Synthesis, Curing, and Thermal Stability of Low-Temperature-Cured Benzoxazine Resins Based on Natural Renewable Resources AITranslate
Abstract AITranslate
For curing bio-based benzoxazine monomers completely below 200 °C, bio-based phloretic acid (PHA), p-coumaric acid (pCOA), and ferulic acid (FEA) containing a carboxylic group as a phenol source and furfurylamine (FA) as an amine source are used to prepare three full bio-based benzoxazines (PHA-fa, pCOA-fa, and FEA-fa). Differential scanning calorimetry experimental results showed that PHA-fa, pCOA-fa, and FEA-fa possessed low ring-opening polymerization temperatures and △H values and could be cured completely below 200 °C. The obtained full bio-based polybenzoxazines (poly(PHA-fa), poly(pCOA-fa), and poly(FEA-fa)) presented lower decomposition rates and higher residual char at 800 °C. In addition, poly(PHA-fa), poly(pCOA-fa), and poly(FEA-fa) were predicted to have good flame retardancy due to low heat release capacity and total heat release values. From the above results, it is known that natural renewable resources, PHA, pCOA, FEA, and FA, contribute to obtaining high-performance bio-based thermosets with excellent low-temperature curing performance and high char at 800 °C, which make them suitable for applications of plant fiber-reinforced composites.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00361
Chinese Library Classification Number:
Citation Information:
For curing bio-based benzoxazine monomers completely below 200 °C, bio-based phloretic acid (PHA), p-coumaric acid (pCOA), and ferulic acid (FEA) containing a carboxylic group as a phenol source and furfurylamine (FA) as an amine source are used to prepare three full bio-based benzoxazines (PHA-fa, pCOA-fa, and FEA-fa). Differential scanning calorimetry experimental results showed that PHA-fa, pCOA-fa, and FEA-fa possessed low ring-opening polymerization temperatures and △H values and could be cured completely below 200 °C. The obtained full bio-based polybenzoxazines (poly(PHA-fa), poly(pCOA-fa), and poly(FEA-fa)) presented lower decomposition rates and higher residual char at 800 °C. In addition, poly(PHA-fa), poly(pCOA-fa), and poly(FEA-fa) were predicted to have good flame retardancy due to low heat release capacity and total heat release values. From the above results, it is known that natural renewable resources, PHA, pCOA, FEA, and FA, contribute to obtaining high-performance bio-based thermosets with excellent low-temperature curing performance and high char at 800 °C, which make them suitable for applications of plant fiber-reinforced composites.
quote
| GB/T 7714-2015 | [1] Hongqiang Yan, Zuomin Zhan, Huaqing Wang, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00361. |
| MLA | [1] Hongqiang Yan, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00361. |
| APA | [1] Hongqiang Yan, Zuomin Zhan, Huaqing Wang, Jie Cheng, & Zhengping Fang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00361 |
| IEEE | [1] Hongqiang Yan, Zuomin Zhan, Huaqing Wang, Jie Cheng, and Zhengping Fang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00361. keywords: {full biobased benzoxazine;synthesis;lowtemperature curing performance;thermal stability;flame retardancy} |