Research on the Process of Preparing High-Purity Ammonium Dimolybdate from Industrial Molybdenum Oxide by Extraction Method AITranslate

Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.;Jinduicheng Molybdenum Industry Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of the current situation of low-purity of ammonium dimolybdate prepared by existing ex-traction processes from industrial molybdenum oxide,the process of extracting and purifying industrial mo-lybdenum oxide alkaline leachate with primary amine N1923 was investigated,and the effects of various ex-traction and stripping conditions on Mo extraction rate,stripping rate,and ammonium dimolybdate purity were explored.The results show that under the optimized single-stage extraction conditions of room tem-perature,pH value adjustment of the alkaline leachate to 4 through sulfuric acid addition,organic phase composition of 40%N1923+20%isoamyl alcohol+40%sulfonated kerosene,O/A ratio of 1∶1,and extraction time of 3 min,the Mo extraction rate exceeds 94%.Under the conditions of 9%ammonia solu-tion as the stripping agent,O/A ratio of 3∶1,three-stage stripping,room temperature,and stripping time of 3 min,the Mo stripping rate reaches 98%.Ammonium dimolybdate product with a purity of up to 99.99%is obtained by evaporating and crystallizing the stripping solution.However,due to its high tung-sten content,further targeted tungsten removal is required in subsequent steps.

KeyWords AITranslate

N1923 industrial molybdenum oxide extraction stripping ammonium dimolybdate
No data

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程]

Citation Information:

In view of the current situation of low-purity of ammonium dimolybdate prepared by existing ex-traction processes from industrial molybdenum oxide,the process of extracting and purifying industrial mo-lybdenum oxide alkaline leachate with primary amine N1923 was investigated,and the effects of various ex-traction and stripping conditions on Mo extraction rate,stripping rate,and ammonium dimolybdate purity were explored.The results show that under the optimized single-stage extraction conditions of room tem-perature,pH value adjustment of the alkaline leachate to 4 through sulfuric acid addition,organic phase composition of 40%N1923+20%isoamyl alcohol+40%sulfonated kerosene,O/A ratio of 1∶1,and extraction time of 3 min,the Mo extraction rate exceeds 94%.Under the conditions of 9%ammonia solu-tion as the stripping agent,O/A ratio of 3∶1,three-stage stripping,room temperature,and stripping time of 3 min,the Mo stripping rate reaches 98%.Ammonium dimolybdate product with a purity of up to 99.99%is obtained by evaporating and crystallizing the stripping solution.However,due to its high tung-sten content,further targeted tungsten removal is required in subsequent steps.

quote

GB/T 7714-2015 [1] DUAN Lin-lin, ZHANG Shu-jia, BU Chun-yang, et al. Research on the Process of Preparing High-Purity Ammonium Dimolybdate from Industrial Molybdenum Oxide by Extraction Method[J]. Rare Metals and Cemented Carbides, 2025(4): 1-7.
MLA [1] DUAN Lin-lin, et al., "Research on the Process of Preparing High-Purity Ammonium Dimolybdate from Industrial Molybdenum Oxide by Extraction Method." Rare Metals and Cemented Carbides, no. 4, 2025, pp. 1-7.
APA [1] DUAN Lin-lin, ZHANG Shu-jia, BU Chun-yang, QU Kun, QU Hang, NIU Shuai, LI Sen, & ZHANG Ling-yun. (2025). Research on the Process of Preparing High-Purity Ammonium Dimolybdate from Industrial Molybdenum Oxide by Extraction Method. Rare Metals and Cemented Carbides(4), 1-7.
IEEE [1] DUAN Lin-lin, ZHANG Shu-jia, BU Chun-yang, QU Kun, QU Hang, NIU Shuai, LI Sen, and ZHANG Ling-yun, "Research on the Process of Preparing High-Purity Ammonium Dimolybdate from Industrial Molybdenum Oxide by Extraction Method," Rare Metals and Cemented Carbides, no. 4, pp. 1-7, 2025. keywords: {N1923;industrial molybdenum oxide;extraction;stripping;ammonium dimolybdate}