daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Constitutive Relationship of Ti-B25High StrengthβTitanium Alloy during High Temperature Deformation AITranslate

Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research;Northwest Institute for Nonferrous Metal Research
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The thermal compression tests of Ti-B25 alloy were conducted on Gleeble 3800 thermal simulator under the conditions of 800~1000℃ temperature,0.01~10s^-1 strain rate and 70% strain.The results show that in the initial deformation stage of Ti-B25 alloy,the flow stress increases rapidly with the increase of strain.However,after reaching the peak value,the flow stress begins to decrease and gradually stabilizes, showing a steady flow characteristic.During high temperature deformation,both steady stress and peak stress decrease significantly with the increase of temperature and the decrease of strain rate.Through regression processing of the data,the functional relationships are fitted between the thermal deformation activation energy Q,the structural factor A,the stress index nor the stress level parameterαand the strainε, and then the constitutive equation of the alloy during high temperature deformation is obtained.

KeyWords AITranslate

Ti-B25 alloy thermal compression deformation flow stress thermal deformation activation energy constitutive equation

1戚运连,曾卫东,赵永庆.Ti600合金的高温本构方程[J].热加工工艺,2006,35(17):5-8. 被引量:14

2周佳宇,哈军.钛合金材料在舰船管系上的应用[J].材料开发与应用,2006,21(3):40-42. 被引量:28

3杨英丽,罗媛媛,赵恒章,郭荻子,吴金平,苏航标,赵彬.我国舰船用钛合金研究应用现状[J].稀有金属材料与工程,2011,40(S2):538-544. 被引量:50

4黄晓艳,刘波,李雪.钛合金在舰船上的应用[J].南方金属,2005(6):10-11. 被引量:17

5张艳姝,潘利永,骆俊廷,刘晓飞.TC4钛合金高温本构关系的研究[J].热加工工艺,2013,42(2):24-27. 被引量:17

6胡会娥,杨丽,甄良,邵文柱,张宝友.Relationship between boundary misorientation angle and true strain during high temperature deformation of 7050 aluminum alloy[J].中国有色金属学会会刊:英文版,2008,18(4):795-798. 被引量:9

1孙花梅,刘伟,戚运莲,李修雷,毛小南,洪权.Ti-B25钛合金管材挤压成形数值模拟及实验研究[J].钛工业进展,2021,38(1):25-29. 被引量:5

2孙花梅,刘伟,戚运莲,李修雷,南榕.Ti-B25合金高温变形时的塑性流动软化行为[J].钛工业进展,2022,39(1):6-11.

1孙花梅,刘伟,戚运莲,李修雷,南榕.Ti-B25合金高温变形时的塑性流动软化行为[J].钛工业进展,2022,39(1):6-11.

2孟凡玲,赵剑博,张志强,柏春光.钛合金型材挤压数值模拟技术研究现状及展望[J].沈阳理工大学学报,2022,41(3):32-40.

3屈磊,辛社伟,李婷,杜宇,邹磊,应扬,郭荻子,王晓.热连轧工艺制备TC4钛合金无缝管材组织及力学性能研究[J].钛工业进展,2022,39(5):13-16.

4李婷,杜宇,屈磊,郭荻子,应扬,孙花梅,邹磊.热处理对TA34钛合金管材组织性能与成材率的影响[J].钛工业进展,2022,39(5):22-26.

5王田,南迎飞,王伟,岳旭,乔恩利,叶红川.Ti-811合金棒材热连轧过程有限元数值模拟及验证[J].钛工业进展,2023,40(4):26-34.

1刘骁,赵春芳,叶翔.深冷处理工艺对低温阀门用25合金钢组织和性能的研究[J].热处理技术与装备,2018,39(5):8-14. 被引量:2

2刘乐乐,韩茂盛,梁晨,苑伟.BFe10-1-1合金的热压缩变形行为与本构关系研究[J].热加工工艺,2018,47(22):97-100. 被引量:2

3刘丽玉,高翔宇,孔焕平,刘昌奎.K4125合金涡轮叶片榫齿荧光显示缺陷研究[J].失效分析与预防,2018,13(6):397-402.

4马艳霞,苑伟,梁晨,周铁柱.CuNi10Fe1.6Mn铜镍合金热压缩流变应力行为研究[J].锻压装备与制造技术,2018,53(6):130-133. 被引量:2

5齐永杰,余新平,吕航鹰,潘光永.6061铝合金热变形动态再结晶行为研究[J].特种铸造及有色合金,2018,0(11):1185-1188. 被引量:6

6周伟,葛鹏,赵永庆,辛社伟,李倩,王晶,黄朝文,陈军.一种新型高强β钛合金力学性能和显微组织的关系研究(英文)[J].稀有金属材料与工程,2017,46(8):2076-2079. 被引量:2

7甘守武,陈志军,赵磊娜.基于单隐藏层BP神经网络Ti-55531合金流变应力预测模型的建立[J].热加工工艺,2018,47(22):59-61. 被引量:2

8杨博文,薛勇,张治民,王强,刘震.热等静压态TC4钛合金高温变形行为研究[J].热加工工艺,2018,47(23):38-43. 被引量:4

9刘兵.穿过非穿越 分类来把舵[J].数学学习与研究,2018(24):107-107.

10周伟,葛鹏,赵永庆,辛社伟,李倩,陈军,张思远,黄朝文.一种新型高强钛合金热处理过程中初生相形态演变和力学性能(英文)[J].稀有金属材料与工程,2017,46(10):2852-2856. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

The thermal compression tests of Ti-B25 alloy were conducted on Gleeble 3800 thermal simulator under the conditions of 800~1000℃ temperature,0.01~10s^-1 strain rate and 70% strain.The results show that in the initial deformation stage of Ti-B25 alloy,the flow stress increases rapidly with the increase of strain.However,after reaching the peak value,the flow stress begins to decrease and gradually stabilizes, showing a steady flow characteristic.During high temperature deformation,both steady stress and peak stress decrease significantly with the increase of temperature and the decrease of strain rate.Through regression processing of the data,the functional relationships are fitted between the thermal deformation activation energy Q,the structural factor A,the stress index nor the stress level parameterαand the strainε, and then the constitutive equation of the alloy during high temperature deformation is obtained.

quote

GB/T 7714-2015 [1] TAN Wei-li, LIU Wei, QI Yun-lian, et al. Study on Constitutive Relationship of Ti-B25High StrengthβTitanium Alloy during High Temperature Deformation[J]. Rare Metals and Cemented Carbides, 2018(6): 57-62.
MLA [1] TAN Wei-li, et al., "Study on Constitutive Relationship of Ti-B25High StrengthβTitanium Alloy during High Temperature Deformation." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 57-62.
APA [1] TAN Wei-li, LIU Wei, QI Yun-lian, XIE Chong-bo, & SUN Hua-mei. (2018). Study on Constitutive Relationship of Ti-B25High StrengthβTitanium Alloy during High Temperature Deformation. Rare Metals and Cemented Carbides(6), 57-62.
IEEE [1] TAN Wei-li, LIU Wei, QI Yun-lian, XIE Chong-bo, and SUN Hua-mei, "Study on Constitutive Relationship of Ti-B25High StrengthβTitanium Alloy during High Temperature Deformation," Rare Metals and Cemented Carbides, no. 6, pp. 57-62, 2018. keywords: {Ti-B25 alloy;thermal compression deformation;flow stress;thermal deformation activation energy;constitutive equation}