Thermal Characterization of Metal-Diamond Composite Heat Spreaders Using Low-Frequency-Domain Thermoreflectance Thermal Characterization of Metal-Diamond Composite Heat Spreaders Using Low-Frequency-Domain Thermoreflectance AITranslate

University of Bristol; University of Bristol;RHP-Technology GmbH, TFZ Technologie- und Forschungszentrum Seibersdorf; University of Bristol
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

High thermal conductivity and an appropriate coefficient of thermal expansion are the key features of a perfect heat spreader for electronic device packaging, especially for applications with increased power density and the increasing demand for higher reliability and semiconductor device performance. For the past decade, metal-diamond composites have been thoroughly studied as a heat spreader, thanks to their high thermal conductivities and tailored coefficients of thermal expansion. While existing thermal characterization methods are good for quality control purposes, a more accurate method is needed to determine detailed thermal properties of these composite materials, especially if clad with metal. Low-frequency-range-domain thermoreflectance has been adopted to measure the thermal conductivity of a metal-diamond composite sandwiched between metal cladding layers. Due to this technique’s low modulation frequencies, from 10 Hz to 10 kHz, multiple layers can be probed and measured at depths ranging from tens of micrometers to a few millimeters.

KeyWords AITranslate

metaldiamond composite heat spreader frequencydomain thermoreflectance thermal characterization thermal conductivityShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00771

Chinese Library Classification Number:

Citation Information:

High thermal conductivity and an appropriate coefficient of thermal expansion are the key features of a perfect heat spreader for electronic device packaging, especially for applications with increased power density and the increasing demand for higher reliability and semiconductor device performance. For the past decade, metal-diamond composites have been thoroughly studied as a heat spreader, thanks to their high thermal conductivities and tailored coefficients of thermal expansion. While existing thermal characterization methods are good for quality control purposes, a more accurate method is needed to determine detailed thermal properties of these composite materials, especially if clad with metal. Low-frequency-range-domain thermoreflectance has been adopted to measure the thermal conductivity of a metal-diamond composite sandwiched between metal cladding layers. Due to this technique’s low modulation frequencies, from 10 Hz to 10 kHz, multiple layers can be probed and measured at depths ranging from tens of micrometers to a few millimeters.

quote

GB/T 7714-2015 [1] Zeina Abdallah, James W. Pomeroy, Erich Neubauer, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00771.
MLA [1] Zeina Abdallah, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00771.
APA [1] Zeina Abdallah, James W. Pomeroy, Erich Neubauer, & Martin Kuball. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00771
IEEE [1] Zeina Abdallah, James W. Pomeroy, Erich Neubauer, and Martin Kuball, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00771. keywords: {metaldiamond composite heat spreader frequencydomain thermoreflectance thermal characterization thermal conductivityShow More}