Predictive computations of intermetallic σ phase evolution in duplex steel. I) Thermodynamic modeling of σ phase in the Fe–Cr–Mn–Mo–Ni system AITranslate

Christian Doppler Laboratory Interfaces and Precipitation Engineering; Austria|Institute of Materials Science and Technology
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Thermodynamic modeling of the σ phase was revised according to the three sublattice model developed for the Fe–Cr system (Fe,Cr)10(Fe,Cr)4(Fe,Cr)16 in the view of simulating thermodynamics and kinetics for duplex stainless steels. The alloying elements Mn, Mo and Ni relevant in duplex steels were added to the σ phase model and their thermodynamic parameters were optimized. As a consequence of the change of thermodynamic model and parameters for the σ phases, alloy phases were also re-optimized. The present work include re-optimization of binaries and ternaries sub-systems in order to build a consistent bottom-up Calphad dataset for the thermokinetic simulation of duplex steels.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2020.101998

Chinese Library Classification Number:

Citation Information:

Thermodynamic modeling of the σ phase was revised according to the three sublattice model developed for the Fe–Cr system (Fe,Cr)10(Fe,Cr)4(Fe,Cr)16 in the view of simulating thermodynamics and kinetics for duplex stainless steels. The alloying elements Mn, Mo and Ni relevant in duplex steels were added to the σ phase model and their thermodynamic parameters were optimized. As a consequence of the change of thermodynamic model and parameters for the σ phases, alloy phases were also re-optimized. The present work include re-optimization of binaries and ternaries sub-systems in order to build a consistent bottom-up Calphad dataset for the thermokinetic simulation of duplex steels.

quote

GB/T 7714-2015 [1] Aurélie Jacob, Erwin PovodenKaradeniz. Calphad, 2020(71). DOI:10.1016/j.calphad.2020.101998.
MLA [1] Aurélie Jacob, and Erwin PovodenKaradeniz. Calphad, no. 71, 2020, https://doi.org/10.1016/j.calphad.2020.101998.
APA [1] Aurélie Jacob, & Erwin PovodenKaradeniz. (2020). Calphad(71). https://doi.org/10.1016/j.calphad.2020.101998
IEEE [1] Aurélie Jacob and Erwin PovodenKaradeniz, Calphad, no. 71, 2020, doi: 10.1016/j.calphad.2020.101998.