Research on Catalytic Denitrification Performance of Rare Earth Tailings in CO Atmosphere AITranslate
Abstract AITranslate
The catalytic denitrification performance of Bayan Obo rare earth tailings was studied.The results show that the rare earth tailings have good catalytic denitration performance.With the increase of reaction temperature and carbon to nitrogen ratio,denitration efficiency of the tailings obviously increases.When carbon to nitrogen ratio is 4∶1 and temperature is 900 ℃,NO conversion rate with catalysis of un-calcined tailings reaches 97%.Fe element in the rare earth tailings exists mainly in the form of Fe2O3 and Fe3O4,and Fe element changes to a low-valent state during CO reduction of NO catalyzed by the tailings.The increase of Fe-containing substances and the synergistic effect of various substances can enhance the catalytic denitration activity of the tailings.The natural tailings contain a large amount of Ce^3+,and the amount further increases in CO reducing atmosphere to improve denitrification ability of the tailings.Temperature-programmed reduction experimental results show that the tailings have excellent reducing ability.
KeyWords AITranslate
1张世荣,涂赣峰,任存治,张成祥,李春材.氟碳铈矿热分解行为的研究[J].稀有金属,1998,22(3):185-189. 被引量:23
2张光学,周安琪,范海燕,王进卿,池作和.铁铈氧化物SCR脱硝催化剂的制备及性能[J].燃料化学学报,2015,43(10):1267-1272. 被引量:10
3王芳,姚桂焕,归柯庭.铁基催化剂选择性催化还原烟气脱硝特性比较研究[J].中国电机工程学报,2009,29(29):47-51. 被引量:19
4陈杏.低氮燃烧+选择性非催化还原烟气脱硝技术(SNCR)在循环流化床锅炉脱硝工程上的应用[J].能源环境保护,2013,27(4):33-35. 被引量:11
5向军,张成祥,涂赣峰,任存治.N_2气氛中氟碳铈矿焙烧产物分析[J].稀土,1994,15(1):66-68. 被引量:12
6苏亚欣,成豪,苏阿龙,邓文义.再燃脱硝过程中NO及HCN/NH_3的催化还原的研究进展[J].化工进展,2011,30(S1):714-717. 被引量:2
7刘艳华,车得福,惠世恩,徐通模.再燃技术研究现状及其在流化床中的应用前景[J].热力发电,2001,30(2):5-8. 被引量:5
8孙凡,朱涛,王磊,马建新.稀土氧化物上SO_2和NO的催化还原Ⅳ.掺杂Ce的钙钛矿型氧化物催化剂的脱硫和脱氮研究[J].化学世界,2005,46(7):389-392. 被引量:8
1胡志斐,王振峰,汪思瀛,武文斐,侯丽敏,张凯,白心蕊.矿物材料在催化脱硝方面的应用进展[J].矿产保护与利用,2021,41(1):161-165. 被引量:1
2戚瑞,龚志军,侯丽敏,武文斐.稀土尾矿催化半焦脱硝性能研究[J].煤炭转化,2021,44(3):68-75. 被引量:3
1刘丹丹,杨磊,李德文,汤晓君,汤春瑞.一种基于静电感应的检测脱硝网格堵塞的方法[J].煤炭转化,2021,44(6):75-80.
2张义,朱吉颖,张聪,王柔,邹羿菱云,吴振斌.硅藻土在环境领域的研究和应用[J].生态环境学报,2022,31(12):2441-2448.
3张钊,戚瑞,徐亚欣,龚志军.黄铁矿催化CO还原NO性能研究[J].钢铁钒钛,2022,43(6):109-114.
4张钊,戚瑞,徐亚欣,龚志军,武文斐.选铁尾矿催化煤粉脱硝的性能研究[J].煤炭转化,2023,46(2):92-98. 被引量:1
1李娜,张舒宁,梅哲跃,龚志军,罗慧娟,武文斐,张凯.稀土尾矿脱硝催化剂的制备及其CO还原NO性能研究[J].稀土,2019,40(6):88-95. 被引量:3
2张钟涛.草原上的矿山(散文)[J].草原,2019,0(10):45-49.
3王凯兴,龚志军,靳凯,武文斐.稀土精矿催化剂对选择性催化还原脱硝性能及表面吸附特性的研究[J].稀土,2019,40(6):57-65. 被引量:3
4焦坤灵,赵阳国,武文斐,王振峰,龚志军.SO2对稀土精矿催化剂NH3-SCR脱硝催化性能的影响[J].化工学报,2019,70(12):4645-4653. 被引量:3
5张贺,秘雪岳,孙妍,陈翠红,卢媛,展思辉,孙红文.NH3-SCR脱硝技术的研究现状与展望[J].实验室科学,2019,22(6):6-10. 被引量:3
6喻淼,张向飞.基于穴醚化合物对铈离子(Ce3+)的高灵敏选择性荧光检测[J].化学世界,2019,60(11):763-766.
7武蓓,何丽娟,罗瑞,林伟山,张万通,王勇,吴召林,金鑫,祁娟(甘肃农业大学草业学院,草业生态系统教育部重点实验室,甘肃省草业工程实验室,中-美草地.老芒麦体内碳氮分配对氮素添加的响应研究[J].草原与草坪,2019,39(6):19-25. 被引量:2
8李灿.超临界燃煤机组全负荷脱硝改造技术简析[J].电力系统装备,2019,0(23):70-71. 被引量:1
9李杰,曹会彦,黄志刚.干熄炉用碳化硅耐火材料抗CO侵蚀性研究[J].耐火材料,2019,53(6):464-467. 被引量:3
10刘建勋,陈美荣,崔瀛,杨剑平,吴智深.CeO2对玄武岩纤维耐高温性能的影响[J].稀土,2019,40(5):1-8. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:X756[环境科学与工程—环境工程]
Citation Information:
The catalytic denitrification performance of Bayan Obo rare earth tailings was studied.The results show that the rare earth tailings have good catalytic denitration performance.With the increase of reaction temperature and carbon to nitrogen ratio,denitration efficiency of the tailings obviously increases.When carbon to nitrogen ratio is 4∶1 and temperature is 900 ℃,NO conversion rate with catalysis of un-calcined tailings reaches 97%.Fe element in the rare earth tailings exists mainly in the form of Fe2O3 and Fe3O4,and Fe element changes to a low-valent state during CO reduction of NO catalyzed by the tailings.The increase of Fe-containing substances and the synergistic effect of various substances can enhance the catalytic denitration activity of the tailings.The natural tailings contain a large amount of Ce^3+,and the amount further increases in CO reducing atmosphere to improve denitrification ability of the tailings.Temperature-programmed reduction experimental results show that the tailings have excellent reducing ability.
quote
| GB/T 7714-2015 | [1] ZHU Chao, GONG Zhi-jun, JIN Kai, et al. Research on Catalytic Denitrification Performance of Rare Earth Tailings in CO Atmosphere[J]. Rare Metals and Cemented Carbides, 2019(6): 25-32. |
| MLA | [1] ZHU Chao, et al., "Research on Catalytic Denitrification Performance of Rare Earth Tailings in CO Atmosphere." Rare Metals and Cemented Carbides, no. 6, 2019, pp. 25-32. |
| APA | [1] ZHU Chao, GONG Zhi-jun, JIN Kai, LUO Hui-juan, & WU Wen-fei. (2019). Research on Catalytic Denitrification Performance of Rare Earth Tailings in CO Atmosphere. Rare Metals and Cemented Carbides(6), 25-32. |
| IEEE | [1] ZHU Chao, GONG Zhi-jun, JIN Kai, LUO Hui-juan, and WU Wen-fei, "Research on Catalytic Denitrification Performance of Rare Earth Tailings in CO Atmosphere," Rare Metals and Cemented Carbides, no. 6, pp. 25-32, 2019. keywords: {rare earth tailing;denitrification;catalysis;reduction;NO;CO} |