Ion-Conducting, Supramolecular Crosslinked Elastomer with a Wide Linear Range of Strain Resistances AITranslate
Abstract AITranslate
A conductive elastomer is stretchable and can exhibit ionic or electrical conductivity. However, its resistivity increases exponentially when a small number of strain changes are provided owing to irreversible internal deformation. Therefore, securing a wide range of linearity in the resistance–strain relationship is an important topic in the preparation of highly reliable conductive elastomers. Herein, an ionic conductive elastomer is prepared using 2-methoxyethyl acrylate (MA) and a molecular necklace-like polyrotaxane (PRX) cross-linker to impart reversible elastic properties. The MAPRX exhibits a superior stretchability of up to 1420% with a tensile strength of 0.52 MPa. Besides, it shows a wide range of strain–resistance linearities (∼1100%) owing to the slidable supramolecular cross-linkers. Its linear sensitivity to the provided strain makes it possible to apply it to facile wearable strain sensors with good reproducibility.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00773
Chinese Library Classification Number:
Citation Information:
A conductive elastomer is stretchable and can exhibit ionic or electrical conductivity. However, its resistivity increases exponentially when a small number of strain changes are provided owing to irreversible internal deformation. Therefore, securing a wide range of linearity in the resistance–strain relationship is an important topic in the preparation of highly reliable conductive elastomers. Herein, an ionic conductive elastomer is prepared using 2-methoxyethyl acrylate (MA) and a molecular necklace-like polyrotaxane (PRX) cross-linker to impart reversible elastic properties. The MAPRX exhibits a superior stretchability of up to 1420% with a tensile strength of 0.52 MPa. Besides, it shows a wide range of strain–resistance linearities (∼1100%) owing to the slidable supramolecular cross-linkers. Its linear sensitivity to the provided strain makes it possible to apply it to facile wearable strain sensors with good reproducibility.
quote
| GB/T 7714-2015 | [1] Bitgaram Kim, Taesung Park, Soong Ju Oh, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00773. |
| MLA | [1] Bitgaram Kim, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00773. |
| APA | [1] Bitgaram Kim, Taesung Park, Soong Ju Oh, & JiHun Seo. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00773 |
| IEEE | [1] Bitgaram Kim, Taesung Park, Soong Ju Oh, and JiHun Seo, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00773. keywords: {polyrotaxanes;supermolecules;conductive elastomers;slidable crosslinkers;strain sensor} |