Multifunctional Green Electromagnetic Interference Shielding Material for the Sub-6-GHz Band AITranslate

Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics; Army Engineering University of PLA;Nanjing Institute of Industry Technology; Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics; Nanjing University of Aeronautics and Astronautics
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Multifunctionality, green, flexibility, and low reflectivity are promising development tendencies of electromagnetic interference (EMI) shielding materials. However, it is still a challenge to effectively integrate multiple functions into a single material. Herein, we reported a multifunctional, green, and flexible EMI shielding material with low reflection. It is a multilayer structure consisting of a low-infrared emission layer, a polyvinyl chloride (PVC) compensation layer, and a microwave absorption layer. The shielding effectiveness (SE) of the proposed multifunctional material can reach above 28 dB with a green index gs ≥ 1 and reflection loss SER < 3.01 dB in the sub-6 GHz band. Furthermore, an ultralow infrared (IR) emissivity of 0.17 within the 3–15 μm spectrum is obtained by optimizing the pattern of the indium tin oxide (ITO) part. The designed material is also optically transparent, flexible, wide-angle, low-profile, and polarization-insensitive. Excellent consistency between the experimental and simulation results demonstrates that this multifunction shielding material can find practical applications in signal shielding scenarios in the sub-6G microwave and 3–15 μm infrared regimes.

KeyWords AITranslate

multifunction green EMI shielding flexible optical transparency sub6 GHz low infrared
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01250

Chinese Library Classification Number:

Citation Information:

Multifunctionality, green, flexibility, and low reflectivity are promising development tendencies of electromagnetic interference (EMI) shielding materials. However, it is still a challenge to effectively integrate multiple functions into a single material. Herein, we reported a multifunctional, green, and flexible EMI shielding material with low reflection. It is a multilayer structure consisting of a low-infrared emission layer, a polyvinyl chloride (PVC) compensation layer, and a microwave absorption layer. The shielding effectiveness (SE) of the proposed multifunctional material can reach above 28 dB with a green index gs ≥ 1 and reflection loss SER < 3.01 dB in the sub-6 GHz band. Furthermore, an ultralow infrared (IR) emissivity of 0.17 within the 3–15 μm spectrum is obtained by optimizing the pattern of the indium tin oxide (ITO) part. The designed material is also optically transparent, flexible, wide-angle, low-profile, and polarization-insensitive. Excellent consistency between the experimental and simulation results demonstrates that this multifunction shielding material can find practical applications in signal shielding scenarios in the sub-6G microwave and 3–15 μm infrared regimes.

quote

GB/T 7714-2015 [1] Shuying Li, Yuying Jiang, Liyan Zhu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c01250.
MLA [1] Shuying Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c01250.
APA [1] Shuying Li, Yuying Jiang, Liyan Zhu, Huijuan Dai, Chunzi Tang, Liangliang Liu, Changqing Gu, & Zhuo Li. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c01250