Mn-Doped Ge Nanoparticles Grown on SiO2 Thin Films by Molecular Beam Epitaxy for Photodetector and Solar Cell Applications Mn-Doped Ge Nanoparticles Grown on SiO2 Thin Films by Molecular Beam Epitaxy for Photodetector and Solar Cell Applications AITranslate
Abstract AITranslate
In this work, we propose a novel efficient strategy based on the combination of molecular beam epitaxy deposition and the solid-state dewetting process for the growth and self-assembly of magnetic GeMn nanoparticles on the SiO2 substrate. Morphological and structural investigations of magnetic GeMn nanoparticles carried out by AFM and HR-TEM microcopies show that these nanoparticles are very dense (1012 cm–2), are homogeneous, and have a free-defect single-crystalline Ge-Mn phase. The investigations of the magnetic properties carried out by a superconducting quantum interference device (SQUID) reveal that our magnetic GeMn nanoparticles are ferromagnetic and have a Curie record temperature of 325 K. The electrical characterizations of these GeMn nanoparticles when they are inserted in the insulator layer of a metal–insulator–semiconductor Schottky diode show that the nanoparticles contribute to electrical transport and photo-generation of hole–electron pairs when illuminated by white light, resulting in a significant increase in photocurrent of the order of 10 times. This novel growth strategy, which is compatible with CMOS technology, represents a promising path toward the real incorporation of diluted magnetic GeMn nanostructures in photodetection and photovoltaic technologies.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00162
Chinese Library Classification Number:
Citation Information:
In this work, we propose a novel efficient strategy based on the combination of molecular beam epitaxy deposition and the solid-state dewetting process for the growth and self-assembly of magnetic GeMn nanoparticles on the SiO2 substrate. Morphological and structural investigations of magnetic GeMn nanoparticles carried out by AFM and HR-TEM microcopies show that these nanoparticles are very dense (1012 cm–2), are homogeneous, and have a free-defect single-crystalline Ge-Mn phase. The investigations of the magnetic properties carried out by a superconducting quantum interference device (SQUID) reveal that our magnetic GeMn nanoparticles are ferromagnetic and have a Curie record temperature of 325 K. The electrical characterizations of these GeMn nanoparticles when they are inserted in the insulator layer of a metal–insulator–semiconductor Schottky diode show that the nanoparticles contribute to electrical transport and photo-generation of hole–electron pairs when illuminated by white light, resulting in a significant increase in photocurrent of the order of 10 times. This novel growth strategy, which is compatible with CMOS technology, represents a promising path toward the real incorporation of diluted magnetic GeMn nanostructures in photodetection and photovoltaic technologies.
quote
| GB/T 7714-2015 | [1] Mansour Aouassa, Mohammed Bouabdellaoui, Makrem Yahyaoui, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00162. |
| MLA | [1] Mansour Aouassa, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00162. |
| APA | [1] Mansour Aouassa, Mohammed Bouabdellaoui, Makrem Yahyaoui, Tarak Kallel, Thouraya Ettaghzouti, Saud A. Algarni, & Ibrahim O. Althobaiti. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00162 |
| IEEE | [1] Mansour Aouassa, Mohammed Bouabdellaoui, Makrem Yahyaoui, Tarak Kallel, Thouraya Ettaghzouti, Saud A. Algarni, and Ibrahim O. Althobaiti, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00162. keywords: {magnetic GeMn nanoparticles MIS solar cells photodetector MBE growth solidstate dewetting electrical characterizationShow More} |