Enhancing Efficiency of Organic Solar Cells with Alkyl Diamines Doped PEDOT: PSS AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; Guangxi University; South China University of Technology; South China University of Technology; The Hong Kong Polytechnic University; Guangxi University; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Poly(3,4-ethylenedioxythiophene): poly(styrene-sulfonate) (PEDOT: PSS) has been the most popular conductive polymer as a hole transport material in organic solar cells (OSCs). Modification of PEDOT: PSS can improve its various properties to realize high performance in OSCs. The conductivity of PEDOT: PSS is an essential factor in determining device performance. In this work, PEDOT: PSS-BA, PEDOT: PSS-HA, and PEDOT: PSS-OA are prepared via facile doping of corresponding alkyl diamines into PEDOT: PSS, considering the amino ion can interact with redundant sulfonic acid groups of PSS. All the modified products exhibit enhanced conductivities due to their more ordered molecular packing comparing PEDOT: PSS. Using PTQ10 and m-BTP-PhC6 as the binary active layer, the OSC devices based on PEDOT: PSS-BA yield a superior power conversion efficiency of 18.44%, which ranks as one of the highest values in the binary OSCs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c01078

Chinese Library Classification Number:

Citation Information:

Poly(3,4-ethylenedioxythiophene): poly(styrene-sulfonate) (PEDOT: PSS) has been the most popular conductive polymer as a hole transport material in organic solar cells (OSCs). Modification of PEDOT: PSS can improve its various properties to realize high performance in OSCs. The conductivity of PEDOT: PSS is an essential factor in determining device performance. In this work, PEDOT: PSS-BA, PEDOT: PSS-HA, and PEDOT: PSS-OA are prepared via facile doping of corresponding alkyl diamines into PEDOT: PSS, considering the amino ion can interact with redundant sulfonic acid groups of PSS. All the modified products exhibit enhanced conductivities due to their more ordered molecular packing comparing PEDOT: PSS. Using PTQ10 and m-BTP-PhC6 as the binary active layer, the OSC devices based on PEDOT: PSS-BA yield a superior power conversion efficiency of 18.44%, which ranks as one of the highest values in the binary OSCs.

quote

GB/T 7714-2015 [1] Weixuan Liang, Jiaxing Huang, Zejun Wang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c01078.
MLA [1] Weixuan Liang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c01078.
APA [1] Weixuan Liang, Jiaxing Huang, Zejun Wang, Ciyuan Huang, Qi Wei, Chenghui Liao, Ruijie Ma, Tao Liu, Weiya Zhu, & Yuan Li. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c01078
IEEE [1] Weixuan Liang, Jiaxing Huang, Zejun Wang, Ciyuan Huang, Qi Wei, Chenghui Liao, Ruijie Ma, Tao Liu, Weiya Zhu, and Yuan Li, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c01078.