Study on Microstructure of Zr-1Nb-0.1Fe-0.1Cu Zirconium Alloy AITranslate

Western Energy Material Technologies Co.,Ltd;Western Energy Material Technologies Co.,Ltd;Western Energy Material Technologies Co.,Ltd;Western Energy Material Technologies Co.,Ltd;Western Energy Material Technologies Co.,Ltd;Western Energy Material Technologies Co.,Ltd
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Zr-1 Nb-0.1 Fe-0.1 Cu plate samples with a thickness of 1.4 mm were prepared with sponge zirconium by electrode pressing,vacuum consumable arc melting,forging,homogenization treatment,quenching,hot rolling,multi-pass cold rolling and annealing.The metallographic microstructure of Zr-1 Nb-0.1 Fe-0.1 Cu alloy and the composition,size,structure and distribution of the second phase were analyzed by OM,SEM and TEM.The test results show that the metallographic microstructure of Zr-1 Nb-0.1 Fe-0.1 Cu alloy annealed at 580℃for 2 h is basically recrystallized equiaxed crystal,the grain size grade is 13,and the average grain size is less than 6μm.Elliptical second-phase particles are precipitated and dispersed in the grains and grain boundary of the alloy.More than 95%of the second-phase particles have smaller size than 200 nm.There are three kinds of second-phase particles in Zr-1 Nb-0.1 Fe-0.1 Cu alloy,includingβ-Nb precipitate with a large content,a grain size of less than 100 nm,and bcc structure,(Zr,Nb)2Fe precipitate with a less content,a grain size of less than 200 nm,and hcp structure,and Zr;Cu precipitate with the least content,a greater grain size than 200 nm,and tetragonal structure.

KeyWords AITranslate

zirconium alloy microstructure the second phase grain size Zr-Nb-Fe-Cu

1袁改焕,白新德,刘振球.我国锆、铪材加工技术的进步及发展[J].稀有金属快报,2004,23(10):1-4. 被引量:9

2姚美意,李士炉,张欣,彭剑超,周邦新,赵旭山,沈剑韵.添加Nb对Zr-4合金在500℃过热蒸汽中耐腐蚀性能的影响[J].金属学报,2011,47(7):865-871. 被引量:17

3姚美意,张宇,李士炉,张欣,周军,周邦新.Cu含量对Zr-0.80Sn-0.34Nb-0.39Fe-0.10Cr-xCu合金在500℃过热蒸汽中耐腐蚀性能的影响[J].金属学报,2011,47(7):872-876. 被引量:15

4张欣,姚美意,李中奎,周军,李强,周邦新.Zr-0.80Sn-0.4Nb-0.4Fe-0.10Cr-xCu合金在400℃过热蒸气中的耐腐蚀性能[J].稀有金属材料与工程,2013,42(6):1210-1214. 被引量:15

5赵文金,苗志,蒋宏曼,于晓卫,李卫军,李聪,周邦新.Zr-Sn-Nb合金的腐蚀行为研究[J].中国腐蚀与防护学报,2002,22(2):124-128. 被引量:39

6沈保罗,刘明,李聪,邱绍宇,应诗浩,曾明.氢对Zr-4合金在400℃时的低周疲劳性能的影响[J].稀有金属材料与工程,2007,36(7):1135-1139. 被引量:1

7梁建烈,唐轶媛,严嘉琳,朱其明,庄应烘,文国富.Zr-Sn-Nb-Fe合金金属间化合物及其α/β相变温度的研究[J].材料热处理学报,2009(1):32-35. 被引量:9

1王一心,炊鹏飞,李文刚,冯甜,程尊鹏,尹乐乐,柴步飞,任静静,刘芳辰,景然.Mo含量对生物医用Ti-Zr-Nb合金组织与性能的影响[J].铸造技术,2022,43(3):187-190.

2吴思静.优化英语课外阅读活动设计,全面落实英语学习活动观[J].英语画刊:高级,2022(3):40-42.

3文劲宇,周博,魏利屾.中国未来电力系统储电网初探[J].电力系统保护与控制,2022,50(7):1-10. 被引量:55

4吴剑峰.制度与组织:一个综合性理论——兼论新制度主义对法社会学的意义[J].法律和政治科学,2021(2):196-228. 被引量:1

5俄罗斯研发增强钛合金抗菌作用新技术[J].特种铸造及有色合金,2021,41(12):1548-1548.

6无.福建省人民政府关于省人大常委会会议对2021年上半年国民经济和社会发展计划执行情况报告审议意见办理情况的报告[J].福建省人民代表大会常务委员会公报,2021(6):184-188.

7李永春,尹建平,陈家进,伍志铭,黄奎,甘勇.成品退火对高纯铝箔显微组织及性能的影响[J].铝加工,2022(2):17-22. 被引量:1

8无.福建省人民政府关于省人大常委会会议对财政审计工作审议意见办理情况的报告[J].福建省人民代表大会常务委员会公报,2021(6):192-194.

9木子.国家发展改革委与广东代表团“云端”对话[J].人民之声,2022(3):36-36.

10周琳,刘运玺,付明杰.原位自生TiB增强Ti-55531合金复合材料组织与力学性能研究[J].钛工业进展,2022,39(2):33-37.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.4[金属学及工艺—金属材料]

Citation Information:

Zr-1 Nb-0.1 Fe-0.1 Cu plate samples with a thickness of 1.4 mm were prepared with sponge zirconium by electrode pressing,vacuum consumable arc melting,forging,homogenization treatment,quenching,hot rolling,multi-pass cold rolling and annealing.The metallographic microstructure of Zr-1 Nb-0.1 Fe-0.1 Cu alloy and the composition,size,structure and distribution of the second phase were analyzed by OM,SEM and TEM.The test results show that the metallographic microstructure of Zr-1 Nb-0.1 Fe-0.1 Cu alloy annealed at 580℃for 2 h is basically recrystallized equiaxed crystal,the grain size grade is 13,and the average grain size is less than 6μm.Elliptical second-phase particles are precipitated and dispersed in the grains and grain boundary of the alloy.More than 95%of the second-phase particles have smaller size than 200 nm.There are three kinds of second-phase particles in Zr-1 Nb-0.1 Fe-0.1 Cu alloy,includingβ-Nb precipitate with a large content,a grain size of less than 100 nm,and bcc structure,(Zr,Nb)2Fe precipitate with a less content,a grain size of less than 200 nm,and hcp structure,and Zr;Cu precipitate with the least content,a greater grain size than 200 nm,and tetragonal structure.

quote

GB/T 7714-2015 [1] QU Jing-wen, LEI Jiang, SHI Ming-hua, et al. Study on Microstructure of Zr-1Nb-0.1Fe-0.1Cu Zirconium Alloy[J]. Rare Metals and Cemented Carbides, 2022(2): 57-63.
MLA [1] QU Jing-wen, et al., "Study on Microstructure of Zr-1Nb-0.1Fe-0.1Cu Zirconium Alloy." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 57-63.
APA [1] QU Jing-wen, LEI Jiang, SHI Ming-hua, ZHOU Jun, LI Yu-li, & ZHANG Hai-xia. (2022). Study on Microstructure of Zr-1Nb-0.1Fe-0.1Cu Zirconium Alloy. Rare Metals and Cemented Carbides(2), 57-63.
IEEE [1] QU Jing-wen, LEI Jiang, SHI Ming-hua, ZHOU Jun, LI Yu-li, and ZHANG Hai-xia, "Study on Microstructure of Zr-1Nb-0.1Fe-0.1Cu Zirconium Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 57-63, 2022. keywords: {zirconium alloy;microstructure;the second phase;grain size;Zr-Nb-Fe-Cu}