Study on Electrical Conductivity of Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO Molten Salt System AITranslate
Abstract AITranslate
The resistance was measured of Na3AlF6-AlF3-LiF-MgF2-Al2O3-Nd2O3-CuO molten salt system with TH2810 DLCR digital bridge tester,and then its electrical conductivity was tested by CVCC technique.Meanwhile,the regression equation including temperature,composition and electrical conductivity of the molten salt was developed by data fitting with the least square method.The results show that the molten salt conductivity increases with the increase of temperature or CuO content,but decreases with Nd2O3 and Al2O3content increasing.Simultaneously adding Nd2O3 and CuO of the same mass ratio at a certain temperature,the electrical conductivity of molten salt system increases with the increase of Nd2O3 and CuO content.
KeyWords AITranslate
1于旭光,邱竹贤.熔盐电解制备稀土铝合金的研究[J].稀土,2006,27(6):33-36. 被引量:10
2郭探,王世栋,叶秀深,李权,刘海宁,郭敏,吴志坚.熔盐电解法制备稀土合金研究进展[J].中国科学:化学,2012,42(9):1328-1336. 被引量:40
3王兆文,胡宪伟,高炳亮,石忠宁.CVCC法测定冰晶石系熔盐电导率的应用研究[J].东北大学学报:自然科学版,2006,27(7):786-789. 被引量:22
4于亚鑫,邱竹贤,杨宝刚,黄慧麟.NaF-AlF_3-CaF_2-LiF-Al_2O_3系电导率的研究[J].中国有色金属学报,1998,8(S2):458-460. 被引量:4
5马秀芳,张世荣,李德祥,李国华.Na_3AlF_6-AlF_3-LiF-CaF_2系熔体变温电导率的研究[J].有色金属,1998,50(4):77-81. 被引量:10
6Grjotheim K, Krohn C, Malinovsky M, et al. Aluminium Electrolysis, (2nd edition)[M]. Dusseldorf: Aluminium- Verlag, 1982.131.
7Matiasovsky K,Danek V, Malinovsky M. Effect of LiF and Li3 A1F6 on the electrical conductivity of cryolite-alu- mina melts[J]. Journal of the Electrochemical Society, 1969,116(10):1 381-1 383.
8李学舜,冯法伦,魏绪钧,徐秀芝.氟盐体系电解富镧钕合金熔盐电导率的研究[J].稀土,1998,19(1):33-35. 被引量:4
9曾水平,蔡祺凤,李荐,单勇.2.1NaF·AlF_3─NaCl─MgF_2熔盐体系初晶点及电导率的研究[J].轻金属,1994(8):30-32. 被引量:4
10黄有国,田忠良,赖延清,李庆余.铝电解质熔体电导率研究进展[J].轻金属,2008(6):28-32. 被引量:7
1Chun-fa Liao,Yun-fen Jiao,Xu Wang,Bo-qing Cai,Qiang-chao Sun,Hao Tang.Electrical conductivity optimization of the Na3AlF6–Al2O3–Sm2O3 molten salts system for Al–Sm intermediate binary alloy production[J].矿物冶金与材料学报:英文版,2017,0(9):1034-1042. 被引量:4
2宗国强,肖吉昌.氟化物熔盐的制备及其应用进展[J].化工进展,2018,37(7):2455-2472. 被引量:7
3冷欣伟,汤浩,廖春发,王旭.熔盐电解制备Al-Cu-Y合金电解质体系黏度的研究[J].有色金属科学与工程,2019,10(5):8-11. 被引量:2
4陈淑梅,洪侃,伍昕宇,梁鑫,廖春发,陈东英.LiF-LaF3-La2O3熔盐体系的电导率[J].中国有色金属学报,2020,30(10):2427-2434. 被引量:1
1廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4
2Shu-mei Chen,Chun-fa Liao,Jue-yuan Lin,Bo-qing Cai,Xu Wang,Yun-fen Jiao.Electrical conductivity of molten LiF–DyF3–Dy2O3–Cu2O system for Dy–Cu intermediate alloy production[J].矿物冶金与材料学报:英文版,2019,26(6):701-709. 被引量:1
3贾雷,严红燕,李慧,刘畅,张帅.熔盐电解精炼制备高纯铪工艺研究进展[J].矿产综合利用,2020,0(1):33-38. 被引量:1
4Xiaoping Zhu,Shuchen Sun,Ting Sun,Chuan Liu,Ganfeng Tu,Jiayue Zhang.Electrical conductivity of REF3-LiF(RE=La and Nd) molten salts[J].稀土学报:英文版,2020,38(6):676-682. 被引量:1
5陈淑梅,洪侃,伍昕宇,梁鑫,廖春发,陈东英.LiF-LaF3-La2O3熔盐体系的电导率[J].中国有色金属学报,2020,30(10):2427-2434. 被引量:1
6Xiao-li,Ming Feng,Li-wen Zhang,Zuo-ren Nie.Applications of molten salt and progress of molten salt electrolysis in secondary metal resource recovery[J].矿物冶金与材料学报:英文版,2020,27(12):1599-1617. 被引量:3
7Jun-xiang Wang,Ji-guo Tu,Han-dong Jiao,d Hong-min Zhu.Nanosheet-stacked flake graphite for high-performance Al storage in inorganic molten AlCl_(3)-NaCl salt[J].矿物冶金与材料学报:英文版,2020,27(12):1711-1722. 被引量:1
8康佳,于兵,黄海涛,张全军,刘玉宝,闫奇操.LiF-YF3-Y2O3体系密度与表面张力的研究[J].有色金属:冶炼部分,2020(11):89-94. 被引量:2
9徐家聪,喻小强,吴选高,龚傲,徐志峰,田磊.氟化稀土熔盐电解渣硫酸浸出脱氟研究[J].有色金属科学与工程,2020,11(6):1-9. 被引量:5
10宗国强,向绍基,崔振华,王荣荣,陆人杰,张婷,肖吉昌.核纯级^(7)LiF的制备[J].化学研究与应用,2021,33(11):2240-2246.
1郑鑫,朱卫花,彭光怀,梁金,张小联.NdF_3-LiF-Nd_2O_3体系熔盐电导率的研究[J].中国钨业,2013,28(1):30-33. 被引量:7
2胡宪伟,王兆文,高炳亮,石忠宁.NdF3-LiF-Nd2O3系熔盐电导率的CVCC法研究[J].东北大学学报:自然科学版,2008,29(9):1294-1297. 被引量:11
3章珏,郑鑫,梁金,刘红霞,彭光怀,张小联.NdF_3-LiF-Nd_2O_3体系熔盐电导率影响因素的研究[J].稀有金属与硬质合金,2014,42(4):17-21. 被引量:4
4王兆文,胡宪伟,高炳亮,石忠宁.CVCC法测定冰晶石系熔盐电导率的应用研究[J].东北大学学报:自然科学版,2006,27(7):786-789. 被引量:22
5廖春发,王坤,王旭,杨少华,房孟钊.NaCl-CaCl_2-CaWO_4熔盐体系电导率的研究[J].有色金属科学与工程,2013,4(5):19-22. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF111[冶金工程—冶金物理化学]
Citation Information:
The resistance was measured of Na3AlF6-AlF3-LiF-MgF2-Al2O3-Nd2O3-CuO molten salt system with TH2810 DLCR digital bridge tester,and then its electrical conductivity was tested by CVCC technique.Meanwhile,the regression equation including temperature,composition and electrical conductivity of the molten salt was developed by data fitting with the least square method.The results show that the molten salt conductivity increases with the increase of temperature or CuO content,but decreases with Nd2O3 and Al2O3content increasing.Simultaneously adding Nd2O3 and CuO of the same mass ratio at a certain temperature,the electrical conductivity of molten salt system increases with the increase of Nd2O3 and CuO content.
quote
| GB/T 7714-2015 | [1] LIAO Chun-fa, TANG Hao, WANG Xu, et al. Study on Electrical Conductivity of Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO Molten Salt System[J]. Rare Metals and Cemented Carbides, 2016(1): 60-64. |
| MLA | [1] LIAO Chun-fa, et al., "Study on Electrical Conductivity of Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO Molten Salt System." Rare Metals and Cemented Carbides, no. 1, 2016, pp. 60-64. |
| APA | [1] LIAO Chun-fa, TANG Hao, WANG Xu, LUO Lin-sheng, & FANG Meng-zhao. (2016). Study on Electrical Conductivity of Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO Molten Salt System. Rare Metals and Cemented Carbides(1), 60-64. |
| IEEE | [1] LIAO Chun-fa, TANG Hao, WANG Xu, LUO Lin-sheng, and FANG Meng-zhao, "Study on Electrical Conductivity of Na_3AlF_6-AlF_3-LiF-MgF_2-Al_2O_3-Nd_2O_3-CuO Molten Salt System," Rare Metals and Cemented Carbides, no. 1, pp. 60-64, 2016. keywords: {Na3AlF6-AlF3-LiF-MgF2-Al2O3-Nd2O3-CuO;molten salt system;CVCC technique;electrical conductivity;regression equation} |