Comparative Photoinitiating Performances of Donor–Acceptor Multibranched Triphenylamines Designed for Light-Triggered Micropatterning Applications AITranslate
Abstract AITranslate
The present investigation describes an original structure–reactivity relationship within a series of type II photoinitiators designed on the basis of a multibranched molecular engineering strategy. Each photoinitiator indeed incorporates a triphenylamine subunit decorated with a combination of para-substituents, implying anisole or thioanisole as π-conjugated donor groups and multiple reactive ketones as electron-acceptor functions. Interestingly, we demonstrate that the photoinitiating efficiency of such multipolar derivatives is mainly modulated by a solvent-mediated interplay between intersystem crossing and intramolecular charge transfer processes at the excited singlet state. Such a balancing mechanism drastically regulates the population of highly reactive excited triplet species in such a manner that the photoinitiation performance of the dyes can be enhanced by more than 1 order of magnitude within the series. Taking advantage of this amplified photoreactivity, we illustrated the versatile application potential of the best-performing photoinitiating prototype, which was both employed both in a rapid two-dimensional (2D) photopatterning process through liquid crystal display (LCD) image projection and in three-dimensional (3D) micro-optics fabrication at the surface of an optical fiber.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00316
Chinese Library Classification Number:
Citation Information:
The present investigation describes an original structure–reactivity relationship within a series of type II photoinitiators designed on the basis of a multibranched molecular engineering strategy. Each photoinitiator indeed incorporates a triphenylamine subunit decorated with a combination of para-substituents, implying anisole or thioanisole as π-conjugated donor groups and multiple reactive ketones as electron-acceptor functions. Interestingly, we demonstrate that the photoinitiating efficiency of such multipolar derivatives is mainly modulated by a solvent-mediated interplay between intersystem crossing and intramolecular charge transfer processes at the excited singlet state. Such a balancing mechanism drastically regulates the population of highly reactive excited triplet species in such a manner that the photoinitiation performance of the dyes can be enhanced by more than 1 order of magnitude within the series. Taking advantage of this amplified photoreactivity, we illustrated the versatile application potential of the best-performing photoinitiating prototype, which was both employed both in a rapid two-dimensional (2D) photopatterning process through liquid crystal display (LCD) image projection and in three-dimensional (3D) micro-optics fabrication at the surface of an optical fiber.
quote
| GB/T 7714-2015 | [1] Ruchun Zhou, Rana Mhanna, Ming Jin, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00316. |
| MLA | [1] Ruchun Zhou, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00316. |
| APA | [1] Ruchun Zhou, Rana Mhanna, Ming Jin, Haiyan Pan, Decheng Wan, DavyLouis Versace, Constance Thomas, Fabrice MorletSavary, Olivier Soppera, & JeanPierre Malval. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00316 |
| IEEE | [1] Ruchun Zhou, Rana Mhanna, Ming Jin, Haiyan Pan, Decheng Wan, DavyLouis Versace, Constance Thomas, Fabrice MorletSavary, Olivier Soppera, and JeanPierre Malval, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00316. keywords: {photoinitiators;multibranched dyes;photopolymerization;2D and 3D micropatterning;polymer microtips} |