daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Multifunctional Liquid Crystal Polymer Networks: Azobenzene-Based Monoacrylate Molecules Impart a Photothermal Effect to Polymer Networks AITranslate

Jeonbuk National University; Jeonbuk National University; Jeonbuk National University; Jeonbuk National University; Jeonbuk National University; Jeonbuk National University; University of California; Sapienza University of Rome; Pusan National University; Jeonbuk National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Stimuli-responsive liquid crystal polymer networks (LCPNs) consisting of azobenzene are mostly studied based on ultraviolet (UV)-induced photochemical isomerization. However, depending on the molecular structure and the degree of UV absorption of azobenzene molecules, the photothermal effect can induce stimuli-responsiveness of azobenzene-based LCPN. In this report, an azobenzene-based monoacrylate (AM) monomer that can be easily introduced into an LCPN is designed and synthesized to develop a multifunctional LCPN that exhibits a photothermal effect. An AM LCPN is successfully fabricated with AM, LC monomer, and thiol groups, and the fabricating process is systematically optimized by controlling the ratio of each component. The thermal, mechanical, and structural behaviors of the AM LCPN are confirmed through various experimental analyses, and the shape memory properties are quantitatively and qualitatively verified via dynamic mechanical analysis and photographs. Thanks to the azobenzene molecules present, the AM LCPN exhibits a photothermal effect under UV exposure, which is demonstrated by macroscopic and spectroscopic experiments. Alignment and self-healing experiments indicate that the AM LCPN can be applied to fields requiring orientation or self-healing property.

KeyWords AITranslate

azobenzene photothermal effect shape memory alignment selfhealing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01866

Chinese Library Classification Number:

Citation Information:

Stimuli-responsive liquid crystal polymer networks (LCPNs) consisting of azobenzene are mostly studied based on ultraviolet (UV)-induced photochemical isomerization. However, depending on the molecular structure and the degree of UV absorption of azobenzene molecules, the photothermal effect can induce stimuli-responsiveness of azobenzene-based LCPN. In this report, an azobenzene-based monoacrylate (AM) monomer that can be easily introduced into an LCPN is designed and synthesized to develop a multifunctional LCPN that exhibits a photothermal effect. An AM LCPN is successfully fabricated with AM, LC monomer, and thiol groups, and the fabricating process is systematically optimized by controlling the ratio of each component. The thermal, mechanical, and structural behaviors of the AM LCPN are confirmed through various experimental analyses, and the shape memory properties are quantitatively and qualitatively verified via dynamic mechanical analysis and photographs. Thanks to the azobenzene molecules present, the AM LCPN exhibits a photothermal effect under UV exposure, which is demonstrated by macroscopic and spectroscopic experiments. Alignment and self-healing experiments indicate that the AM LCPN can be applied to fields requiring orientation or self-healing property.

quote

GB/T 7714-2015 [1] Minwoo Rim, Dayoung Jung, Dongmin Yu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01866.
MLA [1] Minwoo Rim, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01866.
APA [1] Minwoo Rim, Dayoung Jung, Dongmin Yu, Hyeyoon Ko, Junhwa Jang, Mintaek Oh, YuJin Choi, Luciano De Sio, Sukkyun Ahn, & KwangUn Jeong. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01866
IEEE [1] Minwoo Rim, Dayoung Jung, Dongmin Yu, Hyeyoon Ko, Junhwa Jang, Mintaek Oh, YuJin Choi, Luciano De Sio, Sukkyun Ahn, and KwangUn Jeong, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01866. keywords: {azobenzene;photothermal effect;shape memory;alignment;selfhealing}