Optimization of Ammonium Tungstate Evaporation and Crystallization Process by Response Surface Method AITranslate
Abstract AITranslate
The process of preparing APT by evaporation and crystallization method is simple, but the particle size of the prepared APT is relatively large, which seriously reduces the quality of subsequent products.The influences of stirring speed, ammonium tungstate concentration, and reaction temperature on the D;and Span of APT were studied by response surface method, and then the evaporation and crystallization process of APT was optimized.The results show that among the three factors, the order of influence on D;is reaction temperature>ammonium tungstate concentration>stirring speed, and the order of influence on Span is ammonium tungstate concentration>stirring speed>reaction temperature.The optimal process conditions are stirring speed of 271 r/min, ammonium tungstate concentration of 178.9 g/L,and reaction temperature of 81.6 ℃.Under the optimal process conditions, the D;and Span of the APT prepared in the experiment are 20.31 μm and 1.323,respectively, which are greatly reduced compared with other samples.The reason for the reduction is that low stirring speed and low reaction temperature inhibit crystal growth, and high ammonium tungstate concentration promotes crystal nucleation.
KeyWords AITranslate
1张璐,陆必志,徐涛.超细碳化钨制备关键技术及评价方法研究的新进展[J].硬质合金,2019,36(6):460-471. 被引量:13
2毛善文,尹超.原始WC粉末粒度分布及球磨时间对超细硬质合金微观结构的影响[J].硬质合金,2019,36(2):126-134. 被引量:8
3朱斌,柏振海,高阳,罗兵辉.WC粒度对WC-15Fe-5Ni硬质合金组织与性能的影响[J].中国有色金属学报,2016,26(5):1065-1074. 被引量:11
4冯志扬,李祖来,山泉,蒋业华,周荣.颗粒粒度对碳化钨颗粒增强铁基复合材料界面的影响[J].材料工程,2016,44(1):83-88. 被引量:16
5万林生,曾学品,赖星任,杨亮,刘鹏.仲钨酸铵结晶掺Cr制备的WC粉和超细硬质合金的性能研究[J].稀有金属与硬质合金,2016,44(6):54-59. 被引量:6
6陈亿,谢中华,李继红,徐双,余春荣,张威.连续结晶法制备粗颗粒仲钨酸铵工艺研究[J].中国钨业,2020,35(2):61-66. 被引量:4
7郭圣达,羊建高,朱二涛,陈颢,吕健.WC-Co复合粉形貌遗传特性及粒度分布研究[J].稀有金属材料与工程,2016,45(5):1330-1334. 被引量:5
8王文华,谢中华,陈树茂,张秋和,江应国.仲钨酸铵形貌和粒度分布对钨粉压坯强度的影响[J].中国钨业,2013,28(2):38-40. 被引量:5
9谢凡,时凯华,顾金宝.优质WC用氧化钨的质量控制[J].硬质合金,2020,37(6):472-481. 被引量:2
10刘觐,易志强,谭敦强,陆磊,康林萍,陈志刚.中和-蒸发联合结晶法制备高品质仲钨酸铵的工艺及机理研究[J].江西科学,2019,37(4):590-594. 被引量:3
1刘晶.煤化工高盐废水的蒸发结晶工艺技术研究[J].化工管理,2023(6):162-164. 被引量:1
1吴琼,王振宇,王迪,李龙刚,邹兆辉.浅析运行工况对单效蒸发器效率的影响[J].水污染及处理,2023,11(3):69-75.
1次仁德吉.响应曲面法优化西藏黑青稞中多酚提取工艺[J].大麦与谷类科学,2022,39(2):42-50.
2李冰,张立攀,王春杰,王俊朋,赵梦瑶,关炳峰,胡桂芳,王永.杜仲叶超微粉馒头制备工艺及品质特性分析[J].食品安全质量检测学报,2022,13(7):2184-2193. 被引量:2
3诸向东,肖劲,毛秋云,张振华,唐雷,仲奇凡.恒压酸浸法回收退役锂离子电池废炭渣[J].中国有色金属学报:英文版,2022,32(5):1691-1704. 被引量:1
4黄硕,胡雨欣,沙露平,刘剑桥,郭永学.响应曲面法优化植物甾醇固体自微乳的工艺条件[J].过程工程学报,2022,22(4):533-541. 被引量:1
5王伟云,王康妮,黄圣钊,毛燎原.有机酸和路易斯酸对玉米芯和玉米秸秆生物质水热法制备木糖影响研究[J].太阳能学报,2022,43(4):480-485.
6苏学军,裘可,范文赟.氧化石墨烯辅助乙醇提取荞麦壳中总黄酮的工艺研究[J].中国饲料,2022(9):108-112. 被引量:1
7黎春红,邱铃岚,雷长毅,汪开拓.小蓟多糖—诺米林复合涂膜剂制备工艺的优化及对柠檬果实贮藏品质的影响[J].西南农业学报,2022,35(3):550-557.
8徐媛,王璐,冷艳,曹新华.藜蒿黄酮微胶囊工艺优化及释放动力学研究[J].食品工业科技,2022,43(9):185-193. 被引量:2
9王兰,钱斌,赖敏辉,严冬霞,宋岑,徐岳正.免浸米的黄酒酿造新工艺研究[J].酿酒科技,2022(5):56-60.
10张梦宇,侯敏婕,时焕军,贾乐,张建军.红平菇锌多糖咀嚼片制备工艺及其体外抗氧化活性研究[J].微生物学杂志,2022,42(2):108-116.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
The process of preparing APT by evaporation and crystallization method is simple, but the particle size of the prepared APT is relatively large, which seriously reduces the quality of subsequent products.The influences of stirring speed, ammonium tungstate concentration, and reaction temperature on the D;and Span of APT were studied by response surface method, and then the evaporation and crystallization process of APT was optimized.The results show that among the three factors, the order of influence on D;is reaction temperature>ammonium tungstate concentration>stirring speed, and the order of influence on Span is ammonium tungstate concentration>stirring speed>reaction temperature.The optimal process conditions are stirring speed of 271 r/min, ammonium tungstate concentration of 178.9 g/L,and reaction temperature of 81.6 ℃.Under the optimal process conditions, the D;and Span of the APT prepared in the experiment are 20.31 μm and 1.323,respectively, which are greatly reduced compared with other samples.The reason for the reduction is that low stirring speed and low reaction temperature inhibit crystal growth, and high ammonium tungstate concentration promotes crystal nucleation.
quote
| GB/T 7714-2015 | [1] XU Li-hua, CHENG Hua-jin, LIU Qing-sheng. Optimization of Ammonium Tungstate Evaporation and Crystallization Process by Response Surface Method[J]. Rare Metals and Cemented Carbides, 2022(2): 8-14. |
| MLA | [1] XU Li-hua, et al., "Optimization of Ammonium Tungstate Evaporation and Crystallization Process by Response Surface Method." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 8-14. |
| APA | [1] XU Li-hua, CHENG Hua-jin, & LIU Qing-sheng. (2022). Optimization of Ammonium Tungstate Evaporation and Crystallization Process by Response Surface Method. Rare Metals and Cemented Carbides(2), 8-14. |
| IEEE | [1] XU Li-hua, CHENG Hua-jin, and LIU Qing-sheng, "Optimization of Ammonium Tungstate Evaporation and Crystallization Process by Response Surface Method," Rare Metals and Cemented Carbides, no. 2, pp. 8-14, 2022. keywords: {APT;ammonium tungstate;response surface method;evaporation and crystallization;D50;Span} |