Study on Microstructure and Texture Evolution Law of Beryllium during Warm-rolling AITranslate
Abstract AITranslate
The texture and microstructure evolution law of hot-pressed sintered beryllium ingot during warm-rolling was studied by electron backscatter diffraction (EBSD). The results show that slip is the main deformation mechanism during warm-rolling. With the increase of rolling deformation, the grains are gradually elongated and refined. When the reduction reaches 37.9%, the basal texture in rolled beryllium sheet reaches a maximum value. And then continuously increasing the reduction, all the texture, grain size and mierohardness of beryllium material no longer change significantly. The annealing process is required during or after rolling of beryllium material. The annealing process has a certain weakening effect on the basal texture of beryllium sheet,which can improve its internal microstructure and rolling performance.
KeyWords AITranslate
1钟景明,许德美,李春光,王战宏,李峰,王莉,李志年.金属铍的应用进展[J].中国材料进展,2014,33(9):568-575. 被引量:18
2王维一,刘兆刚.国内铍箔轧制技术研究[J].湖南有色金属,2015,31(5):57-60. 被引量:2
3王丽娜,杨平,夏伟军,陈振华,陈鼎,李萧,孟利.特殊成形工艺下AZ31镁合金的织构及变形机制[J].金属学报,2009,45(1):58-62. 被引量:13
4黄文,汪洋,李子然,夏源明.温度和应变率对多晶纯钛孪晶变形的影响[J].中国有色金属学报,2008,18(8):1440-1445. 被引量:17
1吕一格,代彦明,刘兆刚,李志年,赵志灵,张健康,魏冬冬.热挤压对铍铝合金显微组织和性能的影响研究[J].稀有金属与硬质合金,2019,47(5):60-63. 被引量:3
2吕一格,张健康,代彦明,李美岁,赵志灵,李志年,李军义,魏冬冬.62Be-38Al合金高、低温力学性能及断裂机制[J].稀有金属与硬质合金,2020,48(3):73-76. 被引量:2
3王维一,徐平,王蓓,张子富,刘宁.铍材轧制过程温度对其塑性及显微组织的影响[J].稀有金属与硬质合金,2022,50(3):78-81.
4王维一,徐平,张子富,邵伟,田青,刘宁,司祎.制备工艺对铍锭轧制性能及效果的影响[J].稀有金属与硬质合金,2023,51(2):85-89.
1吕一格,张健康,代彦明,李美岁,赵志灵,李志年,李军义,魏冬冬.62Be-38Al合金高、低温力学性能及断裂机制[J].稀有金属与硬质合金,2020,48(3):73-76. 被引量:2
2鲍文科,高世阳,刘均波,魏文庆,张丽娜.热挤压及固溶对Al-7Zn-2.5Mg-2.5Cu高强铝合金组织与性能的影响[J].热加工工艺,2020,49(19):105-107. 被引量:1
3夏一骁,匡泽洋,鞠渤宇,杨文澍,武高辉.铍/铝复合材料制备技术与性能设计研究进展[J].铸造技术,2023,44(6):514-524.
4王晶,彭仕先,王旻,张晨,张新建.基于球形铍粉制备的Be-50Al合金热变形行为研究[J].稀有金属材料与工程,2023,52(8):2901-2908.
1陈林恒,牛刚,武会宾,张达.轧制工艺对304不锈钢/Q345复合板组织和性能的影响[J].热加工工艺,2018,47(2):148-153. 被引量:2
2王财玉,吴波.时间参照对绿色消费的影响:环保意识和产品环境怀疑的调节作用[J].心理科学,2018,41(3):621-626. 被引量:17
3宋倍倍.影响40~60mm厚规格Q345E低温冲击韧性的工艺因素分析及改进措施[J].河南科技,2018,0(10):33-35.
4牛神,义行.高硅取向钢板的生产方法[J].武钢技术,1997,35(2):43-45. 被引量:1
5杨小鹏.热处理对45钢煤矿巷道支护锚杆组织与性能的影响[J].铸造技术,2018,39(5):1111-1114. 被引量:3
6刘巧沐.锻态TC25G钛合金棒材的显微组织和织构[J].材料热处理学报,2018,39(6):21-25. 被引量:1
7许杰,胡号.不同变形量下轴承套圈冷轧残余应力演化规律研究[J].武汉交通职业学院学报,2018,20(1):95-101.
8杨涛,王一晴,闻明.Ni-5Pt合金在冷轧过程中的结构演变及力学性能(英文)[J].贵金属,2018,39(1):23-29. 被引量:1
9卫广运,李双江,董廷亮,李建新,王重君,刘伟建,刘晓娟.板坯重压下对改善铸坯内部质量的研究[J].炼钢,2018,34(3):56-61. 被引量:5
10万雯,简发萍.高压扭转大塑性变形对Al-Zn-Mg-Cu-Mn铝合金组织和织构的影响[J].热加工工艺,2018,47(11):144-146. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG339[金属学及工艺—金属压力加工]
Citation Information:
The texture and microstructure evolution law of hot-pressed sintered beryllium ingot during warm-rolling was studied by electron backscatter diffraction (EBSD). The results show that slip is the main deformation mechanism during warm-rolling. With the increase of rolling deformation, the grains are gradually elongated and refined. When the reduction reaches 37.9%, the basal texture in rolled beryllium sheet reaches a maximum value. And then continuously increasing the reduction, all the texture, grain size and mierohardness of beryllium material no longer change significantly. The annealing process is required during or after rolling of beryllium material. The annealing process has a certain weakening effect on the basal texture of beryllium sheet,which can improve its internal microstructure and rolling performance.
quote
| GB/T 7714-2015 | [1] LV Yi-ge, ZHONG Jing-ming, XIN Meng-ming, et al. Study on Microstructure and Texture Evolution Law of Beryllium during Warm-rolling[J]. Rare Metals and Cemented Carbides, 2018(3): 44-48. |
| MLA | [1] LV Yi-ge, et al., "Study on Microstructure and Texture Evolution Law of Beryllium during Warm-rolling." Rare Metals and Cemented Carbides, no. 3, 2018, pp. 44-48. |
| APA | [1] LV Yi-ge, ZHONG Jing-ming, XIN Meng-ming, DAI Yan-ming, LI Mei-sui, WANG Wei-yi, ZHANG Jian-kang, & ZHAO Zhi-ling. (2018). Study on Microstructure and Texture Evolution Law of Beryllium during Warm-rolling. Rare Metals and Cemented Carbides(3), 44-48. |
| IEEE | [1] LV Yi-ge, ZHONG Jing-ming, XIN Meng-ming, DAI Yan-ming, LI Mei-sui, WANG Wei-yi, ZHANG Jian-kang, and ZHAO Zhi-ling, "Study on Microstructure and Texture Evolution Law of Beryllium during Warm-rolling," Rare Metals and Cemented Carbides, no. 3, pp. 44-48, 2018. keywords: {beryllium material;warm-rolling;reduction;texture;annealing} |