Study on Microstructure and Corrosion Resistance of Al_2CrFeNiCo_x CuTi High Entropy Alloy AITranslate
Abstract AITranslate
The multi element high entropy alloys Al2 CrFeNiCox CuTi (x = 0. 5,1. 0,1. 5,2. 0) with different Co contents were prepared using laser cladding method. Electrochemical performances of the alloys were tested in 1 mol/L NaC1 solution and 0.5 mol/L H2SO4 solution,and the corresponding polarization curves were drawn. The results show that the high entropy alloys are columnar and equiaxed crystals, with the phase structure of fcc and hcc. The phase of fcc increases gradually with the increase of Co content in the alloys, enhancing intergranular corrosion and then reducing corrosion resistance of the alloys.
KeyWords AITranslate
1Yeh J W,Chen S K ,Lin S J , etal. Nanost ructured high-entropy alloys with multiple principal element[J].Advanced Engineering Material, 2004,6(5): 299-303.
2刘源,李言祥,陈祥,陈敏.多主元高熵合金研究进展[J].材料导报,2006,20(4):4-6. 被引量:80
3Zhou Y J, Zhang Y, Kim T N,et al. Microstructure char- acterizations and strengthening mechanism of multiprin cipal component AlCoCrFeNiTi0.5 solid solution alloy with excellent mechanical properties[J].Materials Let- ters,2008,62(17-18):2 673-2 676.
4Chen Y Y, Hong U T, Shih H C, et al. Electrochemical kinetics of the high entropy alloys in aqueous environ- ments a comparison with type 304 stainless steel [J]. Corrosion Science, 2005,47 (11) : 2 679-2 699.
5Wu J M,Lin S J,Yeh J W,etal. Adhesive wear behavior of AlxCoCrCuFeNi high-entropy alloys as a function of aluminum content[J]. Wear,2006,261(5-6) :513-519.
6崔忠圻.金属学与热处理[M].北京:机械工业出版社,2008,80-86.
7李伟,刘贵仲,郭景杰.AlFeCuCoNiCrTi_x高熵合金的组织结构及电化学性能[J].特种铸造及有色合金,2009(10):941-944. 被引量:29
8童重缙.Cu-Co-Ni-Cr-Al-Fe高熵合金变形结构与高温特性之研究[D].台北:国立清华大学,2002.
9李伟,刘贵仲,郭景杰.AlxFeCoNiCrTi系高熵合金的组织结构及电化学性能研究[J].铸造,2009(5):431-435. 被引量:21
1安旭龙,刘其斌,郑波.激光熔覆制备高熵合金MoFeCrTiWAl_xSi_y涂层的组织与性能[J].红外与激光工程,2014,43(4):1140-1144. 被引量:22
2李栋梁,周芳,余师豪.激光熔覆FeCrNiMnMo_xB_(0.5)高熵合金涂层组织与耐蚀性能[J].强激光与粒子束,2016,28(2):190-195. 被引量:18
3赵腾雄,康蓉,李培友.高熵合金薄膜涂层研究进展[J].铸造技术,2017,38(4):746-748. 被引量:5
4王茵,尚晓娟,田兴强,郭亚雄,汪震,陈佳.激光熔覆(FeCrCo/Ni)_5-SiTiNbMoW高熵合金涂层组织及性能研究[J].稀有金属与硬质合金,2018,46(5):30-36. 被引量:6
5张世一,王勇,韩彬,杨涛,李美艳.激光熔覆多主元高熵合金涂层的研究进展[J].材料导报,2017,31(A01):485-488. 被引量:6
6董世知,韦宝权,隋心,王恩杰.FeAlCrCuCoTi_(0.4)高熵合金涂层冲蚀磨损性能[J].辽宁工程技术大学学报:自然科学版,2018,37(2):376-380. 被引量:2
7周子钧,姜芙林,宋鹏芳,杨发展,王玉玲,杨勇,梁鹏.激光熔覆高熵合金涂层的耐腐蚀性能研究进展[J].表面技术,2021,50(12):257-270. 被引量:8
8张志彬,张舒研,陈永雄,高洋洋,梁秀兵.合金组元与含量对激光熔覆高熵合金涂层的影响研究综述[J].中国表面工程,2021,34(5):76-91. 被引量:6
9左润燕,孙荣禄,牛伟,郝文俊,谷米,李小龙.激光熔覆CoCrFeNiTi_(x)高熵合金涂层的组织与性能[J].表面技术,2022,51(3):363-370. 被引量:4
1张华,张岩,吴畏.浅谈家用电器零部件盐雾试验标准的一些误区——以电镀件、螺钉为例[J].家电科技,2022(S01):748-750.
2崔天晓,石岩.激光熔覆制备高熵合金的研究现状及发展趋势[J].机械工程师,2015(2):199-201. 被引量:7
3周芳,刘其斌,郑波.Si,Al对激光熔覆MoFeCrTiW高熵合金涂层组织性能的影响[J].强激光与粒子束,2015,27(11):266-271. 被引量:18
4周芳,刘其斌,郑波.Si、Al添加对MoFeCrTiW高熵合金涂层组织性能的影响[J].中国激光,2016,43(2):52-59. 被引量:11
5李相阳,朱红梅.激光熔覆制备高熵合金涂层的研究进展[J].热加工工艺,2016,45(22):19-23. 被引量:14
6王彦芳,李豪,石志强,肖亚梅,孙旭,王亭.激光熔覆高耐蚀Fe基固溶体合金涂层[J].红外与激光工程,2017,46(8):53-57. 被引量:8
7周斌,石世宏,邓志强,石拓,傅戈雁,方琴琴.基于中空激光光内送粉技术的扇形结构件激光成形研究[J].红外与激光工程,2017,46(9):48-53. 被引量:4
8尚晓娟,刘其斌,郭亚雄,徐鹏,周芳.退火对激光熔覆MoFeCrTiWAlNb高熔点高熵合金涂层组织与性能的影响[J].材料热处理学报,2017,38(11):101-107. 被引量:10
9郭亚雄,刘其斌,周芳.激光熔覆高熔点AlCrFeMoNb_xTiW高熵合金涂层组织及耐磨性能[J].稀有金属,2017,41(12):1327-1332. 被引量:26
10徐翠翠,刘刚.CoCrFeNiTi_x合金的混合熵计算及分析[J].西安工业大学学报,2017,37(8):621-627. 被引量:3
1易荣喜,谢世坤,潘晓亮,郑志强.稀土对AlSi7合金半固态性能的影响[J].热加工工艺,2009(3):25-27. 被引量:8
2张宪(译).晶体组织受控生长的CVDα—Al2O3涂层的沉积、显微结构和特性[J].工具展望,2007(2):10-15. 被引量:1
3廖先富(编译).用于高速高效加工的CVD超级FF刀具涂层[J].工具展望,2009(5):26-28.
4金潇明,何鹤林,伍利群,王志坚.金属材料在振动切削时脆化机理的研究[J].新技术新工艺,2009(3):78-80. 被引量:1
5魏志君,陈乐生,申乾宏,张玲洁,杨辉,樊先平,吴新合,向文之.焊料种类及焊缝显微形貌对焊接钎着率的影响[J].电工材料,2014(2):3-7. 被引量:2
6谷月峰,刘毅,林栋梁,郭建亭,董林.Zr对Ni_3Al合金中晶界与位错交互作用的影响[J].电子显微学报,1994,13(6):497-497.
7高泽生.A356合金α(Al)的晶粒细化[J].特种铸造及有色合金,1999(5):26-27. 被引量:12
8王维东,胡秀莲,冯志平,孙德伟,何艳玲.磁化镀液化学镀层的微观结构[J].材料工程,1998(5):24-25. 被引量:2
9安金敏,任忠鸣,李伟轩,钟云波,雷作胜,邓康.连续定向凝固技术研究[J].上海金属,2005,27(6):19-25. 被引量:2
10付志凯,王文健,丁昊昊,张勇强,刘启跃,朱旻昊.激光熔覆铁基合金对轮轨材料磨损与损伤性能的影响[J].材料热处理学报,2015,36(8):217-222. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:TG146[金属学及工艺—金属材料]
Citation Information:
The multi element high entropy alloys Al2 CrFeNiCox CuTi (x = 0. 5,1. 0,1. 5,2. 0) with different Co contents were prepared using laser cladding method. Electrochemical performances of the alloys were tested in 1 mol/L NaC1 solution and 0.5 mol/L H2SO4 solution,and the corresponding polarization curves were drawn. The results show that the high entropy alloys are columnar and equiaxed crystals, with the phase structure of fcc and hcc. The phase of fcc increases gradually with the increase of Co content in the alloys, enhancing intergranular corrosion and then reducing corrosion resistance of the alloys.
quote
| GB/T 7714-2015 | [1] HE Li, ZHANG Yun-peng, QIU Xing-wu. Study on Microstructure and Corrosion Resistance of Al_2CrFeNiCo_x CuTi High Entropy Alloy[J]. Rare Metals and Cemented Carbides, 2013(4): 38-41. |
| MLA | [1] HE Li, et al., "Study on Microstructure and Corrosion Resistance of Al_2CrFeNiCo_x CuTi High Entropy Alloy." Rare Metals and Cemented Carbides, no. 4, 2013, pp. 38-41. |
| APA | [1] HE Li, ZHANG Yun-peng, & QIU Xing-wu. (2013). Study on Microstructure and Corrosion Resistance of Al_2CrFeNiCo_x CuTi High Entropy Alloy. Rare Metals and Cemented Carbides(4), 38-41. |
| IEEE | [1] HE Li, ZHANG Yun-peng, and QIU Xing-wu, "Study on Microstructure and Corrosion Resistance of Al_2CrFeNiCo_x CuTi High Entropy Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 38-41, 2013. keywords: {Al2 CrFeNiCox CuTi;high entropy alloy;laser cladding;polarization curve;microstructure} |