Electronic and Chemical Properties of Nickel Oxide Thin Films and the Intrinsic Defects Compensation Mechanism Electronic and Chemical Properties of Nickel Oxide Thin Films and the Intrinsic Defects Compensation Mechanism AITranslate
Abstract AITranslate
Although largely studied, contradictory results on nickel oxide (NiO) properties can be found in the literature. We herein propose a comprehensive study that aims at leveling contradictions related to NiO materials with a focus on its conductivity, surface properties, and the intrinsic charge defects compensation mechanism with regards to the conditions preparation. The experiments were performed by in situ photoelectron spectroscopy, electron energy loss spectroscopy, and optical as well as electrical measurements on polycrystalline NiO thin films prepared under various preparation conditions by reactive sputtering. The results show that surface and bulk properties were strongly related to the deposition temperature with in particular the observation of Fermi level pinning, high work function, and unstable oxygen-rich grain boundaries for the thin films produced at room temperature but not at high temperature (>200 °C). Finally, this study provides substantial information about surface and bulk NiO properties enabling to unveil the origin of the high electrical conductivity of room temperature NiO thin films and also for supporting a general electronic charge compensation mechanism of intrinsic defects according to the deposition temperature.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c00230
Chinese Library Classification Number:
Citation Information:
Although largely studied, contradictory results on nickel oxide (NiO) properties can be found in the literature. We herein propose a comprehensive study that aims at leveling contradictions related to NiO materials with a focus on its conductivity, surface properties, and the intrinsic charge defects compensation mechanism with regards to the conditions preparation. The experiments were performed by in situ photoelectron spectroscopy, electron energy loss spectroscopy, and optical as well as electrical measurements on polycrystalline NiO thin films prepared under various preparation conditions by reactive sputtering. The results show that surface and bulk properties were strongly related to the deposition temperature with in particular the observation of Fermi level pinning, high work function, and unstable oxygen-rich grain boundaries for the thin films produced at room temperature but not at high temperature (>200 °C). Finally, this study provides substantial information about surface and bulk NiO properties enabling to unveil the origin of the high electrical conductivity of room temperature NiO thin films and also for supporting a general electronic charge compensation mechanism of intrinsic defects according to the deposition temperature.
quote
| GB/T 7714-2015 | [1] Raphaël Poulain, Gunnar Lumbeeck, Jonas Hunka, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00230. |
| MLA | [1] Raphaël Poulain, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00230. |
| APA | [1] Raphaël Poulain, Gunnar Lumbeeck, Jonas Hunka, Joris Proost, Henri Savolainen, Hosni Idrissi, Dominique Schryvers, Nicolas Gauquelin, & Andreas Klein. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00230 |
| IEEE | [1] Raphaël Poulain, Gunnar Lumbeeck, Jonas Hunka, Joris Proost, Henri Savolainen, Hosni Idrissi, Dominique Schryvers, Nicolas Gauquelin, and Andreas Klein, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00230. keywords: {nickel oxide defects compensation conductivity grain boundaries Fermi level photoelectron spectroscopy} |