daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

In-situ Optical Control of Local Periodical Ferroelastic Domain Evolution in CH3NH3PbI3 Perovskites In-situ Optical Control of Local Periodical Ferroelastic Domain Evolution in CH3NH3PbI3 Perovskites AITranslate

University of Chinese Academy of Sciences; Shanghai Institute of Ceramics; Shanghai Institute of Ceramics; Shanghai Institute of Ceramics; Shanghai Institute of Ceramics; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Local pulse mid-infrared (IR) light at 1468 cm–1 corresponding to the C–N dipoles within the CH3NH3+ rock was incorporated into the present study to explore ferroic domain dynamics of the methylammonium lead triiodide (MAPbI3) crystal. The pulsed IR illumination was found to induce the CH3 asymmetric deformation, rotation of the MA+ ion, and inorganic PbI6 octahedra framework deformation, resulting in a remarkable strain as a driving force for domain wall movement, local ions migration, and properties tailoring of the MAPbI3 system. Local chemical mapping, nanoscale IR spectrum, and local thermal ionic imaging demonstrated that the strain plays an important role in the redistribution of mobile CH3NH3+ ions, contributing to local triangle- or spindle-shaped nucleation and growth kinetic behavior of periodical, stripe twin domains. The results offer insights into the interplay of the strain level, ferroic properties, and chemical ion migration on the optoelectronic performance of metal halide perovskites-based solar cells and suggest a promising optical modulation approach for periodical ferroelastic domain configurations to enhance the optoelectronic performance of metal halide perovskites-based solar cells.

KeyWords AITranslate

methylammonium lead triiodide crystals perovskitesbased solar cells ferroic domain nucleation and growth pulsed IR illumination AFMIR
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01385

Chinese Library Classification Number:

Citation Information:

Local pulse mid-infrared (IR) light at 1468 cm–1 corresponding to the C–N dipoles within the CH3NH3+ rock was incorporated into the present study to explore ferroic domain dynamics of the methylammonium lead triiodide (MAPbI3) crystal. The pulsed IR illumination was found to induce the CH3 asymmetric deformation, rotation of the MA+ ion, and inorganic PbI6 octahedra framework deformation, resulting in a remarkable strain as a driving force for domain wall movement, local ions migration, and properties tailoring of the MAPbI3 system. Local chemical mapping, nanoscale IR spectrum, and local thermal ionic imaging demonstrated that the strain plays an important role in the redistribution of mobile CH3NH3+ ions, contributing to local triangle- or spindle-shaped nucleation and growth kinetic behavior of periodical, stripe twin domains. The results offer insights into the interplay of the strain level, ferroic properties, and chemical ion migration on the optoelectronic performance of metal halide perovskites-based solar cells and suggest a promising optical modulation approach for periodical ferroelastic domain configurations to enhance the optoelectronic performance of metal halide perovskites-based solar cells.

quote

GB/T 7714-2015 [1] Yuxin Ying, Weiwei Yang, Cheng Yi, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01385.
MLA [1] Yuxin Ying, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01385.
APA [1] Yuxin Ying, Weiwei Yang, Cheng Yi, Kunyu Zhao, Guorong Li, & Huarong Zeng. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01385
IEEE [1] Yuxin Ying, Weiwei Yang, Cheng Yi, Kunyu Zhao, Guorong Li, and Huarong Zeng, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01385. keywords: {methylammonium lead triiodide crystals perovskitesbased solar cells ferroic domain nucleation and growth pulsed IR illumination AFMIR}