Purification of LaB_6 Prepared by Teraboron Carbide Reduction AITranslate

Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute;Hunan Rare Earth Metal Material Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

LaB6 is prepared by teraboron carbide reduction. In order through chemical treatment before used to reduce La20a, followed by to obtain LaB6 powder containing Fe 0.01% and C 0.02 %. The yield to improve LaB6 purity, B4C goes pickling and distilled water washing of LaB6 is up to 79.5%

KeyWords AITranslate

LaB6 teraboron carbide La2O3 chemical treatment reduction preparation purification

1Paderno Y B,Paderno V,Filippov V. Some crystal chemistry relationships in eutectic crystallization o{ d- and f-transition metals borides[J]. J Alloy Compounds, 1995, 219:116-118.

2Paderno V, Paderno Y. Features of the real structure of LaB6 single crystals[J]. J Alloys Compounds, 1995,219 :228-231.

3Paderno Y,Paderno V, Filippov V. Some peculiarities of structure formation in eutectic at- and f-transition metals boride alloys[J]. J Alloys and Compounds, 1990, 163: 561-569.

4郑树起,闵光辉,邹增大,于化顺,张川江.硼热还原法制备LaB_6粉末[J].硅酸盐学报,2001,29(2):128-131. 被引量:17

5张廷安,豆志河,杨欢.自蔓延高温合成LaB_6微粉的制备及表征[J].东北大学学报:自然科学版,2005,26(1):67-69. 被引量:11

1张小琴,郝占忠,张海玲.稀土元素硼化物的研究进展[J].稀土,2013,34(2):74-80. 被引量:12

2喇培清,王霞,卢雪峰,魏玉鹏.Mg含量对燃烧合成制备LaB_6粉体的纯度和粒度的影响[J].粉末冶金材料科学与工程,2014,19(4):601-607. 被引量:1

3梁海,侯万良.含铝、钛元素的镍基高温钎料的表面反应[J].焊接,2015(9):59-61. 被引量:2

4余艺平,王松,李伟.多元镧基六硼化物固溶体材料研究进展[J].稀有金属材料与工程,2023,52(5):1954-1962.

1成维,黄美松,苏正夫,王志坚,贾帅广,杨露辉.高纯高致密度LaB_6多晶体的制备[J].中国稀土学报,2015,33(3):323-327. 被引量:3

2李岳丽,王雯,王丽红,周青.环境中镧对水稻叶绿体功能元素的影响[J].稀土,2015,36(2):107-112. 被引量:7

3李鹏,叶雷,程耀永,毛唯,吴欣.K447A镍基高温合金钎焊接头组织及性能[J].焊接,2016(3):11-13. 被引量:1

4杨树颜,焦元启,骆伟新.纳米氧化镧掺杂PEO基SPEs的离子导电性能研究[J].稀土,2016,37(3):31-35.

5徐兰兰,孙丛婷,薛冬峰.稀土晶体研究进展[J].中国稀土学报,2018,36(1):1-17. 被引量:22

6许欢,王玺堂,王周福,马妍,刘浩.感应加热碳热还原合成LaB_6粉体[J].人工晶体学报,2018,47(2):354-358. 被引量:1

7Zhengning Li,Yujing Ou,Peiqing La,Yu Shi.Submicron LaB_6 powders with high purity prepared in large scale by salt-assisted combustion synthesis[J].稀土学报:英文版,2018,36(6):623-629.

8陶如玉,包黎红,红莲,那仁格日乐,富泉.多元稀土硼化物Ce_xBa_(1-x)B_6的制备及表征[J].内蒙古师范大学学报:自然科学汉文版,2018,47(3):217-219. 被引量:1

9林旺,谷科城,陈波水,范兴钰,王鑫.硼基抗磨减摩添加剂的研究进展[J].重庆理工大学学报:自然科学,2019,33(4):75-82. 被引量:3

10赵月,章强,王丹,刘金鑫,孙晓林,魏景傲.高温钎料的研究进展及展望[J].科技视界,2019(7):97-98. 被引量:3

1郭亚琴,白晨光,吕学伟,王华,邓青宇,马世伟.温度对碳热还原制备TiC、TiN的影响研究[J].功能材料,2013,44(23):3507-3512. 被引量:3

2我国利用冶炼炉渣生产不锈钢技术取得重大进展[J].铸造技术,2008,29(8):992-992.

3专利介绍[J].中国有色金属,2006(6):73-73.

4铝热还原制备Al-Sc合金的方法[J].铝加工,2013(5):48-48.

5我国利用冶炼炉渣生产不锈钢技术取得重大进展[J].矿山机械,2008,36(11):117-117.

6朱骏,马春红,郭晓菲,朱鸿民.气相还原制备超细微铌和钽粉末[J].稀有金属,2007,31(1):53-56. 被引量:10

7刘年春,谢卫东,彭晓东,魏群义,李海东.镁锶合金的电化学还原制备[J].有色金属:冶炼部分,2008(4):44-46. 被引量:3

8郭晓玲,郭占成,王志.TiO2和Fe2O3直接电解还原制备TiFe合金[J].北京科技大学学报,2008,30(6):620-624. 被引量:12

9樊新,黄可龙,刘素琴.液相还原法制备不同粒度分布的规则球形纳米银粉研究[J].纳米科技,2007,4(1):31-34. 被引量:2

10我国利用冶炼炉渣生产不锈钢技术取得重大进展[J].铸造技术,2009,30(1):10-10.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.454[金属学及工艺—金属材料]

Citation Information:

LaB6 is prepared by teraboron carbide reduction. In order through chemical treatment before used to reduce La20a, followed by to obtain LaB6 powder containing Fe 0.01% and C 0.02 %. The yield to improve LaB6 purity, B4C goes pickling and distilled water washing of LaB6 is up to 79.5%

quote

GB/T 7714-2015 [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, et al. Purification of LaB_6 Prepared by Teraboron Carbide Reduction[J]. Rare Metals and Cemented Carbides, 2011(4): 17-19.
MLA [1] HUANG Mei-song, et al., "Purification of LaB_6 Prepared by Teraboron Carbide Reduction." Rare Metals and Cemented Carbides, no. 4, 2011, pp. 17-19.
APA [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, & ZHANG Ke-xiang. (2011). Purification of LaB_6 Prepared by Teraboron Carbide Reduction. Rare Metals and Cemented Carbides(4), 17-19.
IEEE [1] HUANG Mei-song, CHEN Yun-zhi, ZHANG Yao-bin, and ZHANG Ke-xiang, "Purification of LaB_6 Prepared by Teraboron Carbide Reduction," Rare Metals and Cemented Carbides, no. 4, pp. 17-19, 2011. keywords: {LaB6;teraboron carbide;La2O3;chemical treatment;reduction preparation;purification}