Gold Polyiodide Hybrid Perovskite Solar Cells AITranslate
Abstract AITranslate
In this work, we present the ionic liquid (IL) synthesis of two novel pseudo-2D perovskite-type gold(III)polyiodide compounds, [DodMe2S][AuI4][I3] (1) and [Et3S][AuI4][I5] (2), and their application as active layers in monolithic solar cells. The compounds are composed of tetraiodoaurate anions and polyiodide entities, infinite polyiodide chains in 1 and pentaiodides in 2, which display short intermolecular contacts resulting in relatively small electronic bandgaps. This work represents the first demonstration of film deposition of gold iodide/polyiodide compounds onto porous monolithic substrates with subsequent solar cell characterization. The devices show promising photovoltaic performance and could unlock new materials design possibilities, ultimately moving away from lead-based photovoltaic materials. These findings further highlight the use of simple polyiodide entities to increase the structural and electronic dimensionality of gold perovskite-type anions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c00490
Chinese Library Classification Number:
Citation Information:
In this work, we present the ionic liquid (IL) synthesis of two novel pseudo-2D perovskite-type gold(III)polyiodide compounds, [DodMe2S][AuI4][I3] (1) and [Et3S][AuI4][I5] (2), and their application as active layers in monolithic solar cells. The compounds are composed of tetraiodoaurate anions and polyiodide entities, infinite polyiodide chains in 1 and pentaiodides in 2, which display short intermolecular contacts resulting in relatively small electronic bandgaps. This work represents the first demonstration of film deposition of gold iodide/polyiodide compounds onto porous monolithic substrates with subsequent solar cell characterization. The devices show promising photovoltaic performance and could unlock new materials design possibilities, ultimately moving away from lead-based photovoltaic materials. These findings further highlight the use of simple polyiodide entities to increase the structural and electronic dimensionality of gold perovskite-type anions.
quote
| GB/T 7714-2015 | [1] Allan Starkholm, Lars Kloo, Per H. Svensson. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00490. |
| MLA | [1] Allan Starkholm, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00490. |
| APA | [1] Allan Starkholm, Lars Kloo, & Per H. Svensson. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00490 |
| IEEE | [1] Allan Starkholm, Lars Kloo, and Per H. Svensson, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00490. |