daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Modifiable, Spontaneously Formed Polymer Gel with Zwitterionic and N-Hydroxysuccinimide Moieties for an Enzymatic Biofuel Cell AITranslate

The University of Tokyo; The University of Tokyo; The University of Tokyo
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A modifiable, spontaneously formed and biocompatible polymer gel, composed of phosphorylcholine and N-hydroxysuccinimide ester, is reported, which can be subjected to postmodification by amine-containing mediators to obtain a redox zwitterionic gel. Owing to attractive interactions between the polymer chains, the network structure of the polymer gel is formed spontaneously in ethanol or water. In addition, the designed hydrogel can serve as an enzyme-immobilizing matrix for enzymatic bioelectrodes. We illustrate the potential applications of the hydrogel with a biofuel cell that demonstrated superior operational stability over 10 days and the unaffected current of the bioelectrode in concentrated protein solution (45 mg mL–1). Compared with a typical redox hydrogel, the zwitterionic moieties with high hydration endow the redox zwitterionic hydrogel with (i) better environment for preserving enzyme’s activity and (ii) resistance to biofouling caused by protein adsorption. These properties contribute to overcoming the most challenging issues in the field of implantable bioelectronic applications, as insufficient operational stability and lack of biocompatibility severely limit their feasibility for practical applications.

KeyWords AITranslate

zwitterionic polymer redox hydrogel biofuel cells antifouling enzyme immobilization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.0c00881

Chinese Library Classification Number:

Citation Information:

A modifiable, spontaneously formed and biocompatible polymer gel, composed of phosphorylcholine and N-hydroxysuccinimide ester, is reported, which can be subjected to postmodification by amine-containing mediators to obtain a redox zwitterionic gel. Owing to attractive interactions between the polymer chains, the network structure of the polymer gel is formed spontaneously in ethanol or water. In addition, the designed hydrogel can serve as an enzyme-immobilizing matrix for enzymatic bioelectrodes. We illustrate the potential applications of the hydrogel with a biofuel cell that demonstrated superior operational stability over 10 days and the unaffected current of the bioelectrode in concentrated protein solution (45 mg mL–1). Compared with a typical redox hydrogel, the zwitterionic moieties with high hydration endow the redox zwitterionic hydrogel with (i) better environment for preserving enzyme’s activity and (ii) resistance to biofouling caused by protein adsorption. These properties contribute to overcoming the most challenging issues in the field of implantable bioelectronic applications, as insufficient operational stability and lack of biocompatibility severely limit their feasibility for practical applications.

quote

GB/T 7714-2015 [1] Yixuan Huang, Tsukuru Masuda, Madoka Takai. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c00881.
MLA [1] Yixuan Huang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c00881.
APA [1] Yixuan Huang, Tsukuru Masuda, & Madoka Takai. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c00881
IEEE [1] Yixuan Huang, Tsukuru Masuda, and Madoka Takai, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c00881. keywords: {zwitterionic polymer;redox hydrogel;biofuel cells;antifouling;enzyme immobilization}