Polymer Surface Oxidation by Light-Activated Chlorine Dioxide Radical for Metal–Plastics Adhesion AITranslate
Abstract AITranslate
Metal–plastics adhesion has received much attention from researchers due to its potential use in various industrial applications. However, the adhesion of plastics with metals is poor due to the low surface energy of plastics. Accordingly, the adhesion of plastics usually requires surface modification or the use of an adhesive primer. Recently, we developed a polymer surface modification method using the light-activated chlorine dioxide (ClO2•) radical as oxidant. In this study, we investigated the adhesion behavior of PP film modified by this method. Improvements in hydrophilicity and adhesion property of PP were observed after oxidation. The oxidized PP film exhibited good adhesive properties with Al plate without any adhesives, and the adhesion strength could be further enhanced by increasing the oxidation temperature. Moreover, this study successfully developed an approach for the electroless metal plating on polymer surfaces. In addition, we also found that light irradiation only activated ClO2• but had no direct modification on plastics.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00871
Chinese Library Classification Number:
Citation Information:
Metal–plastics adhesion has received much attention from researchers due to its potential use in various industrial applications. However, the adhesion of plastics with metals is poor due to the low surface energy of plastics. Accordingly, the adhesion of plastics usually requires surface modification or the use of an adhesive primer. Recently, we developed a polymer surface modification method using the light-activated chlorine dioxide (ClO2•) radical as oxidant. In this study, we investigated the adhesion behavior of PP film modified by this method. Improvements in hydrophilicity and adhesion property of PP were observed after oxidation. The oxidized PP film exhibited good adhesive properties with Al plate without any adhesives, and the adhesion strength could be further enhanced by increasing the oxidation temperature. Moreover, this study successfully developed an approach for the electroless metal plating on polymer surfaces. In addition, we also found that light irradiation only activated ClO2• but had no direct modification on plastics.
quote
| GB/T 7714-2015 | [1] Yankun Jia, Jiaxin Chen, Haruyasu Asahara, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00871. |
| MLA | [1] Yankun Jia, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00871. |
| APA | [1] Yankun Jia, Jiaxin Chen, Haruyasu Asahara, TakaAki Asoh, & Hiroshi Uyama. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00871 |