Experimental Research on Antimony Removal from Niobium Liquid by MIBK Extraction for Preparation of High Purity Niobium Oxide AITranslate

Jiujiang Nonferrous Metal Smooth Co., Ltd.;Jiujiang Nonferrous Metal Smooth Co., Ltd.;Jiujiang Nonferrous Metal Smooth Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

MIBK has different extraction performance for Sb(Ⅲ)and Sb(Ⅴ)under certain acidity condition.Therefore,high purity niobium oxide(Sb content10×10^-6)can be obtained by controlling certain acidity and oxidizing Sb(Ⅲ)into Sb(Ⅴ)in the extraction system of HF-H2SO4-MIBK to meet the requirements of Sb extraction separation to the maximum extent.

KeyWords AITranslate

Sb removal niobium liquid MIBK extraction acidity control oxidant Sb(Ⅲ) Sb(Ⅴ)

1韩建设,周勇.钽铌萃取分离工艺与设备进展[J].稀有金属与硬质合金,2004,32(2):15-20. 被引量:16

2胡根火,郭永忠,宋金华.镁粉还原-仲辛醇萃取法从钽铌矿分解液中除Sb的实验研究[J].稀有金属与硬质合金,2014,42(3):12-14. 被引量:2

1朱国荣.降低湿法制砷工艺液相锑浓度的实验研究[J].铜业工程,2019,0(3):46-48.

2张何鹏,孙思聪,梅龙宝,梁粱.调整价态萃取-陶瓷膜过滤联合除锑制取超高纯氧化铌[J].有色金属科学与工程,2020,11(2):71-75. 被引量:1

3鲁东,喻文斌,王诗海,张伟宁,郭洪范.结晶法和萃取法制备高纯氧化铌的研究[J].广州化工,2020,48(20):53-54. 被引量:1

4胡向平,李建新,杨斌,沈义梅,徐光以,许佩琪,荣幸,孟繁艳.Nb2O5原料对H-ZF类高折射率玻璃透过性能的影响因素[J].材料导报,2020,34(S02):138-141.

1刘自喜.铌酸锂多晶粉的制备工艺研究[J].稀有金属与硬质合金,2022,50(5):66-69.

2王鹏,张军战,张颖,覃枫,杨明辉,陈红侠.催化剂对硅氧碳多孔陶瓷结构与性能的影响[J].稀有金属,2022,46(12):1573-1579.

1郭天立.湿法炼锌生产中杂质锑的净化[J].有色矿冶,1997,13(3):42-47. 被引量:3

2Y.Sasaki,S.Kawai,S.Furuya,王岳.铜电解液除锑方法的进展[J].有色冶炼,1993,22(2):38-41. 被引量:1

3刘智明,李崇元,张宗远.加铝除锑砷在焊锡火法精炼生产中的应用[J].有色金属:冶炼部分,1993(3):8-9.

4毛天舒.用溶剂萃取法从硫酸铜溶液中除锑[J].湿法冶金,2000,19(2):71-71.

5张子悦.用氨基膦酸树脂从铜电解液中除锑[J].湿法冶金,2011,30(1):63-63. 被引量:1

6廖亚龙.高锑铅锡合金电解精炼除锑、萃取提铟工艺研究及生产实践[J].湿法冶金,2000,19(3):49-53. 被引量:9

7林茂森.阳极精炼时喷射苏打灰除去铜中的锑[J].有色冶炼,1992,21(3):14-21. 被引量:1

8伊藤研哉,游力挥.从贵铅中分别除去锑和铅的方法[J].株冶科技,1997,25(3):26-27.

9熊道陵,邱苹.甲基异丁基酮富集碘量法测金的探讨[J].南方冶金学院学报,1994,15(3):201-204.

10张耀华,陈既明.用硫化沉淀法从钽铌萃取的反铌水相中除锑[J].稀有金属与硬质合金,1994,22(2):54-57. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

MIBK has different extraction performance for Sb(Ⅲ)and Sb(Ⅴ)under certain acidity condition.Therefore,high purity niobium oxide(Sb content10×10^-6)can be obtained by controlling certain acidity and oxidizing Sb(Ⅲ)into Sb(Ⅴ)in the extraction system of HF-H2SO4-MIBK to meet the requirements of Sb extraction separation to the maximum extent.

quote

GB/T 7714-2015 [1] LIANG Chang-ming, ZHANG He-peng, GUO Yong-zhong. Experimental Research on Antimony Removal from Niobium Liquid by MIBK Extraction for Preparation of High Purity Niobium Oxide[J]. Rare Metals and Cemented Carbides, 2017(1): 1-3.
MLA [1] LIANG Chang-ming, et al., "Experimental Research on Antimony Removal from Niobium Liquid by MIBK Extraction for Preparation of High Purity Niobium Oxide." Rare Metals and Cemented Carbides, no. 1, 2017, pp. 1-3.
APA [1] LIANG Chang-ming, ZHANG He-peng, & GUO Yong-zhong. (2017). Experimental Research on Antimony Removal from Niobium Liquid by MIBK Extraction for Preparation of High Purity Niobium Oxide. Rare Metals and Cemented Carbides(1), 1-3.
IEEE [1] LIANG Chang-ming, ZHANG He-peng, and GUO Yong-zhong, "Experimental Research on Antimony Removal from Niobium Liquid by MIBK Extraction for Preparation of High Purity Niobium Oxide," Rare Metals and Cemented Carbides, no. 1, pp. 1-3, 2017. keywords: {Sb removal;niobium liquid;MIBK extraction;acidity control;oxidant;Sb(Ⅲ);Sb(Ⅴ)}