Halide Composition Engineered a Non-Toxic Perovskite–Silicon Tandem Solar Cell with 30.7% Conversion Efficiency AITranslate

Chitkara University; Arunachal University of Studies; Chitkara University; Chitkara University; Al-Farahidi University; Al-Mustaqbal University College;Institute of Electronics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Since the conversion efficiency of silicon (Si)-based solar cells stagnates at 26.7% in the literature, extensive research and development activities are carried out on perovskite silicon-based tandem solar cells. However, the presence of lead (Pb) and the instability of perovskite prevent their large-scale implementation in the photovoltaic industry. Therefore, it is important to replace the hazardous material (Pb) in perovskite top cells to design non-toxic perovskite–silicon tandem solar cells. The current work yields much-needed studies to develop a non-toxic perovskite–silicon-based tandem solar cell. For the first time, methylammonium tin mixed halide (MASnI3–xBrx)-based materials are comprehensively investigated and optimized with respect to different halide compositions, absorber layer thickness, and bulk defect density in standalone configurations, followed by the development of a lead-free MASnI2Br1–Si-based tandem solar cell. The transfer matrix method and current matching techniques are used to design the two-terminal monolithic tandem cell, which showed a maximum conversion efficiency of 30.7% with an open circuit voltage (VOC) of 2.14 V. The results outlined in this manuscript will pave the way for the progress of highly efficient, non-toxic perovskite–silicon tandem solar cells.

KeyWords AITranslate

nontoxic perovskite silicon tandem efficiency
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01574

Chinese Library Classification Number:

Citation Information:

Since the conversion efficiency of silicon (Si)-based solar cells stagnates at 26.7% in the literature, extensive research and development activities are carried out on perovskite silicon-based tandem solar cells. However, the presence of lead (Pb) and the instability of perovskite prevent their large-scale implementation in the photovoltaic industry. Therefore, it is important to replace the hazardous material (Pb) in perovskite top cells to design non-toxic perovskite–silicon tandem solar cells. The current work yields much-needed studies to develop a non-toxic perovskite–silicon-based tandem solar cell. For the first time, methylammonium tin mixed halide (MASnI3–xBrx)-based materials are comprehensively investigated and optimized with respect to different halide compositions, absorber layer thickness, and bulk defect density in standalone configurations, followed by the development of a lead-free MASnI2Br1–Si-based tandem solar cell. The transfer matrix method and current matching techniques are used to design the two-terminal monolithic tandem cell, which showed a maximum conversion efficiency of 30.7% with an open circuit voltage (VOC) of 2.14 V. The results outlined in this manuscript will pave the way for the progress of highly efficient, non-toxic perovskite–silicon tandem solar cells.

quote

GB/T 7714-2015 [1] Rahul Pandey, Sagar Bhattarai, Kulbhushan Sharma, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01574.
MLA [1] Rahul Pandey, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01574.