Study of Reactive Plasma Spraying of TiN-Al_3Ti-Al Composite Coating AITranslate

School of Materials at Hebei University of Technology;School of Materials at Hebei University of Technology;School of Materials at Hebei University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

TiN-Al3Ti-Al composite coating is prepared by reactive plasma spraying. Phase analysis and surface morphological analysis is done through XRD,SEM. The results show that the coating mainly consists of TiN-Al3Ti-Al;the structure of the coating is multilayer which includes rich horniness and rich flexible composition stacking together. The Vickers-hardness indentation and the fractography show that the toughness of the composite coatings is much better than that of the Al2O3 coatings.

KeyWords AITranslate

plasma spraying reactive plasma spraying TiN-Al3Ti-Al composite coating

1Akira Kobayashi.Formation of high hardness zirlonia coatings by gas tunnel type plasma spraying[J].Surface & Coatings Technology,1997,90:197-202.

2石玉龙,彭红瑞,李世直,李建华.高速钢工件表面物理化学气相沉积TiN[J].金属热处理,1997(11):22-23. 被引量:10

3程宇航.刀具涂层材料的使用概况[J].材料导报,1998,12(6):45-47. 被引量:9

4薛玉娥,林香祝,陈仁悟.氮化钛涂层的磨损特性[J].稀有金属材料与工程,1990(2):42-46. 被引量:5

5Dallaire Sand Cliché G.The influence of composition and process parameters on the microstructure of TiC-Fe multiphase and multilayer coatings[J].Surface & Coatings Technology,1992,50:233-239.

6陈文威.金属表面涂层技术及应用[M].北京:人民交通出版社,1996.99-101.

1索.,ИН,谷守铭.用喷涂法制作热风炉炉衬[J].钢铁译文集,1992(3):89-92.

2陈石卿.高品质钛[J].钛合金信息,1995(6):5-7.

3高永义.Fe-Ti-C系反应等离子喷涂粉末制备工艺比较[J].一重技术,2013(3):39-41.

4许纯良,徐宏权.绝热板冷中间包喷涂防氧化涂料新技术[J].首钢科技,1989(1):21-23.

5吴晓莉,杨德统.含镍粉末冶金钢的组织与镍的分布[J].南京理工大学学报,2001,25(4):400-403. 被引量:1

6王连超,谢佳,席赟.多孔金属陶瓷膜研究进展[J].粉末冶金工业,2016,26(3):69-77. 被引量:9

7郝艳霞,朱俊武,杨绪杰,陆路德,汪信.溶胶-凝胶法Al_2O_3涂层碳纤维的制备与表征[J].南京理工大学学报,2004,28(6):653-657. 被引量:3

8王剑泯.宝钢高炉用喷涂法施工新型渣棉陶棉纤维[J].施工技术与管理,1991(1):25-33.

9李晓红,解子章,杨让,胡淑文.机械活化Mo-Cu粉末的烧结[J].北京科技大学学报,1996,18(5):424-427. 被引量:6

10陈联满,罗秀梅,杨丽珠.机尾电除尘风机破裂分析[J].理化检验:物理分册,1999,35(11):508-511.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.41[冶金工程—粉末冶金]

Citation Information:

TiN-Al3Ti-Al composite coating is prepared by reactive plasma spraying. Phase analysis and surface morphological analysis is done through XRD,SEM. The results show that the coating mainly consists of TiN-Al3Ti-Al;the structure of the coating is multilayer which includes rich horniness and rich flexible composition stacking together. The Vickers-hardness indentation and the fractography show that the toughness of the composite coatings is much better than that of the Al2O3 coatings.

quote

GB/T 7714-2015 [1] ZOU Dong-li, YAN Dian-ran, HE Ji-ning. Study of Reactive Plasma Spraying of TiN-Al_3Ti-Al Composite Coating[J]. Rare Metals and Cemented Carbides, 2007(1): 14-17.
MLA [1] ZOU Dong-li, et al., "Study of Reactive Plasma Spraying of TiN-Al_3Ti-Al Composite Coating." Rare Metals and Cemented Carbides, no. 1, 2007, pp. 14-17.
APA [1] ZOU Dong-li, YAN Dian-ran, & HE Ji-ning. (2007). Study of Reactive Plasma Spraying of TiN-Al_3Ti-Al Composite Coating. Rare Metals and Cemented Carbides(1), 14-17.
IEEE [1] ZOU Dong-li, YAN Dian-ran, and HE Ji-ning, "Study of Reactive Plasma Spraying of TiN-Al_3Ti-Al Composite Coating," Rare Metals and Cemented Carbides, no. 1, pp. 14-17, 2007. keywords: {plasma spraying reactive plasma spraying, TiN-Al3Ti-Al, composite coating}