daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

From Glassy Plastic to Ductile Elastomer: Vegetable Oil-Based UV-Curable Vitrimers and Their Potential Use in 3D Printing AITranslate

Washington State University; Shanghai Jiao Tong University; Washington State University; Washington State University; Washington State University; Washington State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Current UV-curable resins based on acrylate or methacrylate monomers are mostly derived from nonrenewable petroleum feedstocks, and the cured resins are not easily repairable or reprocessable due to the stable cross-linked network. In this work, bio-based UV-curable dimethacrylate compounds are synthesized via reaction of the vegetable oil-derived dimer acid with glycidyl methacrylate. The length and flexibility of the chain segment between the two methacrylate groups are manipulated to tune the properties of the cross-linked polymer materials. The UV-cured materials exhibit a tensile strength of up to 9.2 MPa and an elongation at break of up to 66.4%. At elevated temperatures (>160 °C), the thermally induced dynamic transesterification reaction (DTER) between hydroxyl groups and ester bonds in the network structure provides repairability to the material. Use of the UV resin for three-dimensional (3D) printing is demonstrated. The printed objects exhibit unique welding and shape-changing properties owing to the thermally induced DTER. This work integrates the concepts of UV curing, vitrimer preparation, 3D printing, and bio-based polymers, demonstrating a feasible approach for the sustainable design of polymer materials.

KeyWords AITranslate

vitrimer biocontent dynamic transesterification UV curable 3D printing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00063

Chinese Library Classification Number:

Citation Information:

Current UV-curable resins based on acrylate or methacrylate monomers are mostly derived from nonrenewable petroleum feedstocks, and the cured resins are not easily repairable or reprocessable due to the stable cross-linked network. In this work, bio-based UV-curable dimethacrylate compounds are synthesized via reaction of the vegetable oil-derived dimer acid with glycidyl methacrylate. The length and flexibility of the chain segment between the two methacrylate groups are manipulated to tune the properties of the cross-linked polymer materials. The UV-cured materials exhibit a tensile strength of up to 9.2 MPa and an elongation at break of up to 66.4%. At elevated temperatures (>160 °C), the thermally induced dynamic transesterification reaction (DTER) between hydroxyl groups and ester bonds in the network structure provides repairability to the material. Use of the UV resin for three-dimensional (3D) printing is demonstrated. The printed objects exhibit unique welding and shape-changing properties owing to the thermally induced DTER. This work integrates the concepts of UV curing, vitrimer preparation, 3D printing, and bio-based polymers, demonstrating a feasible approach for the sustainable design of polymer materials.

quote

GB/T 7714-2015 [1] Mingen Fei, Tuan Liu, Baoming Zhao, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00063.
MLA [1] Mingen Fei, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00063.
APA [1] Mingen Fei, Tuan Liu, Baoming Zhao, Anthony Otero, YuChung Chang, & Jinwen Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00063
IEEE [1] Mingen Fei, Tuan Liu, Baoming Zhao, Anthony Otero, YuChung Chang, and Jinwen Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00063. keywords: {vitrimer;biocontent;dynamic transesterification;UV curable;3D printing}