daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Biocompatible Lignin-Containing Hydrogels with Self-Adhesion, Conductivity, UV Shielding, and Antioxidant Activity as Wearable Sensors AITranslate

Ningde Normal University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University; Ningde Normal University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University; Fujian Agriculture and Forestry University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogels have drawn intensive attention as emerging materials for various applications in wearable sensors, soft robotics, and implantable devices. However, fabricating hydrogels with UV-shielding and antioxidant properties still remains a challenge. Herein, we prepared biocompatible 3-allyloxy-2-hydroxypropyl-lignin/polyacrylic acid (AHP-lignin/PAA) hydrogels with self-adhesion, conductivity, UV shielding, and antioxidant activity as wearable sensors by the incorporation of lignin into PAA. The structure, lap shear strength, and biocompatibility were characterized using the UV–vis spectrometer, universal testing machine, and cell test. The hydrogels showed strong adhesion to various substrates. The AHP-lignin/PAA hydrogels had excellent UV shielding and free radical scavenging capacity. Meanwhile, AHP-lignin/PAA hydrogels exhibited excellent sensitivity to tiny changes in low pressure. Notably, the hydrogels could adhere to the skin well without any other adhesives to monitor the movement signals of the body motion accurately. The biocompatible AHP-lignin/PAA hydrogels with self-adhesion, conductivity, UV shielding, and antioxidant activity offer great potential applications in wearable sensors.

KeyWords AITranslate

adhesive antioxidant conductive hydrogel lignin UV shielding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01817

Chinese Library Classification Number:

Citation Information:

Hydrogels have drawn intensive attention as emerging materials for various applications in wearable sensors, soft robotics, and implantable devices. However, fabricating hydrogels with UV-shielding and antioxidant properties still remains a challenge. Herein, we prepared biocompatible 3-allyloxy-2-hydroxypropyl-lignin/polyacrylic acid (AHP-lignin/PAA) hydrogels with self-adhesion, conductivity, UV shielding, and antioxidant activity as wearable sensors by the incorporation of lignin into PAA. The structure, lap shear strength, and biocompatibility were characterized using the UV–vis spectrometer, universal testing machine, and cell test. The hydrogels showed strong adhesion to various substrates. The AHP-lignin/PAA hydrogels had excellent UV shielding and free radical scavenging capacity. Meanwhile, AHP-lignin/PAA hydrogels exhibited excellent sensitivity to tiny changes in low pressure. Notably, the hydrogels could adhere to the skin well without any other adhesives to monitor the movement signals of the body motion accurately. The biocompatible AHP-lignin/PAA hydrogels with self-adhesion, conductivity, UV shielding, and antioxidant activity offer great potential applications in wearable sensors.

quote

GB/T 7714-2015 [1] Yanan Miao, Zuwu Tang, Qingwei Zhang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01817.
MLA [1] Yanan Miao, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01817.
APA [1] Yanan Miao, Zuwu Tang, Qingwei Zhang, Aikebaier Reheman, He Xiao, Min Zhang, Kai Liu, Liulian Huang, Lihui Chen, & Hui Wu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01817
IEEE [1] Yanan Miao, Zuwu Tang, Qingwei Zhang, Aikebaier Reheman, He Xiao, Min Zhang, Kai Liu, Liulian Huang, Lihui Chen, and Hui Wu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01817. keywords: {adhesive;antioxidant;conductive;hydrogel;lignin;UV shielding}