates a peak-to-peak voltage of ∼1050 V under open-circuit condition and an output current density of 31.25 × 10–2 A m–2 equivalent to an output power density of 56.25 W m–2. Furthermore, the application of the G-TENG as a realistic portable electrical power source is shown by powering over 400 market-available red light-emitting diodes and liquid crystal displays. The G-TENG shows mechanical stability over 9500 cycles and ambient stability over 150 days. Parallel to the scavenging of electrical energy from mechanical energy, we demonstrate the use of G-TENG for flexible self-powered health care applications. The synthesis of tribo-positive G-PVDF copolymer as a green energy-harvesting material has great potential for a variety of applications considering the versatile use of pristine PVDF.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c01005
Chinese Library Classification Number:
Citation Information:
Poly(vinylidene fluoride) (PVDF) and its copolymers are useful for a diverse range of applications in energy production and storage, sensors, actuators, separator, and filter membranes. Herein, we report on the single-step transformation of electroactive tribo-negative pristine PVDF into tribo-positive PVDF copolymer (G-PVDF) by grafting poly(diethylene glycol methyl ether methacrylate) on the backbone by a coupled atom-transfer radical polymerization protocol. The resultant G-PVDF with rough spherulitic morphology is utilized to fabricate a triboelectric nanogenerator (G-TENG) using the combination of tribo-negative polydimethylsiloxane as active materials. Highly robust G-TENG generates a peak-to-peak voltage of ∼1050 V under open-circuit condition and an output current density of 31.25 × 10–2 A m–2 equivalent to an output power density of 56.25 W m–2. Furthermore, the application of the G-TENG as a realistic portable electrical power source is shown by powering over 400 market-available red light-emitting diodes and liquid crystal displays. The G-TENG shows mechanical stability over 9500 cycles and ambient stability over 150 days. Parallel to the scavenging of electrical energy from mechanical energy, we demonstrate the use of G-TENG for flexible self-powered health care applications. The synthesis of tribo-positive G-PVDF copolymer as a green energy-harvesting material has great potential for a variety of applications considering the versatile use of pristine PVDF.
quote
| GB/T 7714-2015 | [1] Tapas Kamilya, Mahuya Pakhira, Piyush Kanti Sarkar, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01005. |
| MLA | [1] Tapas Kamilya, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01005. |
| APA | [1] Tapas Kamilya, Mahuya Pakhira, Piyush Kanti Sarkar, Md Yousuf Sk, Sanjib Naskar, & Somobrata Acharya. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01005 |
| IEEE | [1] Tapas Kamilya, Mahuya Pakhira, Piyush Kanti Sarkar, Md Yousuf Sk, Sanjib Naskar, and Somobrata Acharya, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01005. keywords: {PVDF GPVDF atomtransfer radical polymerization GTENG selfpowered applications} |