Recovery of K2TiF6 from Ta/Nb Ore Extraction Raffinate AITranslate
Abstract AITranslate
Study is made of the process for recovery of Ti from Ta/Nb ore extraction raffinate. The results show that commercial can be produced K2TiF6 from Ti-containing extraction raffinate by HF(in gas state) acid control,KCl conversion,cooling and crystallization, centrifugal filtering and drying. The process is simple with less environmental pollution and better economic benefit.
KeyWords AITranslate
1泽列克曼A H,等.稀有金属冶金学[M].北京:冶金工业出版社,1982.
1姜老师信箱[J].中国生物工程杂志,2011,31(11):30-30.
2李媛,徐书景,张庆,王丽敏,于波,鞠建松,赵宝华.采用钠盐调酸发酵生产D-乳酸的工艺研究[J].河北师范大学学报:自然科学版,2014,38(3):296-300. 被引量:2
3吕碧涛,袁文,徐盛明,刘百峰,曹莉.大鼠Nogo受体基因RNA干扰慢病毒载体的构建与鉴定[J].第二军医大学学报,2007,28(1):40-43. 被引量:2
4李立民,惠洪文,王明芳.纳豆激酶分离提纯方法中试研究[J].内蒙古农业大学学报:自然科学版,2003,24(4):51-54. 被引量:5
5曹小红,闫仲丽,王春玲.家蝇变形期抗菌蛋白的提取及其抑菌活性研究(英文)[J].中国生物工程杂志,2006,26(1):33-37. 被引量:1
6李升锋,徐玉娟,陈智毅,刘学铭,张友胜,吴继军.微乳薄层层析法分离桑叶中的黄酮类化合物[J].食品科学,2008,29(6):87-89. 被引量:11
7赵一凡,谷克仁,牛付欢.植物甾醇提取新工艺[J].食品科学,2008,29(7):192-196. 被引量:9
8刘宝树,王亚川,孙华,崔雪君,王禄.胡椒醛球形聚结工艺研究[J].中国食品添加剂,2016,0(3):127-131.
9彭涤非,钟彩虹,周海燕,曾斌,王中炎.三叶木通(Akebia trifoliata)果实乙醇提取物对酪氨酸酶体外活性的影响[J].武汉植物学研究,2008,26(2):183-185. 被引量:21
10姜贵全,方桂珍.地榆根中低聚原花青素的提取工艺[J].东北林业大学学报,2008,36(1):41-42. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:Q135.13[生物学—普通生物学]
Citation Information:
Study is made of the process for recovery of Ti from Ta/Nb ore extraction raffinate. The results show that commercial can be produced K2TiF6 from Ti-containing extraction raffinate by HF(in gas state) acid control,KCl conversion,cooling and crystallization, centrifugal filtering and drying. The process is simple with less environmental pollution and better economic benefit.
quote
| GB/T 7714-2015 | [1] WU Zun-zhong. Recovery of K2TiF6 from Ta/Nb Ore Extraction Raffinate[J]. Rare Metals and Cemented Carbides, 2006(1): 46-48. |
| MLA | [1] WU Zun-zhong. "Recovery of K2TiF6 from Ta/Nb Ore Extraction Raffinate." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 46-48. |
| APA | [1] WU Zun-zhong. (2006). Recovery of K2TiF6 from Ta/Nb Ore Extraction Raffinate. Rare Metals and Cemented Carbides(1), 46-48. |
| IEEE | [1] WU Zun-zhong, "Recovery of K2TiF6 from Ta/Nb Ore Extraction Raffinate," Rare Metals and Cemented Carbides, no. 1, pp. 46-48, 2006. keywords: {Ti-containing Ta/Nb ore;extraction raffinate;K2TiF6 recovery} |