Commercial-scale Test of the Surperfine W Powder & Tungsten Carbide Powder from ART AITranslate
Abstract AITranslate
The paper describes the commercial-scale ies t of superfineW powder & tungsten carbide powder from ART.Results show that thissuperfine powder is applicable for microdrills and ul trafine-grain cemented carbide.
KeyWords AITranslate
1方名尧.试论硬质合金微型钻及其材质问题[J].稀有金属与硬质合金,1992,20(2):34-38. 被引量:1
2熊继.超细晶粒硬质合金[J].稀有金属与硬质合金,1992,20(2):41-47. 被引量:2
1柴永新,吴晓东,戴起勋.纳米金属钨粉制备方法的研究进展[J].江西冶金,2005,25(5):37-41.
2刘辉明,范景莲,田家敏,游峰.超细钨粉的研究与应用[J].中国钨业,2009,24(1):29-32. 被引量:16
3黄忠耿.研制和生产粒度小于0.6μm碳化钨粉的工艺技术发展动态[J].稀有金属与硬质合金,1998,26(4):51-56. 被引量:8
4张文朴.钨钼基础工业化学(十)[J].中国钨业,1997,0(12):21-27.
1陈强,冯鹏发,武洲,胡林.热等离子法制备高致密球形钼粉颗粒[J].中国粉体技术,2013,19(1):42-44. 被引量:3
2吴其山.超细WC-Co硬质合金研究综述[J].中国钨业,2005,20(6):35-40. 被引量:19
3程涛,汪重露.纳米硬质合金的研究进展[J].稀有金属与硬质合金,2006,34(3):46-50. 被引量:13
4郝立伟,肖简正,洪小虎.激光粒度分布仪检测细碳化钨粉方法[J].中国钨业,2010,25(4):47-50. 被引量:4
5张彩霞,周阳.高性能超细钨粉的制备工艺研究[J].上海有色金属,2010,31(4):189-193. 被引量:2
6廖春发,杨文强,王旭,谢泉文,肖志华.由钨酸盐熔盐电解直接制备钨粉的可行性分析[J].有色金属科学与工程,2011,2(4):4-6. 被引量:5
7刘晓平,陈进.感应等离子工艺参数对制备纳米球形钨粉的影响[J].热加工工艺,2011,40(20):170-172. 被引量:4
8陈强,冯鹏发,武洲,胡林.热等离子法制取高致密球形钼粉工艺探讨[J].中国科技博览,2012(36):638-639.
9黄化,秦明礼,曲选辉,李睿.气流磨处理钨粉的研究[J].稀有金属材料与工程,2012,41(12):2210-2214. 被引量:7
10陈强,冯鹏发,武洲,胡林.高致密球形钼粉制备工艺研究[J].中国钼业,2013,37(4):38-41. 被引量:1
1孙维礼,王剑志.ANKERHARTH—电炉炉膛最佳砌筑和维护系统[J].长城技术,1992(4):70-76.
2CHENKaixian,LIYong,等.The State-of-art of Magnesia-chrome Refractories for P-S Converter in China's Non-ferrous Industry[J].中国耐火材料:英文版,2002,11(2):18-21.
3王世文,张颖,张学东,谢元旦.利用神经网络识别车辆牌照字符[J].鞍山钢铁学院学报,2001,24(1):50-52. 被引量:5
4Conn.,CL,李学芳.选择合适的WC和Co粉用于生产硬质合金[J].国外难熔金属与硬质材料,2001,17(1):1-7. 被引量:1
5WENG Yu-qing 1,YANG Cai-fu 2,SHANG Cheng-jia 3 (1.The Chinese Society for Metals,Beijing,PR China,2.Centre Iron and Steel Research Institute,Beijing,PR China,3.University of Science and Technology Beijing,Beijing,PR China).The State-of-Art and Development Trends of HSLA Steels in China[J].钢铁研究学报:英文版,2011(S1):1-13. 被引量:5
6BOOM Rob.Oxygen and Iron-and Steelmaking:Best Friends and Arch-Enemies[J].钢铁研究学报:英文版,2011(S2):16-27. 被引量:3
7沈含熙,凌蓉.STUDIES ON THE CHROMOPHORIC REACTIONS OF MIXED POLYNUCLEAR COMPLEXES OF RARE EARTH-ARSENAZO Ⅲ-COPPERO-PHENANTHROLINE[J].稀土学报:英文版,1990,0(3):218-223.
8Reinhard BARDENHEIER.Advanced test methods of material property characterization:high strain-rate testing and experimental simulation of multiaxial stress states[J].宝钢技术研究:英文版,2010,0(S1):122-122.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金];TF123.31[冶金工程—粉末冶金]
Citation Information:
The paper describes the commercial-scale ies t of superfineW powder & tungsten carbide powder from ART.Results show that thissuperfine powder is applicable for microdrills and ul trafine-grain cemented carbide.
quote
| GB/T 7714-2015 | [1] LIU Hui. Commercial-scale Test of the Surperfine W Powder & Tungsten Carbide Powder from ART[J]. Rare Metals and Cemented Carbides, 1995(2): 8-10. |
| MLA | [1] LIU Hui. "Commercial-scale Test of the Surperfine W Powder & Tungsten Carbide Powder from ART." Rare Metals and Cemented Carbides, no. 2, 1995, pp. 8-10. |
| APA | [1] LIU Hui. (1995). Commercial-scale Test of the Surperfine W Powder & Tungsten Carbide Powder from ART. Rare Metals and Cemented Carbides(2), 8-10. |
| IEEE | [1] LIU Hui, "Commercial-scale Test of the Surperfine W Powder & Tungsten Carbide Powder from ART," Rare Metals and Cemented Carbides, no. 2, pp. 8-10, 1995. keywords: {ART;super-fine W powder;super-fine tungsten carbide;commercial scafe test} |