daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Rapid Underwater Adhesive Utilizing Crosslinker and Amine Catalyst-Filled Microcapsules AITranslate

The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory; The Johns Hopkins University Applied Physics Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rapidly curing underwater adhesives were tested on untreated substrates and demonstrated high ultimate shear strength. An isocyanate resin was combined with microcapsules containing both a polyol crosslinker and a tertiary amine catalyst. The polyurea microcapsules were synthesized on a large scale via an inverse Pickering emulsion utilizing inexpensive reagents. The microcapsules were stable to ambient conditions and gentle mixing but released their contents when appropriate shearing forces were applied. The final polyurethane adhesive achieved high bonding strength (2.88 ± 0.8 MPa) over a short time period (1 min).

KeyWords AITranslate

microcapsules interfacial polymerization underwater adhesive polyurethane polyurea
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c01277

Chinese Library Classification Number:

Citation Information:

Rapidly curing underwater adhesives were tested on untreated substrates and demonstrated high ultimate shear strength. An isocyanate resin was combined with microcapsules containing both a polyol crosslinker and a tertiary amine catalyst. The polyurea microcapsules were synthesized on a large scale via an inverse Pickering emulsion utilizing inexpensive reagents. The microcapsules were stable to ambient conditions and gentle mixing but released their contents when appropriate shearing forces were applied. The final polyurethane adhesive achieved high bonding strength (2.88 ± 0.8 MPa) over a short time period (1 min).

quote

GB/T 7714-2015 [1] Reid E. Messersmith, Mairead E. Bartlett, Daniel J. Rose, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01277.
MLA [1] Reid E. Messersmith, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01277.
APA [1] Reid E. Messersmith, Mairead E. Bartlett, Daniel J. Rose, Douglas A. Smith, Marcia W. Patchan, Jason J. Benkoski, Morgana M. Trexler, & Christopher M. Hoffman. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01277
IEEE [1] Reid E. Messersmith, Mairead E. Bartlett, Daniel J. Rose, Douglas A. Smith, Marcia W. Patchan, Jason J. Benkoski, Morgana M. Trexler, and Christopher M. Hoffman, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01277. keywords: {microcapsules;interfacial polymerization;underwater adhesive;polyurethane;polyurea}