Abstract AITranslate

Cerium rich concentrate was employed as the raw material,dissolved in sulfuric acid and then separated by extraction with P204-kerosene.The raffinate was neutralized with MgO and then separated by extraction again with P204-kerosene,realizing tetravalent cerium separation from other trivalent rare earth and obtaining qualified cerium products and mixed rare earth chloride for the national standards.

KeyWords AITranslate

cerium rich concentrate Ce refinement extraction mixed rare earth chloride rare earth smelting by-product

1徐光宪.白云鄂博矿钍资源开发利用迫在眉睫[J].稀土信息,2005,11(5):4-5. 被引量:28

1甘肃省引进北方稀土重组甘肃稀土新材料[J].新材料产业,2018,0(2):95-95.

2图嘎,张燕.影响混合稀土金属电解过程的几个因素[J].内蒙古科技与经济,1999,0(6):49-49.

3胡丽芳.如何保存眼药[J].财会月刊,2015,0(11).

4赵凤英,白雪峰.角膜胶原膜治疗眼碱烧伤[J].中外健康文摘:临床医师,2007,4(7):91-91.

5晏晓清,曹丹,张艳芳,何新安,李玉强.高效液相色谱法同时测定植物油中BaP、BHT、BHA、TBHQ的含量[J].科学中国人,2017,0(3X):52-52.

6刘杰,黄焜,吴怀之,刘会洲.大相比鼓泡油膜萃取氰化废水中的低浓度金[J].中国有色金属学报,2018,28(1):199-204. 被引量:3

7郑丽卿,方志成,崔锦良,金秋萍,阙小峰,司文会.火焰原子吸收光度法测定奥美拉唑镁原料药中的镁含量[J].健康之路,2017,0(4):259-259.

8张红梅.珍菊降压片生产工艺改进[J].中外健康文摘:医药月刊,2007,4(1):77-79. 被引量:1

9孙辉,毛志幸,陈宗道.茶膏包埋型泡腾片制备工艺优化和质量分析[J].食品工业,2018,39(2):156-162. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

Cerium rich concentrate was employed as the raw material,dissolved in sulfuric acid and then separated by extraction with P204-kerosene.The raffinate was neutralized with MgO and then separated by extraction again with P204-kerosene,realizing tetravalent cerium separation from other trivalent rare earth and obtaining qualified cerium products and mixed rare earth chloride for the national standards.

quote

GB/T 7714-2015 [1] WANG Hong-wei, LIU Yun-long. Research on Refinement of Cerium Rich Concentrate as Rare Earth Smelting By-product[J]. Rare Metals and Cemented Carbides, 2017(6): 5-7.
MLA [1] WANG Hong-wei, and LIU Yun-long. "Research on Refinement of Cerium Rich Concentrate as Rare Earth Smelting By-product." Rare Metals and Cemented Carbides, no. 6, 2017, pp. 5-7.
APA [1] WANG Hong-wei, & LIU Yun-long. (2017). Research on Refinement of Cerium Rich Concentrate as Rare Earth Smelting By-product. Rare Metals and Cemented Carbides(6), 5-7.
IEEE [1] WANG Hong-wei and LIU Yun-long, "Research on Refinement of Cerium Rich Concentrate as Rare Earth Smelting By-product," Rare Metals and Cemented Carbides, no. 6, pp. 5-7, 2017. keywords: {cerium rich concentrate;Ce;refinement;extraction;mixed rare earth chloride;rare earth smelting by-product}