Single-Ion Conducting Polyurethane-Ester Solid Polymer Electrolyte Membrane toward Lithium Metal Batteries AITranslate

Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

It is a severe challenge to exploit single-ion polymer electrolytes combining excellent mechanical properties and ionic conductivities. Here, a polyurethane-ester single-ion polymer electrolyte membrane is prepared, and the relationship between the microstructure and the properties of ionomers is investigated. The electrolytes with different micro-phase morphologies, local hydrogen bonding states, ionic association states, and electrochemical properties are synthesized by regulating the chain length of polyethylene oxide (PEG). It is found that the hard domains of polyurethane electrolytes can ensure high carrier concentration and mechanical stability. All samples exhibit a two-phase behavior and low soft-phase glass-transition temperatures close to those of pure PEG, achieving good electrochemical, thermal, and mechanical properties. The membranes show outstanding interfacial compatibility and stability with lithium metal anodes, enabling the Li/LFP cells to exhibit excellent capacity (∼175 mA h g–1) as well as cycling stability at 0.1 C. Hence, the developed polyurethane-ester single-ion polymer electrolyte meets the application requirements of the next-generation lithium batteries.

KeyWords AITranslate

lithiumion battery singleion polymer electrolytes polyurethane microphase separation ion state
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c02197

Chinese Library Classification Number:

Citation Information:

It is a severe challenge to exploit single-ion polymer electrolytes combining excellent mechanical properties and ionic conductivities. Here, a polyurethane-ester single-ion polymer electrolyte membrane is prepared, and the relationship between the microstructure and the properties of ionomers is investigated. The electrolytes with different micro-phase morphologies, local hydrogen bonding states, ionic association states, and electrochemical properties are synthesized by regulating the chain length of polyethylene oxide (PEG). It is found that the hard domains of polyurethane electrolytes can ensure high carrier concentration and mechanical stability. All samples exhibit a two-phase behavior and low soft-phase glass-transition temperatures close to those of pure PEG, achieving good electrochemical, thermal, and mechanical properties. The membranes show outstanding interfacial compatibility and stability with lithium metal anodes, enabling the Li/LFP cells to exhibit excellent capacity (∼175 mA h g–1) as well as cycling stability at 0.1 C. Hence, the developed polyurethane-ester single-ion polymer electrolyte meets the application requirements of the next-generation lithium batteries.

quote

GB/T 7714-2015 [1] Naijie Wang, Di Qin, Qiu Sun, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c02197.
MLA [1] Naijie Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c02197.
APA [1] Naijie Wang, Di Qin, Qiu Sun, Xiangqun Chen, Ying Song, & Tiezhu Xin. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c02197
IEEE [1] Naijie Wang, Di Qin, Qiu Sun, Xiangqun Chen, Ying Song, and Tiezhu Xin, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c02197. keywords: {lithiumion battery;singleion polymer electrolytes;polyurethane;microphase separation;ion state}