daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Synergistic Approach of Interfacial Layer Engineering and READ-Voltage Optimization in HfO2-Based FeFETs for In-Memory-Computing Applications Synergistic Approach of Interfacial Layer Engineering and READ-Voltage Optimization in HfO2-Based FeFETs for In-Memory-Computing Applications AITranslate

Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;GlobalFoundries;GlobalFoundries;GlobalFoundries;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Fraunhofer-Institut für Photonische Mikrosysteme IPMS - Center Nanoelectronic Technologies;Technische Universität Bergakademie Freiberg
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This article reports an improvement in the performance of the hafnium oxide-based (HfO2) ferroelectric field-effect transistors (FeFET) achieved by a synergistic approach of interfacial layer (IL) engineering and READ-voltage optimization. FeFET devices with silicon dioxide (SiO2) and silicon oxynitride (SiON) as IL were fabricated and characterized. Although the FeFETs with SiO2 interfaces demonstrated better low-frequency characteristics compared to the FeFETs with SiON interfaces, the latter demonstrated better WRITE endurance and retention. Finally, the neuromorphic simulation was conducted to evaluate the performance of FeFETs with SiO2 and SiON IL as synaptic devices. We observed that the WRITE endurance in both types of FeFETs was insufficient (<108)(<108) to carry out online neural network training. Therefore, we consider an inference-only operation with offline neural network training. The system-level simulation reveals that the impact of systematic degradation via retention degradation is much more significant for inference-only operation than low-frequency noise. The neural network with FeFETs based on SiON IL in the synaptic core shows 96% accuracy for the inference operation on the handwritten digit from the Modified National Institute of Standards and Technology (MNIST) data set in the presence of flicker noise and retention degradation, which is only a 2.5% deviation from the software baseline.

KeyWords AITranslate

neuromorphic computing Flicker noise interface traps FeFET hafnium oxide interface treatments
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00771

Chinese Library Classification Number:

Citation Information:

This article reports an improvement in the performance of the hafnium oxide-based (HfO2) ferroelectric field-effect transistors (FeFET) achieved by a synergistic approach of interfacial layer (IL) engineering and READ-voltage optimization. FeFET devices with silicon dioxide (SiO2) and silicon oxynitride (SiON) as IL were fabricated and characterized. Although the FeFETs with SiO2 interfaces demonstrated better low-frequency characteristics compared to the FeFETs with SiON interfaces, the latter demonstrated better WRITE endurance and retention. Finally, the neuromorphic simulation was conducted to evaluate the performance of FeFETs with SiO2 and SiON IL as synaptic devices. We observed that the WRITE endurance in both types of FeFETs was insufficient (<108)(<108) to carry out online neural network training. Therefore, we consider an inference-only operation with offline neural network training. The system-level simulation reveals that the impact of systematic degradation via retention degradation is much more significant for inference-only operation than low-frequency noise. The neural network with FeFETs based on SiON IL in the synaptic core shows 96% accuracy for the inference operation on the handwritten digit from the Modified National Institute of Standards and Technology (MNIST) data set in the presence of flicker noise and retention degradation, which is only a 2.5% deviation from the software baseline.

quote

GB/T 7714-2015 [1] Yannick Raffel, Sourav De, Maximilian Lederer, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00771.
MLA [1] Yannick Raffel, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00771.
APA [1] Yannick Raffel, Sourav De, Maximilian Lederer, Ricardo Revello Olivo, Raik Hoffmann, Sunanda Thunder, Luca Pirro, Sven Beyer, Talha Chohan, Thomas Kämpfe, Konrad Seidel, & Johannes Heitmann. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00771
IEEE [1] Yannick Raffel, Sourav De, Maximilian Lederer, Ricardo Revello Olivo, Raik Hoffmann, Sunanda Thunder, Luca Pirro, Sven Beyer, Talha Chohan, Thomas Kämpfe, Konrad Seidel, and Johannes Heitmann, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00771. keywords: {neuromorphic computing Flicker noise interface traps FeFET hafnium oxide interface treatments}