Effect of Cu and Zr Substitution on Magnetic Properties of Sm2Co7 Melt-Spun Ribbons AITranslate
Abstract AITranslate
Sm2Co7-xRx(R=Cu,Zr;x=0,0.1,0.2,0.3,0.4)melt-spun ribbons were prepared by induction melting and melt spinning.The effects of substitution elements,substitution amount,and melt spinning rate on magnetic properties,intergranular interaction and irreversible reversal field of the melt-spun ribbons were studied.The results of the magnetic property test show that Cu and Zr substitution causes strong pinning effect within the melt-spun ribbons,contributing to improving the coercivity of the melt-spun ribbons,and both achieve maximum coercivity at x=0.3.When the substitution amount x of Cu is 0.1,0.2 and 0.4,the remanence and maximum magnetic energy product of the melt-spun ribbons gradually decrease with the melt spinning rate,while they gradually increase at x=0.3.When the Zr substitution amount x is 0.1~0.4,the remanence and maximum magnetic energy product of the melt-spun ribbons increase at first and then decrease with the increase of melt spinning rate.The Henkel curve test results indicate that for both Cu and Zr substitution,δM value reaches its maximum at x=0.3,indicating that the intergranular exchange coupling effect in the melt-spun ribbons reaches its maximum at this point.The ma-ximumδM values of Sm2(Co,Cu)7 and Sm2(Co,Zr)7 melt-spun ribbons are 1.48 and 1.04,respectively.A moderate substitution amount of Cu and Zr elements can enhance the irreversible reversal field Hn of the Sm2Co7 magnet during demagnetization.
KeyWords AITranslate
1俞珺,姜峰,陈云志,刘宇晖,朱望伟,彭雁,王川.添加Ti对烧结NdFeB磁体微观组织和性能的影响[J].稀有金属与硬质合金,2017,45(6):44-47. 被引量:2
2唐杰,张林,魏成富,杨梨容,赵导文.铸锭冷却方式对NdFeB磁体微观结构和磁性能的影响[J].稀有金属与硬质合金,2011,39(1):45-47. 被引量:1
3宋春燕,王书桓,张凯璇,赵定国.快冷微晶钐铁合金微观结构及渗氮行为[J].稀有金属与硬质合金,2018,46(6):81-85. 被引量:1
4Yitong Zhuge,Yuqing Li,Xiaochang Xu,Dongtao Zhang,Hongguo Zhang,Weiqiang Liu,Ming Yue.Morphology and magnetic properties of Sm_(2)Co_(7)/α-Fe nanocomposite magnets produced by high energy ball milling and spark plasma sintering[J].Journal of Rare Earths,2021,39(3):312-316. 被引量:4
5马强,贾美爽,胡智峰,岳明,刘艳丽,赵同云,沈保根.Texture analysis of ultra-high coercivity Sm_(2)Co_(7) hot deformation magnets[J].Chinese Physics B,2021,30(4):526-529. 被引量:1
1喻俊.基于真实情境的化学深度学习实践——以“剥开皮蛋的奥秘”教学为例[J].实验教学与仪器,2023,40(11):29-32.
2汉高和科思创合作致力于提升工程木材粘合剂的可持续性[J].橡塑智造与节能环保,2024(2):48-48.
3魏明玉,王建豹,Jitendar Kumar,羌建兵,王英敏,刘天鸷,封范,练友运,刘翔.钨/低活化钢钎焊用铁基非晶钎料与接头微结构[J].核聚变与等离子体物理,2023,43(2):132-139.
4葛佳濠,栗伟周,马德稷,曾鹿滨,裴瑞琳.线切割、激光切割工艺对电机用硅钢磁性能的影响[J].电工钢,2024,6(2):10-16.
5汉高集团2023年有机销售额增长4.2%[J].生活用纸,2024,24(5):15-15.
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
Sm2Co7-xRx(R=Cu,Zr;x=0,0.1,0.2,0.3,0.4)melt-spun ribbons were prepared by induction melting and melt spinning.The effects of substitution elements,substitution amount,and melt spinning rate on magnetic properties,intergranular interaction and irreversible reversal field of the melt-spun ribbons were studied.The results of the magnetic property test show that Cu and Zr substitution causes strong pinning effect within the melt-spun ribbons,contributing to improving the coercivity of the melt-spun ribbons,and both achieve maximum coercivity at x=0.3.When the substitution amount x of Cu is 0.1,0.2 and 0.4,the remanence and maximum magnetic energy product of the melt-spun ribbons gradually decrease with the melt spinning rate,while they gradually increase at x=0.3.When the Zr substitution amount x is 0.1~0.4,the remanence and maximum magnetic energy product of the melt-spun ribbons increase at first and then decrease with the increase of melt spinning rate.The Henkel curve test results indicate that for both Cu and Zr substitution,δM value reaches its maximum at x=0.3,indicating that the intergranular exchange coupling effect in the melt-spun ribbons reaches its maximum at this point.The ma-ximumδM values of Sm2(Co,Cu)7 and Sm2(Co,Zr)7 melt-spun ribbons are 1.48 and 1.04,respectively.A moderate substitution amount of Cu and Zr elements can enhance the irreversible reversal field Hn of the Sm2Co7 magnet during demagnetization.
quote
| GB/T 7714-2015 | [1] HOU Yong-jie, ZUO Jian-hua, LI Min-min, et al. Effect of Cu and Zr Substitution on Magnetic Properties of Sm2Co7 Melt-Spun Ribbons[J]. Rare Metals and Cemented Carbides, 2024(2): 50-54. |
| MLA | [1] HOU Yong-jie, et al., "Effect of Cu and Zr Substitution on Magnetic Properties of Sm2Co7 Melt-Spun Ribbons." Rare Metals and Cemented Carbides, no. 2, 2024, pp. 50-54. |
| APA | [1] HOU Yong-jie, ZUO Jian-hua, LI Min-min, BO Yu, ZHANG Ming, DONG Fu-hai, & BAI Suo. (2024). Effect of Cu and Zr Substitution on Magnetic Properties of Sm2Co7 Melt-Spun Ribbons. Rare Metals and Cemented Carbides(2), 50-54. |
| IEEE | [1] HOU Yong-jie, ZUO Jian-hua, LI Min-min, BO Yu, ZHANG Ming, DONG Fu-hai, and BAI Suo, "Effect of Cu and Zr Substitution on Magnetic Properties of Sm2Co7 Melt-Spun Ribbons," Rare Metals and Cemented Carbides, no. 2, pp. 50-54, 2024. keywords: {SmCo;melt-spun ribbon;Cu and Zr substitution;melt spinning rate;magnetic property;ex-change coupling;irreversible reversal field} |