daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Diagnosis of ASR damage in highway pavement after 15 years of service in wet-freeze climate region AITranslate

Institute of Fundamental Technological Research Polish Academy of Sciences;Institute of Fundamental Technological Research Polish Academy of Sciences;Institute of Fundamental Technological Research Polish Academy of Sciences;Institute of Fundamental Technological Research Polish Academy of Sciences;Institute of Fundamental Technological Research Polish Academy of Sciences;Institute of Fundamental Technological Research Polish Academy of Sciences
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Diagnostic tests were carried out on specimens drilled from a section of jointed, unreinforced highway pavement after 15 years of service. The section of highway was exposed to heavy road traffic, environmental actions of wet-freeze climate zone and associated winter maintenance including application of deicing salt. Premature pavement damage was manifested by visible cracking, mostly along transverse joints and in slab corners. Tests performed on core specimens included petrographic analysis of concrete and its components, using optical and scanning electron microscopy, also evaluation of elastic and transport properties, expansion potential, cracks and air void system. Numerous cracks in the grains of coarse quartzite aggregate were found. Reactive forms of quartz in quartzite aggregate - microcrystalline and cryptocrystalline quartz - were abundant. The gel-like products in cracks in quartzite grains and in surrounding cement paste were identified as alkali-silica reaction products. Expansion of specimens exposed to an alkali-silica reaction-promoting environment indicated the potential for further development of such reaction. Substantial cracking and reduction of modulus of elasticity was correlated with the presence of reactive quartz in quartzite aggregate. The role of additional destructive factors, such as the impact of heavy vehicles traffic and freeze-thaw aggression was indicated by greater cracks in the slow traffic lane compared than in the emergency lane, associated with local marginal air entrainment of concrete.

KeyWords AITranslate

Alkalisilica reaction Concrete Cracking Durability Highway pavement
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2022.e01226

Chinese Library Classification Number:

Citation Information:

Diagnostic tests were carried out on specimens drilled from a section of jointed, unreinforced highway pavement after 15 years of service. The section of highway was exposed to heavy road traffic, environmental actions of wet-freeze climate zone and associated winter maintenance including application of deicing salt. Premature pavement damage was manifested by visible cracking, mostly along transverse joints and in slab corners. Tests performed on core specimens included petrographic analysis of concrete and its components, using optical and scanning electron microscopy, also evaluation of elastic and transport properties, expansion potential, cracks and air void system. Numerous cracks in the grains of coarse quartzite aggregate were found. Reactive forms of quartz in quartzite aggregate - microcrystalline and cryptocrystalline quartz - were abundant. The gel-like products in cracks in quartzite grains and in surrounding cement paste were identified as alkali-silica reaction products. Expansion of specimens exposed to an alkali-silica reaction-promoting environment indicated the potential for further development of such reaction. Substantial cracking and reduction of modulus of elasticity was correlated with the presence of reactive quartz in quartzite aggregate. The role of additional destructive factors, such as the impact of heavy vehicles traffic and freeze-thaw aggression was indicated by greater cracks in the slow traffic lane compared than in the emergency lane, associated with local marginal air entrainment of concrete.

quote

GB/T 7714-2015 [1] Michał A. Glinicki, Daria JóźwiakNiedźwiedzka, Aneta Antolik, et al. Case Studies in Construction Materials, 2022(17). DOI:10.1016/j.cscm.2022.e01226.
MLA [1] Michał A. Glinicki, et al., Case Studies in Construction Materials, no. 17, 2022, https://doi.org/10.1016/j.cscm.2022.e01226.
APA [1] Michał A. Glinicki, Daria JóźwiakNiedźwiedzka, Aneta Antolik, Kinga Dziedzic, Mariusz Dąbrowski, & Karolina Bogusz. (2022). Case Studies in Construction Materials(17). https://doi.org/10.1016/j.cscm.2022.e01226
IEEE [1] Michał A. Glinicki, Daria JóźwiakNiedźwiedzka, Aneta Antolik, Kinga Dziedzic, Mariusz Dąbrowski, and Karolina Bogusz, Case Studies in Construction Materials, no. 17, 2022, doi: 10.1016/j.cscm.2022.e01226. keywords: {Alkalisilica reaction;Concrete;Cracking;Durability;Highway pavement}