daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on a New Process of Tungsten Recovery from Tungsten Slag AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper presents a systematical study on a new process of tungsten recovery from tungsten slag. The tungsten leaching rate reaches more than 860/00 with 1% additive A,20% hydrochloric acid mass fraction, 100℃acid leaching temperature,3 h leaching time and 3 : 1 liquid-solid ratio. Moreover,tungsten and other valuable metals could be well separated by ion exchange of weakly basic anion exchange resin and purification process. The process is characterized by reasonable product structure, high recovery, less inrcial operation and quick effect with very good industrial application prospect.

KeyWords AITranslate

tungsten slag hydrochloric acid acid leaching sodium tungstate ion exchange recovery

1肖超,刘景槐,吴海国.低品位钨渣处理工艺试验研究[J].湖南有色金属,2012,28(4):24-26. 被引量:19

2朱海玲,邓海波,吴承桧,何小民.钨渣的综合回收利用技术研究现状[J].中国钨业,2010,25(4):15-18. 被引量:25

3戴艳阳,钟晖,钟海云.钨渣回收制备四氧化三锰新工艺[J].中国有色金属学报,2012,22(4):1242-1247. 被引量:18

4杨利群.苏打烧结法处理低品位钨矿及废钨渣的研究[J].中国钼业,2008,32(4):25-27. 被引量:31

5张立,钟晖,戴艳阳.钨渣酸浸与钠碱熔融回收钽铌的研究[J].稀有金属与硬质合金,2008,36(2):6-9. 被引量:21

6钟学明.从钨渣中提取氧化钪的工艺研究[J].江西冶金,2002,22(3):19-22. 被引量:24

7镲光宪.稀土(上册)[M].北京:冶金工业出版社,1995.

8赵天从.有色金属提取冶金手册:稀有高熔点金属(W、Mo、Re、Ti)[M].北京:冶金工业出版社,1999.

9蒋汉赢.湿法冶金过程物理化学[M].北京:冶金工业出版社,1984.

1杨少华,王君,谢宝如,赖晓晖,王浩然.低品位钨渣处理工艺[J].有色金属科学与工程,2015,6(6):29-32. 被引量:10

2谢建清.钨渣回收利用技术研究现状[J].中国钨业,2019,34(1):50-57. 被引量:5

3朱心蕊,刘旭恒,陈星宇,李江涛,何利华,赵中伟.钨冶炼渣的综合利用及发展趋势[J].矿产保护与利用,2019,39(3):119-124. 被引量:9

4范科彪,郑雅杰,王钫,李海波.电解回收铁钨锡合金粉中的铁[J].中国有色金属学报,2019,29(10):2421-2432. 被引量:3

5郭少毓,霍瑞浩,谢岁,王良辉,郭超,廖春发.碱煮钨渣综合回收利用研究进展[J].稀有金属与硬质合金,2021,49(5):1-6. 被引量:1

6廖春发,王良辉,霍瑞浩,谢岁,郭少毓,刘德刚.碱煮黑钨渣还原熔炼回收有价金属的研究[J].稀有金属与硬质合金,2021,49(5):7-12.

7Xu Wang,Xiao‑Dong Ma,Kun Su,Chun‑Fa Liao,Bao‑Jun Zhao.Fundamental studies for high temperature processing of tungsten leaching residues for alloy formation[J].钨科技(英文),2020,2(4):362-370.

8龚丹丹,李祖怡,张勇,万林生,任嗣利.钨渣回收利用技术研究现状[J].稀有金属与硬质合金,2021,49(6):1-8. 被引量:2

9彭映林,范科彪,郑雅杰.铁钨锡合金粉电解的阳极行为[J].中国有色金属学报,2022,32(1):227-235.

10张金祥,罗教生,管建红,洪侃,黄叶钿,普建,李忠岐,陈远林,郭学益.我国钨渣处理现状与研究进展[J].中国钨业,2021,36(6):62-70.

1杨俊彦,齐申,刘海,王文科,黄景存,张建东,车小奎,宋波,王力军.钨冶炼渣综合回收利用的研究进展[J].工程科学学报,2018,40(12):1468-1475. 被引量:5

2李林山,杨少华,赵宇娟,王昭文.CP熔盐电化学方法检测LiCl-KCl熔盐La(Ⅲ)浓度[J].有色金属科学与工程,2017,8(6):1-6. 被引量:2

3何艺,徐双,靳晓勤,林晓,陶莉,许海青.中国钨渣产生特性及资源化利用技术研究现状[J].中国钨业,2018,33(5):51-56. 被引量:8

4朱心蕊,刘旭恒,陈星宇,李江涛,何利华,赵中伟.钨冶炼渣的综合利用及发展趋势[J].矿产保护与利用,2019,39(3):119-124. 被引量:9

5余春荣,黄亮,徐双,李跃海,陆晓晖.钨渣脱水过程中加压过滤机的应用实践[J].中国钨业,2019,34(6):43-47.

6范泽坤,黄超,徐国钻,杨正锋,胡家园,唐孝江,梁勇.钨冶炼渣酸分解减量资源化实验研究[J].稀有金属与硬质合金,2020,48(2):1-4. 被引量:4

7鲁东,喻文斌,王诗海,张伟宁,郭洪范.钨在氟铌酸溶液中的沉淀行为研究[J].云南冶金,2020,49(5):38-40.

8吴昊,曾欣荣,刘宏博,王庆旭,黄楠楠,王雪娇,田书磊.我国钨渣管理存在的问题及建议[J].硬质合金,2020,37(6):460-465. 被引量:1

9王博,陈朝轶,李军旗,王林珠,兰苑培,王仕愈,申园园.阴极改性对含钛废渣电脱氧过程的影响[J].中国有色金属学报,2021,31(2):470-478.

10马兵,杜布云,严小飞,康国栋.钨渣制备玻璃化产物危险特性与力学性能研究[J].生态与农村环境学报,2021,37(9):1218-1224.

1我国应大力发展不锈钢炼钢生产[J].武钢技术,2004,42(6):58-58.

2李青刚,曾理,艾馨鹏,肖连生,张启修.一种弱碱性阴离子树脂对石煤浸出液中钒的吸附形态研究[J].稀有金属,2007,31(S1):64-69. 被引量:6

3张展雷,于恒,宋志芳,周成科,余正伟,周峰,刘臣.钒钛磁铁精矿复合造块试验研究[J].烧结球团,2014,39(4):1-5. 被引量:3

4林纲,边全胜.碳化铁—一种新型炼钢原料[J].国外钢铁,1994,19(8):16-20. 被引量:1

5刘丹,贺昕,熊晓东.离子交换法深度除杂制备高纯钴的研究[J].稀有金属,2013,37(1):112-115. 被引量:8

6孙宁磊,戴江洪,殷书岩,李少龙.赤铁矿沉淀除铁工艺产品化学质量的影响因素探讨[J].有色冶金节能,2015,31(2):11-13. 被引量:1

7刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4

8黄威,杨磊,徐渊.硫氰酸盐对弱碱性阴离子树脂的吸附影响[J].新疆有色金属,2003,26(S2):45-47.

9张晓东,成肇安.用Swc树脂提取钼的研究[J].中国钼业,1997,21(1):26-27. 被引量:4

10卢国贤,袁爱群,周泽广,黄增尉,韦冬萍,马少妹.2种回转窑工艺还原低品位软锰矿的效果评价[J].中国锰业,2014,32(3):25-29. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]

Citation Information:

This paper presents a systematical study on a new process of tungsten recovery from tungsten slag. The tungsten leaching rate reaches more than 860/00 with 1% additive A,20% hydrochloric acid mass fraction, 100℃acid leaching temperature,3 h leaching time and 3 : 1 liquid-solid ratio. Moreover,tungsten and other valuable metals could be well separated by ion exchange of weakly basic anion exchange resin and purification process. The process is characterized by reasonable product structure, high recovery, less inrcial operation and quick effect with very good industrial application prospect.

quote

GB/T 7714-2015 [1] SU Zheng-fu, LIU Yu-hui. Study on a New Process of Tungsten Recovery from Tungsten Slag[J]. Rare Metals and Cemented Carbides, 2014(4): 11-13.
MLA [1] SU Zheng-fu, and LIU Yu-hui. "Study on a New Process of Tungsten Recovery from Tungsten Slag." Rare Metals and Cemented Carbides, no. 4, 2014, pp. 11-13.
APA [1] SU Zheng-fu, & LIU Yu-hui. (2014). Study on a New Process of Tungsten Recovery from Tungsten Slag. Rare Metals and Cemented Carbides(4), 11-13.
IEEE [1] SU Zheng-fu and LIU Yu-hui, "Study on a New Process of Tungsten Recovery from Tungsten Slag," Rare Metals and Cemented Carbides, no. 4, pp. 11-13, 2014. keywords: {tungsten slag;hydrochloric acid;acid leaching;sodium tungstate;ion exchange;recovery}