Review on Application of Carbon Materials in Lithium-Oxygen/ Lithium-Carbon Dioxide Batteries AITranslate
Abstract AITranslate
The application of carbon materials in lithium-oxygen and lithium-carbon dioxide batteries is reviewed, including commercial carbon materials, carbon nano materials, heteroatom modified carbon materials, metal and its oxide modified carbon materials and biomass derived carbon materials.The reasons for the performance improvement of lithium-oxygen and lithium-carbon dioxide batteries with carbon materials as the air cathode are systematically discussed.It provides guidance for the future design of high-perfor-mance carbon materials applied in lithium-oxygen and lithium-carbon dioxide batteries.
KeyWords AITranslate
1李翔,杨思勰,冯宁宁,何平,周豪慎.Li-CO_2电池机理、催化剂和性能研究进展(英文)[J].催化学报(英文),2016,37(7):1016-1024. 被引量:7
1师小勤,赵杰,王琳琳,王琳,翟运开,高景宏.基于大数据分析技术的精准医疗应用综述[J].中国医院管理,2021,41(5):26-31. 被引量:8
2冯柳.风险管理在外科护理管理中的应用综述[J].益寿宝典,2020(15):0033-0033.
3余法松,肖曾.某型进口航改型燃机表面防护技术应用综述[J].装备维修技术,2021(11):0083-0083.
4庄惟敏,吴春花.三问“城市总设计师制”[J].建筑技艺,2021,27(3):8-9. 被引量:3
5邵斌,李静,龚瑞昆,崔传金.基于金属有机骨架的非酶葡萄糖电化学传感器[J].化学通报,2021,84(4):339-345. 被引量:1
6罗璇,王睿祺,李改赢,汤諹.新型技术在瘢痕疙瘩中的临床应用[J].皮肤病与性病,2021,43(2):171-174. 被引量:1
7张换高,李永超,高胜生,李淼,李红江.环境剖面转换引导情景分析的产品技术预见方法[J].机械设计与研究,2021,37(2):163-167. 被引量:1
8谭炜,张子卿,屈骁,张英杰,卢新根,张燕峰.跨音速涡轮定常与非定常叶尖泄漏流机理分析[J].风机技术,2021,63(2):1-11. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TM910.4[电气工程—电力电子与电力传动]
Citation Information:
The application of carbon materials in lithium-oxygen and lithium-carbon dioxide batteries is reviewed, including commercial carbon materials, carbon nano materials, heteroatom modified carbon materials, metal and its oxide modified carbon materials and biomass derived carbon materials.The reasons for the performance improvement of lithium-oxygen and lithium-carbon dioxide batteries with carbon materials as the air cathode are systematically discussed.It provides guidance for the future design of high-perfor-mance carbon materials applied in lithium-oxygen and lithium-carbon dioxide batteries.
quote
| GB/T 7714-2015 | [1] GU Yang, WANG Zhen, WU Hong-kun, et al. Review on Application of Carbon Materials in Lithium-Oxygen/ Lithium-Carbon Dioxide Batteries[J]. Rare Metals and Cemented Carbides, 2021(2): 52-56. |
| MLA | [1] GU Yang, et al., "Review on Application of Carbon Materials in Lithium-Oxygen/ Lithium-Carbon Dioxide Batteries." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 52-56. |
| APA | [1] GU Yang, WANG Zhen, WU Hong-kun, LI Xue, & ZENG Xiao-yuan. (2021). Review on Application of Carbon Materials in Lithium-Oxygen/ Lithium-Carbon Dioxide Batteries. Rare Metals and Cemented Carbides(2), 52-56. |
| IEEE | [1] GU Yang, WANG Zhen, WU Hong-kun, LI Xue, and ZENG Xiao-yuan, "Review on Application of Carbon Materials in Lithium-Oxygen/ Lithium-Carbon Dioxide Batteries," Rare Metals and Cemented Carbides, no. 2, pp. 52-56, 2021. keywords: {carbon material;air cathode;lithium-oxygen battery;lithium-carbon dioxide battery} |