Solid-Phase Microcontact Printing for Precise Patterning of Rough Surfaces: Using Polymer-Tethered Elastomeric Stamps for the Transfer of Reactive Silanes AITranslate

University of Potsdam;Fraunhofer Institute for Applied Polymer Research (IAP) Geiselbergstr. 69; University of Potsdam; University of Potsdam;Fraunhofer Institute for Applied Polymer Research (IAP) Geiselbergstr. 69; University of Potsdam;Fraunhofer Institute for Applied Polymer Research (IAP) Geiselbergstr. 69;Fraunhofer Institute for Applied Polymer Research (IAP) Geiselbergstr. 69
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We present a microcontact printing (μCP) routine suitable to introduce defined (sub-) microscale patterns on surface substrates exhibiting a high capillary activity and receptive to a silane-based chemistry. This is achieved by transferring functional trivalent alkoxysilanes, such as (3-aminopropyl)-triethoxysilane (APTES) as a low-molecular weight ink via reversible covalent attachment to polymer brushes grafted from elastomeric polydimethylsiloxane (PDMS) stamps. The brushes consist of poly{N-[tris(hydroxymethyl)-methyl]acrylamide} (PTrisAAm) synthesized by reversible addition–fragmentation chain-transfer (RAFT)-polymerization and used for immobilization of the alkoxysilane-based ink by substituting the alkoxy moieties with polymer-bound hydroxyl groups. Upon physical contact of the silane-carrying polymers with surfaces, the conjugated silane transfers to the substrate, thus completely suppressing ink-flow and, in turn, maximizing printing accuracy even for otherwise not addressable substrate topographies. We provide a concisely conducted investigation on polymer brush formation using atomic force microscopy (AFM) and ellipsometry as well as ink immobilization utilizing two-dimensional proton nuclear Overhauser enhancement spectroscopy (1H–1H-NOESY-NMR). We analyze the μCP process by printing onto Si-wafers and show how even distinctively rough surfaces can be addressed, which otherwise represent particularly challenging substrates.

KeyWords AITranslate

microcontact printing capillaryactive substrates silane chemistry PDMS surface grafting surface patterning shuttled Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00024

Chinese Library Classification Number:

Citation Information:

We present a microcontact printing (μCP) routine suitable to introduce defined (sub-) microscale patterns on surface substrates exhibiting a high capillary activity and receptive to a silane-based chemistry. This is achieved by transferring functional trivalent alkoxysilanes, such as (3-aminopropyl)-triethoxysilane (APTES) as a low-molecular weight ink via reversible covalent attachment to polymer brushes grafted from elastomeric polydimethylsiloxane (PDMS) stamps. The brushes consist of poly{N-[tris(hydroxymethyl)-methyl]acrylamide} (PTrisAAm) synthesized by reversible addition–fragmentation chain-transfer (RAFT)-polymerization and used for immobilization of the alkoxysilane-based ink by substituting the alkoxy moieties with polymer-bound hydroxyl groups. Upon physical contact of the silane-carrying polymers with surfaces, the conjugated silane transfers to the substrate, thus completely suppressing ink-flow and, in turn, maximizing printing accuracy even for otherwise not addressable substrate topographies. We provide a concisely conducted investigation on polymer brush formation using atomic force microscopy (AFM) and ellipsometry as well as ink immobilization utilizing two-dimensional proton nuclear Overhauser enhancement spectroscopy (1H–1H-NOESY-NMR). We analyze the μCP process by printing onto Si-wafers and show how even distinctively rough surfaces can be addressed, which otherwise represent particularly challenging substrates.

quote

GB/T 7714-2015 [1] Pinar Akarsu, Richard Grobe, Julius Nowaczyk, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00024.
MLA [1] Pinar Akarsu, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00024.
APA [1] Pinar Akarsu, Richard Grobe, Julius Nowaczyk, Matthias Hartlieb, Stefan Reinicke, Alexander Böker, Marcel Sperling, & Martin Reifarth. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00024
IEEE [1] Pinar Akarsu, Richard Grobe, Julius Nowaczyk, Matthias Hartlieb, Stefan Reinicke, Alexander Böker, Marcel Sperling, and Martin Reifarth, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00024. keywords: {microcontact printing;capillaryactive substrates;silane chemistry;PDMS surface grafting;surface patterning;shuttled;Show More}