daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ambipolar Doping in π-Conjugated Polymers Ambipolar Doping in π-Conjugated Polymers AITranslate

Indian Institute of Science; University of Colorado Boulder; Indian Institute of Science; Indian Institute of Science; Georgia Institute of Technology; University of Colorado Boulder; University of Colorado Boulder; Indian Institute of Science; Indian Institute of Science; Indian Institute of Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The realization of ambipolar (n- and p-type) doping within a single organic semiconductor is highly desirable for a variety of applications but has rarely been demonstrated in solution-processed π-conjugated polymers. This work reports ambipolar doping in donor–acceptor-based π-conjugated naphthalenediimide-diketopyrrolopyrrole (p(gNDI-TDPP)) polymers. Optical, electrical, electron spin resonance, and photoelectron spectroscopy measurements show evidence of the successful chemical doping of p(gNDI-TDPP) with the n-dopant 4-(2,3-dihydro-1,3-dimethyl-1H-benzimidazol-2-yl)-N,N-dimethylbenzenamine (N-DMBI-H) as well as the related dimer (N-DMBI)2 and the p-dopant tris(4-bromophenyl)ammoniumyl hexachloroantimonate. Temperature-dependent conductivity shows that the barrier for charge transport is decreased at higher doping levels. We observed that the dimer (N-DMBI)2 dopes more efficiently than N-DMBI-H as it reacts rapidly with NDIs and can contribute two electrons per dimer molecule. Comparable charge transport and charge-carrier concentrations in both n- and p-doped polymers were observed. Moreover, while the conductivity of the n-doped material drops on exposure to air, it can be largely recovered upon annealing, indicating that air exposure does not lead to the extensive irreversible chemical decomposition of the doped polymer.

KeyWords AITranslate

solutionprocessable organic semiconductor ambipolarity doping dielectric constant electrical conductivity airstability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01241

Chinese Library Classification Number:

Citation Information:

The realization of ambipolar (n- and p-type) doping within a single organic semiconductor is highly desirable for a variety of applications but has rarely been demonstrated in solution-processed π-conjugated polymers. This work reports ambipolar doping in donor–acceptor-based π-conjugated naphthalenediimide-diketopyrrolopyrrole (p(gNDI-TDPP)) polymers. Optical, electrical, electron spin resonance, and photoelectron spectroscopy measurements show evidence of the successful chemical doping of p(gNDI-TDPP) with the n-dopant 4-(2,3-dihydro-1,3-dimethyl-1H-benzimidazol-2-yl)-N,N-dimethylbenzenamine (N-DMBI-H) as well as the related dimer (N-DMBI)2 and the p-dopant tris(4-bromophenyl)ammoniumyl hexachloroantimonate. Temperature-dependent conductivity shows that the barrier for charge transport is decreased at higher doping levels. We observed that the dimer (N-DMBI)2 dopes more efficiently than N-DMBI-H as it reacts rapidly with NDIs and can contribute two electrons per dimer molecule. Comparable charge transport and charge-carrier concentrations in both n- and p-doped polymers were observed. Moreover, while the conductivity of the n-doped material drops on exposure to air, it can be largely recovered upon annealing, indicating that air exposure does not lead to the extensive irreversible chemical decomposition of the doped polymer.

quote

GB/T 7714-2015 [1] Karandeep Singh, Aiswarya Abhisek Mohapatra, Dipanjan Giri, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01241.
MLA [1] Karandeep Singh, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01241.
APA [1] Karandeep Singh, Aiswarya Abhisek Mohapatra, Dipanjan Giri, Chandrasekhar Gangadharappa, Samik Jhulki, Stephen Barlow, Seth R. Marder, Arindam Ghosh, Satish Patil, & Neha Chauhan. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01241
IEEE [1] Karandeep Singh, Aiswarya Abhisek Mohapatra, Dipanjan Giri, Chandrasekhar Gangadharappa, Samik Jhulki, Stephen Barlow, Seth R. Marder, Arindam Ghosh, Satish Patil, and Neha Chauhan, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01241. keywords: {solutionprocessable organic semiconductor ambipolarity doping dielectric constant electrical conductivity airstability}