Hybrid Magnetic Hydrogels Used as Artificial Marine Animals for Noncontact Cleaning AITranslate
Abstract AITranslate
Here, we developed a one-step method to prepare a highly tough and magnetic (1.2 emu g–1) polyacrylamide-Fe3O4-alginate (PAAM-Fe3O4-ALG) double-network hydrogel. Magnetic Fe3O4 nanoparticles (MNPs) were intercalated into the double network, producing Fe3O4-intercalated hydrogels with ferromagnetism. These kinds of magnetic hydrogels are endowed with good mechanical properties, such as high tensile strength (90 kPa) and superior compressive strength (0.9 MPa). Although such gels contain 20 mg mL–1 magnetic nanoparticles, they could still be stretched more than eight times their original length. The noncontact soft robot, which is a magnetically driven hydrogel, was demonstrated. Two typical soft robots (a scallop and a starfish) were prepared with magnetic hydrogels. Under external magnetic stimulation, these soft robotic marine animals could clean a fish tank without the help of a hand in the water. This approach will extend the application of hydrogels in various fields, such as controlled drug delivery, underwater cleaning robots, and other integrated hydrogel devices.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00019
Chinese Library Classification Number:
Citation Information:
Here, we developed a one-step method to prepare a highly tough and magnetic (1.2 emu g–1) polyacrylamide-Fe3O4-alginate (PAAM-Fe3O4-ALG) double-network hydrogel. Magnetic Fe3O4 nanoparticles (MNPs) were intercalated into the double network, producing Fe3O4-intercalated hydrogels with ferromagnetism. These kinds of magnetic hydrogels are endowed with good mechanical properties, such as high tensile strength (90 kPa) and superior compressive strength (0.9 MPa). Although such gels contain 20 mg mL–1 magnetic nanoparticles, they could still be stretched more than eight times their original length. The noncontact soft robot, which is a magnetically driven hydrogel, was demonstrated. Two typical soft robots (a scallop and a starfish) were prepared with magnetic hydrogels. Under external magnetic stimulation, these soft robotic marine animals could clean a fish tank without the help of a hand in the water. This approach will extend the application of hydrogels in various fields, such as controlled drug delivery, underwater cleaning robots, and other integrated hydrogel devices.
quote
| GB/T 7714-2015 | [1] Qiang Cao, Na Liu, Yushi Xiao, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00019. |
| MLA | [1] Qiang Cao, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00019. |
| APA | [1] Qiang Cao, Na Liu, Yushi Xiao, Rong Huang, Yang Li, & Lidong Wu. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00019 |