Study on Elemental Distribution and Magnetic Properties of RE-Fe-B Sintered Magnets with High Ce Content AITranslate

School of Science,Inner Mongolia University of Science&Technology;School of Science,Inner Mongolia University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To develop commercially valuable RE-Fe-B magnets with high Ce content and improve the utilization of high abundance rare earth Ce,the magnetic properties and microstructure of RE-Fe-B magnets with different substitution amounts of Ce were investigated.The experimental results show that the dual main phase magnet with a Ce/(Ce+Nd)mass fraction of 40%still maintains excellent magnetic properties,with a remanence Brreaching 1.31 T,and a maximum energy product(BH)maxreaching 310.56 kJ/m3.In single and dual main phase magnets with a Ce substitution of 40%,differences appear in the displacement beha-vior of Nd and Ce elements.In single and dual main phase magnets,Nd element tends to enter the main phase grains,while Ce element tends to aggregate in the grain boundary phase or the surface layers of the main phase grains.In addition,the Ce-poor main phase and(Nd0.6Ce0.4)30.5(Fe,M)balB0.97main phase close to the nominal component are formed in the dual main phase magnet.The magnetization behavior of single and dual main phase magnets was analyzed by observing magnetic domain switching,and the enhancement mechanism of coercivity in the dual main phase magnets was studied.The high anisotropy field of the Ce-poor main phase imposes the pinning effect on the magnetic moment of the Ce-rich main phase.The study of the diffusion behavior of Nd and Ce elements provides a basis for the preparation of commercial RE-Fe-B magnets with high Ce content and superior magnetic properties.

KeyWords AITranslate

(Nd Ce)-Fe-B high Cecontent dual main phase magnet magneticdomain magnetic property elemental distribution

1徐冉,朱庆东,李健飞,李华强,王洋.不同过热故障条件下呋喃分子在油-纸界面扩散行为的分子动力学研究[J].绝缘材料,2024,57(2):121-128.

2郑道友,张瑞,唐恩.Nb元素对汽车渗碳齿轮用20CrMnTi钢热处理过程中晶粒粗化的影响[J].金属热处理,2024,49(1):113-118.

3李文涛,孙凯,林文昭.海洋平台硫化氢泄漏事故疏散地点选择[J].石化技术,2024,31(2):46-49.

4向斐斐,李傲,范浩涵,林杨剑,程峰,葛炳辉.金属诱导晶化(MIC)模式非晶晶化的原位透射电子显微学研究[J].电子显微学报,2024,43(1):45-51.

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

To develop commercially valuable RE-Fe-B magnets with high Ce content and improve the utilization of high abundance rare earth Ce,the magnetic properties and microstructure of RE-Fe-B magnets with different substitution amounts of Ce were investigated.The experimental results show that the dual main phase magnet with a Ce/(Ce+Nd)mass fraction of 40%still maintains excellent magnetic properties,with a remanence Brreaching 1.31 T,and a maximum energy product(BH)maxreaching 310.56 kJ/m3.In single and dual main phase magnets with a Ce substitution of 40%,differences appear in the displacement beha-vior of Nd and Ce elements.In single and dual main phase magnets,Nd element tends to enter the main phase grains,while Ce element tends to aggregate in the grain boundary phase or the surface layers of the main phase grains.In addition,the Ce-poor main phase and(Nd0.6Ce0.4)30.5(Fe,M)balB0.97main phase close to the nominal component are formed in the dual main phase magnet.The magnetization behavior of single and dual main phase magnets was analyzed by observing magnetic domain switching,and the enhancement mechanism of coercivity in the dual main phase magnets was studied.The high anisotropy field of the Ce-poor main phase imposes the pinning effect on the magnetic moment of the Ce-rich main phase.The study of the diffusion behavior of Nd and Ce elements provides a basis for the preparation of commercial RE-Fe-B magnets with high Ce content and superior magnetic properties.

quote

GB/T 7714-2015 [1] LI Zhi, LIU Fei. Study on Elemental Distribution and Magnetic Properties of RE-Fe-B Sintered Magnets with High Ce Content[J]. Rare Metals and Cemented Carbides, 2024(1): 38-43.
MLA [1] LI Zhi, and LIU Fei. "Study on Elemental Distribution and Magnetic Properties of RE-Fe-B Sintered Magnets with High Ce Content." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 38-43.
APA [1] LI Zhi, & LIU Fei. (2024). Study on Elemental Distribution and Magnetic Properties of RE-Fe-B Sintered Magnets with High Ce Content. Rare Metals and Cemented Carbides(1), 38-43.
IEEE [1] LI Zhi and LIU Fei, "Study on Elemental Distribution and Magnetic Properties of RE-Fe-B Sintered Magnets with High Ce Content," Rare Metals and Cemented Carbides, no. 1, pp. 38-43, 2024. keywords: {(Nd,Ce)-Fe-B;high Cecontent;dual main phase magnet;magneticdomain;magnetic property;elemental distribution}