Thermodynamic Analysis of Li Extraction from Brine Using CoPO_4 Ion Sieve AITranslate
Abstract AITranslate
The Δ_fGθ of CoPO_4,Co_3(PO_4)_2 and MeCoPO_4(Me=Li,Na,K,Mg_(0.5))was estimated by congeneric linearity rule.Theφ-pH diagram of the Me-Co-P-H_2O system at 298.15 K was drawn according to the thermodynamic calculation.Thermodynamic analysis was made of lithium extraction using lithium ion battery electrode material LiCoPO_4,and the differences were discussed of adsorption behaviors between Na+,K+ or Mg2+ and Li+ in salt lake by CoPO_4.The results show that CoPO_4/LiCoPO_4 electrode is stable in aqueous solution(pH=4~11).Controlling the redox potential of the system at 0.066~0.201V(vs SHE),CoPO_4 material can absorb Li+ selectively from the natural brine containing a large number of Na+,K+ and Mg2+,and then Li+can be desorbed reversibly from lithium-inserted CoPO_4 ion sieve material by controlling the redox potential over 0.201V(vs SHE).
KeyWords AITranslate
1张荣国,杨顺林,郭丽萍,雷家珩.盐湖卤水提锂的研究进展[J].无机盐工业,2005,37(3):1-4. 被引量:19
2刘骆峰,张雨山,黄西平,张家凯,王玉琪.海水卤水提锂高效吸附剂的合成及应用研究[J].化学工业与工程,2010,27(2):138-143. 被引量:8
3肖国萍,彭洁,张钦辉,于建国.LiMn2O4离子筛成型及锂吸附性能[J].无机化学学报,2010(3):435-439. 被引量:8
4申辉,钟辉,黄溢民.离子筛型锂吸附剂的研究现状[J].四川化工,2012,15(3):19-22. 被引量:4
5孙淑英,张钦辉,于建国.纳米MnO_2离子筛的锂吸附性能[J].化工学报,2007,58(7):1757-1761. 被引量:11
6Clearfield A. Role of ion exchange in solid-state chemis- try[J]. Chemical Reviews, 1988,88 ( 1 ) -. 125-148.
7赵中伟,霍广生.Li-Mn-H_2O系热力学分析[J].中国有色金属学报,2004,14(11):1926-1933. 被引量:11
8Shin J R,Lin J R,Lee D C. Method for adsorbing lithium ions from a lithium containing aqueous solution by a Pat: 2003231996,2003-12-18.
9Onodera Y, Iwasaki T, Hayashi H, et al. Preparation method and lithium adsorption property of λ-MnO2-sili- ca composite[J]. Chemistry Letters, 1990, 19:1 801- 1 804.
10Sagara F, Ning W B, Yoshisa I,et al. Preparation and adsorption properties of λ-MnO2-cellulose hybrid-type ion-exchanger for lithium ion. Application to the en- richment of lithium ion from seawater[J]. Separation Science & Technology,1989,24(14):1 227-1 243.
1李茹,刘昉.吸附法从盐湖卤水中提取锂的研究[J].现代化工,2017,37(8):132-134. 被引量:2
1周郭宁.离子交换树脂提取锂及其影响因素的研究[J].化工管理,2022(26):62-67. 被引量:3
2胡雅茹,张东相,李子瑞.基于力场调控机制的离子分离数值仿真[J].中国粉体技术,2023,29(5):101-111.
1刘亚军.关于同系线性规律判据的讨论[J].化学研究,1998,9(4):60-62.
2李娜,刘冬冬,李洪亮.球磨法制备硅/石墨烯锂离子电池材料[J].山东化工,2016,45(2):6-7.
3贾旭宏,李丽娟,曾忠民,刘志启,张燕辉.磷酸三丁酯萃取体系从盐湖卤水提取锂[J].无机盐工业,2011,43(8):29-32. 被引量:11
4张东山.金盐生产技术研究[J].黄金,2003,24(5):4-8. 被引量:3
5汪燕鸣,朱波,刘晓玉,王飞.磷化钴对高电压LiCoPO_4正极材料电化学性能的影响[J].化工新型材料,2017,45(2):76-78. 被引量:1
6黄映恒,童张法,廖森,蓝建京,陈义族.前驱体固相反应合成LiCoPO_4纳米晶过程反应动力学[J].高校化学工程学报,2010,24(6):967-973. 被引量:3
7余朝鹤.色谱法定量校正因子和同系线性规律[J].江西石油化工,1993(1):33-34.
8司秀芬,张伟光,何利华,梁新星,赵中伟.尖晶石锰酸锂卤水提锂热力学[J].中国有色金属学报,2013,23(12):3410-3422. 被引量:4
9离子膜技术直接提取高端锂产品 盐湖卤水可制备电池级碳酸锂[J].江苏氯碱,2015,0(3):22-23.
10黄映恒,童张法,韦藤幼,李斌.固相反应合成LiCoPO_4中间体的反应动力学[J].物理化学学报,2011,27(6):1325-1334. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TQ021.2[化学工程]
Citation Information:
The Δ_fGθ of CoPO_4,Co_3(PO_4)_2 and MeCoPO_4(Me=Li,Na,K,Mg_(0.5))was estimated by congeneric linearity rule.Theφ-pH diagram of the Me-Co-P-H_2O system at 298.15 K was drawn according to the thermodynamic calculation.Thermodynamic analysis was made of lithium extraction using lithium ion battery electrode material LiCoPO_4,and the differences were discussed of adsorption behaviors between Na+,K+ or Mg2+ and Li+ in salt lake by CoPO_4.The results show that CoPO_4/LiCoPO_4 electrode is stable in aqueous solution(pH=4~11).Controlling the redox potential of the system at 0.066~0.201V(vs SHE),CoPO_4 material can absorb Li+ selectively from the natural brine containing a large number of Na+,K+ and Mg2+,and then Li+can be desorbed reversibly from lithium-inserted CoPO_4 ion sieve material by controlling the redox potential over 0.201V(vs SHE).
quote
| GB/T 7714-2015 | [1] WEN Yan-ru, HE Li-hua, LIU Xu-heng. Thermodynamic Analysis of Li Extraction from Brine Using CoPO_4 Ion Sieve[J]. Rare Metals and Cemented Carbides, 2016(2): 6-12. |
| MLA | [1] WEN Yan-ru, et al., "Thermodynamic Analysis of Li Extraction from Brine Using CoPO_4 Ion Sieve." Rare Metals and Cemented Carbides, no. 2, 2016, pp. 6-12. |
| APA | [1] WEN Yan-ru, HE Li-hua, & LIU Xu-heng. (2016). Thermodynamic Analysis of Li Extraction from Brine Using CoPO_4 Ion Sieve. Rare Metals and Cemented Carbides(2), 6-12. |
| IEEE | [1] WEN Yan-ru, HE Li-hua, and LIU Xu-heng, "Thermodynamic Analysis of Li Extraction from Brine Using CoPO_4 Ion Sieve," Rare Metals and Cemented Carbides, no. 2, pp. 6-12, 2016. keywords: {CoPO4ion sieve;LiCoPO4;Li extraction;congeneric linearity rule;thermodynamics;adsorption;brine} |