School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering;School of Materials Science and Engineering
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The methanol oxidation reaction is a critical half-reaction in direct methanol fuel cells(DMFCs),but its efficiency is limited by the low activity and poor stability of traditional electrocatalysts.This study reports the development of a high-performance PtCo/Mo2CTxcatalyst for methanol oxidation in DMFCs.Synthesized by depositing PtCo alloy nanoparticles on Mo2CTxsheets prepared via cetyltrimethylammonium bromide-assisted etching of Mo2Ga2C,the PtCo/Mo2CTxcatalyst achieved enhanced interlayer spacing and excellent dispersion of active sites.The optimized PtCo/Mo2CTxcatalyst exhibited remarkable catalytic activity,reaching a mass activity of 2296 mA·mgPt-1—6.5 times that of commercial Pt/C.Electrochemical studies confirmed the catalyst's low charge transfer resistance,high electrochemical surface area,and strong CO antipoisoning ability.Stability tests showed that the catalyst retained 62.26%activity after 1000 cycles.These improvements are attributed to the synergistic effects between Pt and Co,the conductive and layered structure of Mo2CTx,making PtCo/Mo2CTxa promising,durable anode material for DMFCs in sustainable energy applications.

KeyWords AITranslate

TUNGSTEN MXene PtCo bimetallic Direct methanol fuel cells ELECTROCATALYST
No data

Basic Information:

DOI:

Chinese Library Classification Number:TM911.4[电气工程—电力电子与电力传动];O643.36[理学—物理化学]

Citation Information:

The methanol oxidation reaction is a critical half-reaction in direct methanol fuel cells(DMFCs),but its efficiency is limited by the low activity and poor stability of traditional electrocatalysts.This study reports the development of a high-performance PtCo/Mo2CTxcatalyst for methanol oxidation in DMFCs.Synthesized by depositing PtCo alloy nanoparticles on Mo2CTxsheets prepared via cetyltrimethylammonium bromide-assisted etching of Mo2Ga2C,the PtCo/Mo2CTxcatalyst achieved enhanced interlayer spacing and excellent dispersion of active sites.The optimized PtCo/Mo2CTxcatalyst exhibited remarkable catalytic activity,reaching a mass activity of 2296 mA·mgPt-1—6.5 times that of commercial Pt/C.Electrochemical studies confirmed the catalyst's low charge transfer resistance,high electrochemical surface area,and strong CO antipoisoning ability.Stability tests showed that the catalyst retained 62.26%activity after 1000 cycles.These improvements are attributed to the synergistic effects between Pt and Co,the conductive and layered structure of Mo2CTx,making PtCo/Mo2CTxa promising,durable anode material for DMFCs in sustainable energy applications.

quote

GB/T 7714-2015 [1] Si-Jie Chang, Xin Zhang, Rui-Ge Wang, et al. Tungsten, 2025(4): 898-909.
MLA [1] Si-Jie Chang, et al., Tungsten, no. 4, 2025, pp. 898-909.
APA [1] Si-Jie Chang, Xin Zhang, Rui-Ge Wang, Jun-Kai Wang, Chao-Fan Wang, Long-Fei Zhang, Zhi-Peng Yu, Qian-Ku Hu, & Ai-Guo Zhou. (2025). Tungsten(4), 898-909.
IEEE [1] Si-Jie Chang, Xin Zhang, Rui-Ge Wang, Jun-Kai Wang, Chao-Fan Wang, Long-Fei Zhang, Zhi-Peng Yu, Qian-Ku Hu, and Ai-Guo Zhou, Tungsten, no. 4, pp. 898-909, 2025.