daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tuning Ionic Conductivity in Fluorite Gd-Doped CeO2-Bixbyite RE2O3 (RE = Y and Sm) Multilayer Thin Films by Controlling Interfacial Strain Tuning Ionic Conductivity in Fluorite Gd-Doped CeO2-Bixbyite RE2O3 (RE = Y and Sm) Multilayer Thin Films by Controlling Interfacial Strain AITranslate

University of South Carolina; University of South Carolina; University of South Carolina; University of South Carolina; Oak Ridge National Laboratory; Oak Ridge National Laboratory; University of South Carolina
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Interfacial strain in heteroepitaxial oxide thin films is a powerful tool for discovering properties and recognizing the potential of materials performance. Particularly, facilitating ion conduction by interfacial strain in oxide multilayer thin films has always been seen to be a highly promising route to this goal. However, the effect of interfacial strain on ion transport properties is still controversial due to the difficulty in deconvoluting the strain contribution from other interfacial phenomena, such as space charge effects. Here, we show that interfacial strain can effectively tune the ionic conductivity by successfully growing multilayer thin films composed of an ionic conductor Gd-doped CeO2 (GDC) and an insulator RE2O3 (RE = Y and Sm). In contrast to compressively strained GDC-Y2O3 multilayer films, tensile strained GDC-Sm2O3 multilayer films demonstrate the enhanced ionic conductivity of GDC, which is attributed to the increased concentration of oxygen vacancies. In addition, we demonstrate that increasing the number of interfaces has no impact on the further enhancement of the ionic conductivity in GDC-Sm2O3 multilayer films. Our findings demonstrate the unambiguous role of interfacial strain on ion conduction of oxides and provide insights into the rational design of fast ion conductors through interface engineering.

KeyWords AITranslate

interfacial strain pulsed laser deposition epitaxial straininduced ionic conductivity oxide multilayer thin films fluorite structureShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00724

Chinese Library Classification Number:

Citation Information:

Interfacial strain in heteroepitaxial oxide thin films is a powerful tool for discovering properties and recognizing the potential of materials performance. Particularly, facilitating ion conduction by interfacial strain in oxide multilayer thin films has always been seen to be a highly promising route to this goal. However, the effect of interfacial strain on ion transport properties is still controversial due to the difficulty in deconvoluting the strain contribution from other interfacial phenomena, such as space charge effects. Here, we show that interfacial strain can effectively tune the ionic conductivity by successfully growing multilayer thin films composed of an ionic conductor Gd-doped CeO2 (GDC) and an insulator RE2O3 (RE = Y and Sm). In contrast to compressively strained GDC-Y2O3 multilayer films, tensile strained GDC-Sm2O3 multilayer films demonstrate the enhanced ionic conductivity of GDC, which is attributed to the increased concentration of oxygen vacancies. In addition, we demonstrate that increasing the number of interfaces has no impact on the further enhancement of the ionic conductivity in GDC-Sm2O3 multilayer films. Our findings demonstrate the unambiguous role of interfacial strain on ion conduction of oxides and provide insights into the rational design of fast ion conductors through interface engineering.

quote

GB/T 7714-2015 [1] Gene Yang, Mohammad El Loubani, Habib Rostaghi Chalaki, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00724.
MLA [1] Gene Yang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00724.
APA [1] Gene Yang, Mohammad El Loubani, Habib Rostaghi Chalaki, Jiwon Kim, Jong K. Keum, Christopher M. Rouleau, & Dongkyu Lee. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00724
IEEE [1] Gene Yang, Mohammad El Loubani, Habib Rostaghi Chalaki, Jiwon Kim, Jong K. Keum, Christopher M. Rouleau, and Dongkyu Lee, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00724. keywords: {interfacial strain pulsed laser deposition epitaxial straininduced ionic conductivity oxide multilayer thin films fluorite structureShow More}