Metallization of Polyphenylene Sulfide by Low-Cost Mussel-Inspired Catechol/Polyamine Surface Modification AITranslate

University of Electronic Science and Technology of China; University of Electronic Science and Technology of China; University of Electronic Science and Technology of China; University of Electronic Science and Technology of China; University of Electronic Science and Technology of China
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

An economical and efficient strategy for fabricating high-performance metallic copper layers on polyphenylene sulfide (PPS) for high-frequency microwave applications via mussel-inspired surface modification and electroless copper plating (ECP) is illustrated in this paper. Through UV-induced surface modification of catechol (CA)/polyamine (PA), the modified PPS substrate is capable of adsorbing silver particles, which provides activation sites for subsequent ECP. The impact of CA/PA modification on the relationship between PPS and the deposited copper layer can be determined by water contact angle measurements, X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), and tape peel tests. The involvement of CA/PA has successfully introduced the functional groups for chemical bonding on the PPS surface, which greatly improves the adhesion between the PPS and the deposited copper layer. Moreover, after 40 min of ECP, the produced copper layer exhibits good adhesion at the 5B level (according to the ASTM D3559) and an excellent conductivity of 0.37 S/m (approx. 62% of bulk copper). Meanwhile, the deposited copper layer also has good resistance to acid, alkali, and salt corrosion (less than 25 g/m2 per unit area weight loss after 60 h of corrosion). This approach opens up an efficient path for the surface metallization of PPS, which has a broad potential for application in high-frequency copper-clad laminates (CCLs).

KeyWords AITranslate

polyphenylene sulfide catechol polyamines surface modification electroless copper plating adhesion
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00399

Chinese Library Classification Number:

Citation Information:

An economical and efficient strategy for fabricating high-performance metallic copper layers on polyphenylene sulfide (PPS) for high-frequency microwave applications via mussel-inspired surface modification and electroless copper plating (ECP) is illustrated in this paper. Through UV-induced surface modification of catechol (CA)/polyamine (PA), the modified PPS substrate is capable of adsorbing silver particles, which provides activation sites for subsequent ECP. The impact of CA/PA modification on the relationship between PPS and the deposited copper layer can be determined by water contact angle measurements, X-ray photoelectron spectroscopy (XPS), X-ray diffraction (XRD), and tape peel tests. The involvement of CA/PA has successfully introduced the functional groups for chemical bonding on the PPS surface, which greatly improves the adhesion between the PPS and the deposited copper layer. Moreover, after 40 min of ECP, the produced copper layer exhibits good adhesion at the 5B level (according to the ASTM D3559) and an excellent conductivity of 0.37 S/m (approx. 62% of bulk copper). Meanwhile, the deposited copper layer also has good resistance to acid, alkali, and salt corrosion (less than 25 g/m2 per unit area weight loss after 60 h of corrosion). This approach opens up an efficient path for the surface metallization of PPS, which has a broad potential for application in high-frequency copper-clad laminates (CCLs).

quote

GB/T 7714-2015 [1] Chengyuan Feng, Haijun Chen, Mengyao Yang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00399.
MLA [1] Chengyuan Feng, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00399.
APA [1] Chengyuan Feng, Haijun Chen, Mengyao Yang, Zhesheng Feng, & Yan Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00399
IEEE [1] Chengyuan Feng, Haijun Chen, Mengyao Yang, Zhesheng Feng, and Yan Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00399. keywords: {polyphenylene sulfide;catechol;polyamines;surface modification;electroless copper plating;adhesion}