Current and Future Development of Molybdenite Bioleaching Process AITranslate

Institute of Rare Metal Metallurgy, School of Metallurgical Science and Engineering, Central South University;Institute of Rare Metal Metallurgy, School of Metallurgical Science and Engineering, Central South University;Institute of Rare Metal Metallurgy, School of Metallurgical Science and Engineering, Central South University;Institute of Rare Metal Metallurgy, School of Metallurgical Science and Engineering, Central South University;Institute of Rare Metal Metallurgy, School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper described the latest development both at home and abroad of the molybdenite bioleaching process in respect of the tame of bacteria for leaching,leaching bacteria mechanism and the impact of energy substance as well as culture medium and pulp density on Mo beaching.Some questions are put forward.The future development of the said process is predicted.

KeyWords AITranslate

molybdenum metallurgy molybdenite bio-leaching leaching bacteria bacteria tame

1符剑刚,钟宏,吴江丽,卜向明.常温常压条件下辉钼矿的湿法浸出[J].金属矿山,2004(12):35-38. 被引量:17

2[2]Hammaini A,Ballester A,Gonzalez F,et al.Activated slukge as diosorbent of heavy metals[A].Ballester Eds R A.Biohydrometallurgy and the Environment Toward the Mining of the 21st Century (Part B)[C].Tokyo:Elsevier,1999.185-192.

3[3]Artola A,Balguer M D,Rigola M.Compective biosorption of copper,cadmium,nikea and zinc from metal ion mixtures using anaerbiclly digested sludge[A].Ballester Eds R A.Biohydrometallurgy and the Environment Toward the Mining of the 21st Century (Part B)[C].Tokyo:Elsevier,1999.175-183.

4[4]Hui Niua Volesky,Niwton C M Gomes.Enhancement of gdd-cyanide biosorption by L-cysteine[A].Ballester Eds R A.Biohydrometallurgy and the Environment Toward the Mining of the 21st Century (Part B)[C].Tokyo:Elsevier,1999.493-502.

5[6]Srikrajib S,Tongta A,Thiravetyan P,et al.Cadmium removal by the dry biomass ofsargassum polycystum[A].Ballester Eds R A.Biohydrometallurgy and the Environment Toward the Mining of the 21stCentury (Part B)[C].Tokyo:Elsevier,1999.419-427.

6魏宗武,陈建华,艾光华,刘智林.生物浸出——萃取法分离彩钼铅矿的研究[J].有色矿冶,2007,23(1):22-24. 被引量:4

7吉兆宁,余斌,刘坚,陈何,薛云新,马公望,赵新峰.金堆城低品位钼矿石可浸性研究[J].有色金属:矿山部分,2002,54(5):15-18. 被引量:11

8[10]Mishra D,Kim D J,Ralph D E.Bioleaching of vanadium rich spent refinery catalysts using sulfur oxidizing lithotrophs[J].Hydrometallurgy,2007,(88):202-209.

9[11]Nasernejad B,Kaghazchi T.Bioleaching of molybdenum from low-grade copper ore[J].Process Biochemistry,1999,(35):437-440.

10[12]Askare Zamani M A,Hrroyoshi N,Tsunekawa M.Bioleaching of sarcheshmeh molybdenite concentrate for extraction of rhenium[J].Hydrometallurgy,2005,(80):23-31.

1公彦兵,沈裕军,丁喻,周新东.辉钼矿湿法冶金研究进展[J].矿冶工程,2009,29(1):78-81. 被引量:16

2王锐,邱丽娜,关景洋,佟莹,罗佳,弓爱君,闫海.一株嗜酸硫氧化细菌的分离鉴定及生长特性[J].环境科学学报,2010,30(3):485-489. 被引量:4

3张文朴.加强钼资源综合利用与再生研发 促进我国生态钼业建设[J].中国钼业,2010,34(2):13-18. 被引量:3

4姚维,杨爱江,郭贵香,黎丹丹.硫氧化细菌的分离及其对钼镍尾矿的脱硫作用实验研究[J].贵州大学学报:自然科学版,2014,31(5):115-118. 被引量:1

5牟文宁,张鸿彪,苏志强,宋佩.低品位钼矿钠化焙烧-水浸过程钼的转化研究[J].稀有金属,2015,39(9):854-860. 被引量:5

6卢涛,魏德洲,沈岩柏,张瑞洋,曹飞.胶硫钼矿型难选钼矿的微生物浸出试验研究[J].中国矿业大学学报,2016,45(1):157-162. 被引量:4

7刘俊场,杨大锦,付维琴,牟兴兵,欧根能,陈华君,刁微之,邹维.镍钼共生矿加压酸浸动力学研究[J].有色金属:冶炼部分,2017(1):17-19. 被引量:5

1何树荣.工业氧化钼实用生产技术及进展[J].材料开发与应用,2013,28(1):96-101. 被引量:5

2都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3

3吴贤,李来平,张新,张文钲.用矿浆电解法分解辉钼矿试验研究[J].现代矿业,2009(10):61-64. 被引量:1

4都基峻,田刚,曾萍,刘宇,石应杰,张凡.富氧加压反应器焙烧辉钼矿过程研究[J].环境工程技术学报,2011,1(2):151-156.

5沈裕军,杨文魁,公彦兵,丁喻.碱性加压浸出三次氨浸渣中钼的实验研究[J].矿冶工程,2011,31(4):73-76. 被引量:5

6杨文魁,沈裕军,丁喻.镍钼矿湿法冶金研究现状[J].中国钼业,2011,35(5):11-14. 被引量:6

7张邦胜,蒋开喜,王海北.镍钼矿加压酸浸新工艺研究[J].有色金属:冶炼部分,2012(11):10-12. 被引量:13

8张杜超,杨天足,刘伟锋,吴江华.Pressure leaching of bismuth sulfide concentrate containing molybdenum and tungsten in alkaline solution[J].中南大学学报:英文版,2012,19(12):3390-3395. 被引量:3

9张鸿彪,牟文宁,宋佩,卢媛嫄,孙雷雷.钼矿冶炼新工艺发展概论[J].材料导报:纳米与新材料专辑,2013,27(2):87-90. 被引量:5

10吕振福,冯安生.几种矿产资源综合利用率计算方法的探讨[J].矿产保护与利用,2014,34(2):6-8. 被引量:12

1郑存江,熊英,柏全金,胡建平.小河金矿的细菌预氧化研究[J].陕西地质,2000,18(2):93-97. 被引量:3

2张济祥,谢宏潮,阳岸恒,朱勇,邓志明,陈登权.高纯金制备技术研究现状与展望[J].贵金属,2015,36(3):81-86. 被引量:9

3钼盐文摘[J].无机盐技术,2010(2):53-53.

4黄明清,王贻明,杨保华,王洪江,吴爱祥.辉钼矿生物浸出研究进展[J].中国钼业,2011,35(4):14-17. 被引量:8

5刘升明,王淀佐,孙体昌,陈景河.微生物浸金的研究现状与展望[J].矿产综合利用,2004(6):24-28. 被引量:13

6邓恺,吴凯,施惠生.钢渣在水泥及混凝土中资源化利用的现状和进展[J].建材技术与应用,2015(1):7-10. 被引量:2

7张卫民,荆秀艳,邱木清.永平铜矿浸矿细菌驯化培养研究[J].有色金属:冶炼部分,2004(5):5-8. 被引量:17

8颜慧成,刘浏,郭征.钢铁半固态连铸成形技术的研究现状与展望[J].钢铁研究学报,2003,15(5):64-68.

9杨天钧,高征铠,刘述临,杨世山.铁水炉外脱硫的新进展[J].钢铁,1999,34(1):65-69. 被引量:27

10周峨,刘中华,陈雯,谢海云,袁章福.富铁菌液浸出硫化铜精矿中砷的实验初探[J].过程工程学报,2003,3(3):222-226. 被引量:8

Basic Information:

DOI:

Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]

Citation Information:

The paper described the latest development both at home and abroad of the molybdenite bioleaching process in respect of the tame of bacteria for leaching,leaching bacteria mechanism and the impact of energy substance as well as culture medium and pulp density on Mo beaching.Some questions are put forward.The future development of the said process is predicted.

quote

GB/T 7714-2015 [1] CHEN Jia-wu, GAO Cong-jie, ZHANG Qi-xiu, et al. Current and Future Development of Molybdenite Bioleaching Process[J]. Rare Metals and Cemented Carbides, 2008(1): 46-50.
MLA [1] CHEN Jia-wu, et al., "Current and Future Development of Molybdenite Bioleaching Process." Rare Metals and Cemented Carbides, no. 1, 2008, pp. 46-50.
APA [1] CHEN Jia-wu, GAO Cong-jie, ZHANG Qi-xiu, XIAO Lian-sheng, & ZHANG Gui-qing. (2008). Current and Future Development of Molybdenite Bioleaching Process. Rare Metals and Cemented Carbides(1), 46-50.
IEEE [1] CHEN Jia-wu, GAO Cong-jie, ZHANG Qi-xiu, XIAO Lian-sheng, and ZHANG Gui-qing, "Current and Future Development of Molybdenite Bioleaching Process," Rare Metals and Cemented Carbides, no. 1, pp. 46-50, 2008. keywords: {molybdenum metallurgy;molybdenite;bio-leaching;leaching bacteria;bacteria tame}