Study on the Effect of Calcination Temperature on the Performance of Mn-Ce/TiO2 Denitration Catalyst AITranslate
Abstract AITranslate
The Mn-Ce/TiO2 catalysts prepared by impregnation method were calcined at 300~500℃.XRD,BET,XPS,H2-TPR,NH3-TPD and denitration performance tests were conducted to investigate the effect of calcination temperature on the physical and chemical properties and denitration efficiency of Mn-Ce/TiO2 denitration catalysts.The results show that the proper calcination temperature(400℃)is beneficial to increase the content of Mn4+,Ce3+and chemisorbed oxygen(Oα)of the catalyst,which can promote the denitration reaction.However,excessive calcination temperature(≥450℃)will lead to the increase of the particle size and the decrease of the dispersion of the active component MnOx in the catalyst,and the decrease of the specific surface area of the catalyst.moreover,high calcination temperature also causes the decrease of the n(Mn4+)/n(Mn2++Mn3++Mn4+),n(Ce3+)/n(Ce3++Ce4+),n(Oα)/n(Oα+Oβ)and reducibility of the catalyst,which has an adverse effect on the denitration activity.The catalyst prepared at a calcination temperature of 400℃exhibits the best denitration activity within the flue gas temperature range of 120~270℃.
KeyWords AITranslate
Basic Information:
DOI:
Chinese Library Classification Number:TQ426.6[化学工程]
Citation Information:
The Mn-Ce/TiO2 catalysts prepared by impregnation method were calcined at 300~500℃.XRD,BET,XPS,H2-TPR,NH3-TPD and denitration performance tests were conducted to investigate the effect of calcination temperature on the physical and chemical properties and denitration efficiency of Mn-Ce/TiO2 denitration catalysts.The results show that the proper calcination temperature(400℃)is beneficial to increase the content of Mn4+,Ce3+and chemisorbed oxygen(Oα)of the catalyst,which can promote the denitration reaction.However,excessive calcination temperature(≥450℃)will lead to the increase of the particle size and the decrease of the dispersion of the active component MnOx in the catalyst,and the decrease of the specific surface area of the catalyst.moreover,high calcination temperature also causes the decrease of the n(Mn4+)/n(Mn2++Mn3++Mn4+),n(Ce3+)/n(Ce3++Ce4+),n(Oα)/n(Oα+Oβ)and reducibility of the catalyst,which has an adverse effect on the denitration activity.The catalyst prepared at a calcination temperature of 400℃exhibits the best denitration activity within the flue gas temperature range of 120~270℃.
quote
| GB/T 7714-2015 | [1] YUE Yan-wei, HUANG Li, LU Lu-yang, et al. Study on the Effect of Calcination Temperature on the Performance of Mn-Ce/TiO2 Denitration Catalyst[J]. Rare Metals and Cemented Carbides, 2026(1): 108-113. |
| MLA | [1] YUE Yan-wei, et al., "Study on the Effect of Calcination Temperature on the Performance of Mn-Ce/TiO2 Denitration Catalyst." Rare Metals and Cemented Carbides, no. 1, 2026, pp. 108-113. |
| APA | [1] YUE Yan-wei, HUANG Li, LU Lu-yang, WANG Su-qin, ZONG Yu-hao, LI Jin-ke, WANG Hu, & GUO Li-xing. (2026). Study on the Effect of Calcination Temperature on the Performance of Mn-Ce/TiO2 Denitration Catalyst. Rare Metals and Cemented Carbides(1), 108-113. |
| IEEE | [1] YUE Yan-wei, HUANG Li, LU Lu-yang, WANG Su-qin, ZONG Yu-hao, LI Jin-ke, WANG Hu, and GUO Li-xing, "Study on the Effect of Calcination Temperature on the Performance of Mn-Ce/TiO2 Denitration Catalyst," Rare Metals and Cemented Carbides, no. 1, pp. 108-113, 2026. keywords: {calcination temperature;denitration catalyst;Mn-Ce/TiO;denitration efficiency} |