Study on the Effects of Electrolysis Temperature on Technical Indexes of Rare Earth Electrolytic Cell AITranslate

Xuzhou Jinshi Pengyuan Rare Earth Material Factory;Xuzhou Jinshi Pengyuan Rare Earth Material Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the existing theoretical research results about temperature field in rare earth electrolytic cell,and taking a 6 kA Pr-Nd electrolytic cell as the research object,the relationship between electrolysis temperature and the technical indexes of the rare earth molten salt electrolysis was analyzed according to the measured data during electrolysis production and chemical test results of RE metal products. The re sults show that electrolysis temperature plays an important role in normal electrolysis process. The opti mum electrolysis temperature is 1 090 ℃ to achieve efficient and stable production of the Pr Nd electrolytic cell.

KeyWords AITranslate

rare earth electrolytic cell electrolysis temperature technical index

1郑鑫,朱卫花,彭光怀,韩宝军,张小联.Nd_2O_3-NdF_3-LiF熔盐电解槽温度分布研究[J].赣南师范学院学报,2012,33(6):19-21. 被引量:1

2王军,王春慧,涂赣峰,任雁秋,米兰.10kA底部阴极稀土熔盐电解槽热平衡计算[J].稀土,2008,29(5):61-63. 被引量:12

3王俊,邓左民,张小联.10kA氟化物体系稀土熔盐电解槽热平衡测试研究[J].江西有色金属,2004,18(2):30-32. 被引量:10

4郭巧云,张小联.3kA钕电解槽温度分布研究[J].贵州师范大学学报:自然科学版,2013,31(5):84-86. 被引量:2

5周爱国,陈焱鑫,彭少华,王俊.硅对熔盐电解制备镨钕合金的影响[J].中国钨业,2012,27(2):44-46. 被引量:2

6郭海涛,贾海军,谢兵,任永红,王佐成.3000A金属钕电解槽的能量平衡[J].江西冶金,2007,27(3):13-16. 被引量:4

7张小联,胡珊玲,邓左民,王科军,彭光怀.应用有限元研究稀土电解槽温度场(英文)[J].计算机与应用化学,2006,23(6):535-537. 被引量:4

8伍永福,刘中兴,李曙阳,任永红.稀土熔盐电解槽内温度场数值模拟[J].有色金属:冶炼部分,2012(1):27-31. 被引量:18

9刘中兴,米兰,王春慧,石磊,贺友多.10kA氧化钕电解槽热平衡计算[J].内蒙古科技大学学报,2008,27(1):87-89. 被引量:6

10李建兵,万军,陈虎兵,米玺学.电解槽生产镨钕合金过程中碳含量的控制[J].稀有金属快报,2008,27(11):41-43. 被引量:4

1魏致慧,杨健壮.电解氧化镨工艺过程中石墨阳极的消耗研究[J].甘肃科技,2017,33(13):32-33. 被引量:1

2刘航,张耀,乔晓辉,栾义坤.熔盐电解法制备低氧低钛稀土金属研究[J].稀有金属与硬质合金,2021,49(2):5-8. 被引量:2

3杨培宏,王新春,刘玉宝,张耀,张自雷,吕东澔.稀土熔盐电解智能控制系统研究与应用[J].稀土,2022,43(3):34-40. 被引量:2

4冯小强,张学锋,何金辉,刘中兴,马守营.工艺参数对稀土电解槽的影响研究[J].内蒙古科技大学学报,2023,42(2):196-199.

1廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4

2熊志伟,刘爱民,刘玉宝,王旭,石忠宁.La_(2)O_(3)在LiF⁃NaF熔盐体系中的溶解行为[J].材料与冶金学报,2022,21(3):167-171.

3逄启寿,忻治霖,林小程,龚姚腾,王郅阳.稀土电解槽电化学三维时变流场数值模拟[J].有色金属科学与工程,2022,13(3):152-158. 被引量:1

4尚海,王新春.基于模糊控制的氧化稀土浓度控制研究[J].电工技术,2022(20):13-15.

5徐墨暄,王新春.基于ANFIS的氧化稀土浓度控制研究[J].电子元器件与信息技术,2023,7(6):225-229.

1白茂槐.我国稀土熔盐电解技术获重大突破[J].稀土信息,2003,9(4):17-17.

2R.Dasgupta,谢良贤.矿石和烧结矿强度指标之间的关系[J].烧结球团,1992,17(5):46-49.

3杨杰康,毛林猛,王福才,赵红全,周攻敏.配加钒钛磁铁精矿烧结试验[J].昆钢科技,2014,0(4):7-11.

4朱德庆,吴浩方.梅山烧结矿冷却废气热风烧结工艺的研究[J].烧结球团,1997,22(5):13-17. 被引量:9

5简讯[J].稀土信息,1994(6):8-8.

6杨雪峰,李轶.配合煤结焦特性与焦炭热态强度的关系[J].昆钢科技,2004(3):1-6.

7林伟清,肖祖高,钟延棕.阴极电流密度对熔盐电解技术经济指标影响的研究[J].赣南师范学院学报,2002,23(6):60-62. 被引量:2

8姜洪舟,唐莹,李娟娟,周建,袁润章.微波加热体的水量热法测温装置[J].辽宁石油化工大学学报,2006,26(4):41-43. 被引量:1

9巨国贤.包钢稀土(600111):加强行业自律促市场发展[J].中国金属通报,2008,0(25):19-20.

10栗丽,杨洗陈,董哲.激光熔覆中同轴粉末流温度场的CCD检测[J].中国激光,2009,36(9):2431-2437. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]

Citation Information:

Based on the existing theoretical research results about temperature field in rare earth electrolytic cell,and taking a 6 kA Pr-Nd electrolytic cell as the research object,the relationship between electrolysis temperature and the technical indexes of the rare earth molten salt electrolysis was analyzed according to the measured data during electrolysis production and chemical test results of RE metal products. The re sults show that electrolysis temperature plays an important role in normal electrolysis process. The opti mum electrolysis temperature is 1 090 ℃ to achieve efficient and stable production of the Pr Nd electrolytic cell.

quote

GB/T 7714-2015 [1] LIU Mu-gen, WANG Liang-liang. Study on the Effects of Electrolysis Temperature on Technical Indexes of Rare Earth Electrolytic Cell[J]. Rare Metals and Cemented Carbides, 2014(6): 16-19.
MLA [1] LIU Mu-gen, and WANG Liang-liang. "Study on the Effects of Electrolysis Temperature on Technical Indexes of Rare Earth Electrolytic Cell." Rare Metals and Cemented Carbides, no. 6, 2014, pp. 16-19.
APA [1] LIU Mu-gen, & WANG Liang-liang. (2014). Study on the Effects of Electrolysis Temperature on Technical Indexes of Rare Earth Electrolytic Cell. Rare Metals and Cemented Carbides(6), 16-19.
IEEE [1] LIU Mu-gen and WANG Liang-liang, "Study on the Effects of Electrolysis Temperature on Technical Indexes of Rare Earth Electrolytic Cell," Rare Metals and Cemented Carbides, no. 6, pp. 16-19, 2014. keywords: {rare earth;electrolytic cell;electrolysis temperature;technical index}